会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 7. 发明授权
    • Aluminum alloy composite material for brazing
    • 铝合金复合材料用于钎焊
    • US5350436A
    • 1994-09-27
    • US156827
    • 1993-11-24
    • Osamu TakezoeJun TakigawaTadashi OkamotoMituo HashiuraSunao FukudaKeizo TakeuchiYasuaki Isobe
    • Osamu TakezoeJun TakigawaTadashi OkamotoMituo HashiuraSunao FukudaKeizo TakeuchiYasuaki Isobe
    • B23K35/02B23K35/28B32B15/01F28F13/12F28F21/08B32B15/20
    • C22C21/00B23K35/286B32B15/016C22C21/02C22C21/06C22C21/10F28F13/12F28F21/084F28F21/089B23K35/0238Y10T428/12028Y10T428/12764
    • An aluminum alloy composite material for brazing has a core member, an Al--Si filler member clad on one surface of the core member and an aluminum alloy cladding member clad on the other side of the core member. The core member is made of an aluminum alloy containing 0.3 to 1.3 wt. % of Si, 0.3 to 1.5 wt. % of Mn, 0.02 to 0.3 wt. % of Ti, and, as required, 0.3 wt. % or less of Cr and 0.2 wt. % or less of Zr, the content of Mg being restricted to 0.2 wt. % or less and the content of the Cu being restricted to 0.2 wt. % or less as an impurity. The cladding member is made of an aluminum alloy containing 0.3 to 3 wt. % of Mg, 5 wt. % or less of Zn, 0.1 to 1.0 wt. % of Si. The thickness of the core member is preferably, 2.5 times or more greater than that of the filler member, falling within a range of 0.1 to 1 mm. With this, it is possible to obtain an aluminum alloy composite material which cannot degraded in brazability and corrosion resistance even when brazed by the brazing method with noncorrosive flux and which has enough high strength to be used for a material of a high-strength heat exchanger, highly improved corrosion resistance and excellent brazability.
    • 用于钎焊的铝合金复合材料具有芯构件,包覆在芯构件的一个表面上的Al-Si填充构件和在芯构件的另一侧上包覆的铝合金覆层构件。 芯构件由含有0.3〜1.3重量%的铝合金制成。 %的Si,0.3〜1.5wt。 %的Mn,0.02〜0.3wt。 %的Ti,根据需要,0.3重量% Cr%以下,0.2重量%以下。 %以下的Zr,Mg的含量限定为0.2重量%。 %以下,Cu的含量限制在0.2重量%左右。 %以下的杂质。 包层部件由含有0.3〜3重量%的铝合金制成。 %的Mg,5wt。 %以下的Zn,0.1〜1.0wt。 %的Si。 芯构件的厚度优选为填充构件的厚度的2.5倍以上,落在0.1〜1mm的范围内。 由此,可以获得即使用非腐蚀性焊剂钎焊法钎焊而且钎焊耐腐蚀性也不劣化的铝合金复合材料,其具有足够高的强度用于高强度热交换器的材料 耐腐蚀性高,钎焊性优异。