    • 4. 发明授权
    • Use of thermoplastic molding materials for GID/WIT
    • 使用热塑性成型材料进行GID / WIT
    • US08425829B2
    • 2013-04-23
    • US13478971
    • 2012-05-23
    • Andreas EipperRainer KlenzThomas FritzscheMark Völkel
    • Andreas EipperRainer KlenzThomas FritzscheMark Völkel
    • B29C43/34B29C43/52C08L67/03
    • C08L67/02C08K7/02C08K7/16C08L67/00C08L69/00C08L2666/18
    • Use of thermoplastic molding compositions comprising A) from 10 to 89% by weight of a polyethylene terephthalate which can comprise up to 65% by weight, based on 100% by weight of A), of another polyester, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, part 2), or B2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1, or a mixture of these, C) from 10 to 60% by weight of a fibrous or particulate filler, and D) from 0 to 20% by weight of further additives, where the total of the percentages by weight of components A) to D) is 100%, for the production of moldings by means of the internal-gas-pressure process and/or the water-injection process.
    • 使用热塑性模塑组合物,其包含A)10至89重量%的聚对苯二甲酸乙二醇酯,其可以包含至多65重量%,基于100重量%的A),另一个聚酯,B)0.01至50重量% 至少一种高度支化或超支化的聚碳酸酯,其OH值为1至600mg KOH / g聚碳酸酯(根据DIN 53240,第2部分)或B2)至少一种高度支化或超支化的AxBy聚酯 类型,其中x为至少1.1,y为至少2.1,或这些的混合物,C)10至60重量%的纤维或颗粒填料,以及D)0至20重量%的其它添加剂 ,其中组分A)至D)的重量百分比的总和为100%,用于通过内部气体压力法和/或注水方法生产模制品。
    • 5. 发明申请
    • USE OF THERMOPLASTIC MOLDING MATERIALS FOR GID/WIT
    • 用于GID / WIT的热塑性模塑材料的使用
    • US20100249311A1
    • 2010-09-30
    • US12743530
    • 2008-11-18
    • Andreas EipperRainer KlenzThomas FritzscheMark Völkel
    • Andreas EipperRainer KlenzThomas FritzscheMark Völkel
    • B29C45/18C08L65/00C08L69/00
    • C08L67/02C08K7/02C08K7/16C08L67/00C08L69/00C08L2666/18
    • Use of thermoplastic molding compositions comprising A) from 10 to 89% by weight of a polyethylene terephthalate which can comprise up to 65% by weight, based on 100% by weight of A), of another polyester, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, part 2), or B2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1, or a mixture of these, C) from 10 to 60% by weight of a fibrous or particulate filler, and D) from 0 to 20% by weight of further additives, where the total of the percentages by weight of components A) to D) is 100%, for the production of moldings by means of the internal-gas-pressure process and/or the water-injection process.
    • 使用热塑性模塑组合物,其包含A)10至89重量%的聚对苯二甲酸乙二醇酯,其可以包含至多65重量%,基于100重量%的A),另一个聚酯,B)0.01至50重量% 至少一种高度支化或超支化的聚碳酸酯,其OH值为1至600mg KOH / g聚碳酸酯(根据DIN 53240,第2部分)或B2)至少一种高度支化或超支化的AxBy聚酯 类型,其中x为至少1.1,y为至少2.1,或这些的混合物,C)10至60重量%的纤维或颗粒填料,以及D)0至20重量%的其它添加剂 ,其中组分A)至D)的重量百分比的总和为100%,用于通过内部气体压力法和/或注水方法生产模制品。
    • 6. 发明申请
    • USE OF THERMOPLASTIC MOLDING MATERIALS FOR GID/WIT
    • 用于GID / WIT的热塑性模塑材料的使用
    • US20120261866A1
    • 2012-10-18
    • US13478971
    • 2012-05-23
    • Andreas EipperRainer KlenzThomas FritzscheMark Völkel
    • Andreas EipperRainer KlenzThomas FritzscheMark Völkel
    • B29C49/06
    • C08L67/02C08K7/02C08K7/16C08L67/00C08L69/00C08L2666/18
    • Use of thermoplastic molding compositions comprising A) from 10 to 89% by weight of a polyethylene terephthalate which can comprise up to 65% by weight, based on 100% by weight of A), of another polyester, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, part 2), or B2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1, or a mixture of these, C) from 10 to 60% by weight of a fibrous or particulate filler, and D) from 0 to 20% by weight of further additives, where the total of the percentages by weight of components A) to D) is 100%, for the production of moldings by means of the internal-gas-pressure process and/or the water-injection process.
    • 使用热塑性模塑组合物,其包含A)10至89重量%的聚对苯二甲酸乙二醇酯,其可以包含至多65重量%,基于100重量%的A),另一个聚酯,B)0.01至50重量% 至少一种高度支化或超支化的聚碳酸酯,其OH值为1至600mg KOH / g聚碳酸酯(根据DIN 53240,第2部分)或B2)至少一种高度支化或超支化的AxBy聚酯 类型,其中x为至少1.1,y为至少2.1,或这些的混合物,C)10至60重量%的纤维或颗粒填料,以及D)0至20重量%的其它添加剂 ,其中组分A)至D)的重量百分比的总和为100%,用于通过内部气体压力法和/或注水方法生产模制品。
    • 8. 发明授权
    • Cleaning material for extruders
    • 挤出机清洗材料
    • US06673759B1
    • 2004-01-06
    • US09868096
    • 2001-06-14
    • Uwe KochRainer KlenzPeter FrielBrigitte Gareiss
    • Uwe KochRainer KlenzPeter FrielBrigitte Gareiss
    • C11D337
    • B29C47/0877B29C47/0009B29K2077/00
    • The invention relates to a cleaning composition for apparatus for processing thermoplastic melts, which composition essentially comprises discrete particles capable of plastic deformation and made from a thermoplastic (A) with a melting point above 200° C. and with a crystallinity of not more than 50%, and comprises an amorphous or semicrystalline thermoplastic (B) with a processing temperature below the melting point of the thermoplastic (A). The proportion of the thermoplastic (A) is from 1 to 95% by weight and that of the thermoplastic (B) is from 5 to 95% by weight. The total of the percentage proportions by weight of (A) and (B) is always 100% or less. The discrete particles made from the thermoplastic (A) and capable of plastic deformation have a very effective cleaning action, while the amorphous or semicrystalline thermoplastic (B) acts as a liquid or flowable carrier for the particles, which are made from the thermoplastic (A) and/or contamination which has been released, and are capable of plastic deformation.
    • 本发明涉及一种用于加工热塑性熔体的设备的清洁组合物,该组合物基本上包括能够塑性变形的离散颗粒,并由熔点高于200℃的热塑性(A)和不超过50的结晶度 %,并且包括处理温度低于热塑性塑料(A)的熔点的无定形或半结晶的热塑性塑料(B)。 热塑性(A)的比例为1〜95重量%,热塑性(B)的比例为5〜95重量%。 (A)和(B)的重量百分比的总和总是为100%以下。由热塑性(A)制成并且能够塑性变形的离散颗粒具有非常有效的清洁作用,而无定形或半结晶 热塑性(B)作为颗粒的液体或可流动载体,其由热塑性(A)和/或已被释放并且能够塑性变形的污染物制成。
    • 10. 发明申请
    • LOW-EMISSION PBT VIA INJECTION MOLDING WITH VENT APPARATUS
    • 低排放PBT通过注射成型与通风装置
    • US20090039557A1
    • 2009-02-12
    • US12278442
    • 2007-02-01
    • Rainer KlenzNorbert EffenMark VolkelAndreas EipperJens AssmannMichael Dahlke
    • Rainer KlenzNorbert EffenMark VolkelAndreas EipperJens AssmannMichael Dahlke
    • B29C45/00
    • B29C45/0001B29C45/63B29K2067/006C08L25/12C08L25/14C08L67/02C08L2666/06
    • A process is proposed for production of low-emission moldings for continuous operating temperatures >50° C. composed of a thermoplastic molding composition comprising A) from 10 to 99.9% by weight of polybutylene terephthalate or a mixture thereof with polyethylene terephthalate and/or polypropylene terephthalate, B) from 0.1 to 50% by weight of at least one terpolymer obtainable from b1) at least one vinylaromatic monomer, b2) at least one C1-C4-alkyl (meth)acrylate or (meth)acrylonitrile, and b3) from 0.1 to 10% by weight, based on the total weight of components b1) to b3), of at least one monomer which comprises an α,β-unsaturated anhydride, and C) from 0 to 60% by weight of other additives, where the total of the percentages by weight of the components (A) to (C) is 100%, via injection molding, which comprises carrying out the injection molding by means of a vented plastifying unit with a cylinder with inlet aperture for the thermoplastic molding composition, with a screw which conveys and plastifies the thermoplastic molding composition within a screw channel, and with one or more vents for discharge of volatile content from the plastified thermoplastic molding composition from the screw channel outward from the vented plastifying unit.
    • 提出了一种生产用于连续工作温度> 50℃的低排放模制品的方法,其由热塑性模塑组合物组成,其包含A)10至99.9重量%的聚对苯二甲酸丁二醇酯或其与聚对苯二甲酸乙二醇酯和/或聚丙烯的混合物 B)0.1至50重量%的至少一种由b1)至少一种乙烯基芳族单体获得的至少一种三元共聚物,b2)至少一种(甲基)丙烯酸C 1 -C 4烷基酯或(甲基)丙烯腈,和b 3)从 0.1至10重量%,基于组分b1)至b3)的总重量,至少一种包含α,β-不饱和酸酐的单体,和C)0至60重量%的其它添加剂,其中 通过注射成型,组分(A)至(C)的重量百分比的总和为100%,其包括通过具有用于热塑性模塑组合物的入口孔的气缸进行注射成型 ,用螺丝w 在螺旋通道内传送和塑化热塑性模塑组合物,以及一个或多个排气孔,用于从膨胀的塑化模塑组合物从膨胀塑化单元向外的螺旋通道排放挥发物。