    • POLYETHLENE BLEND COMPOSITION SUITABLE FOR BLOWN FILM, METHOD OF PRODUCING THE SAME, AND FILMS MADE THEREFORM
    • 适用于薄膜的聚乙烯混合组合物,其制备方法及其制备方法
    • US20140134364A1
    • 2014-05-15
    • US14118652
    • 2012-07-02
    • Lawrence J. EfflerNilesh R. SavargaonkarTeresa P. KarjalaCristina SerratJian Wang
    • Lawrence J. EfflerNilesh R. SavargaonkarTeresa P. KarjalaCristina SerratJian Wang
    • C08L23/06
    • C08L23/06C08J5/18C08J2323/08C08L23/0815C08L2205/02C08L2205/025Y10T428/1352
    • The instant invention provides a polyethylene blend composition suitable for blown film, method of producing the same, and films made therefrom. The polyethylene blend composition suitable for blown film, according to the present invention, comprises the melt blending product of: (a) from 5 percent or less by weight of a first low density polyethylene (first LDPE) having a density in the range of from 0.915 to 0.935 g/cm3, and a melt index (I2) in the range of from greater than 0.8 to less than or equal to 5 g/10 minutes, and a molecular weight distribution (Mw/Mn) in the range of from 6 to 10; (b) from 5 to 50 percent by weight of a second low density polyethylene (second LDPE) having a density in the range of from 0.915 to 0.935 g/cm3, and a melt index (I2) in the range of from 0.1 to less than or equal to 5 g/10 minutes, and a molecular weight distribution (Mw/Mn) in the range of from 6 to 10; with the proviso that the second LDPE has a melt index (I2) that is different from the melt index (I2) of first LDPE; (c) from 44 percent or greater by weight of a heterogeneous linear low density polyethylene (hLLDPE) having a density in the range of from 0.917 to 0.950 g/cm3, and a melt index (I2) in the range of from 0.1 to less than or equal to 5 g/10 minutes; (d) optionally a hydrotalcite based neutralizing agent (e) optionally one or more nucleating agents; and (f) optionally one or more antioxidants. When said polyethylene blend-composition is formed into a film via a blown film process, the output rate is improved at least 6 percent, for example 7 percent, relative to a polyethylene blend composition consisting essentially of (a) a similar heterogeneous linear low density polyethylene component; and (b) a similar second low density polyethylene component.
    • 本发明提供了适用于吹塑薄膜的聚乙烯共混组合物,其制备方法和由其制成的薄膜。 根据本发明的适用于吹塑薄膜的聚乙烯共混组合物包括熔融共混产物:(a)5重量%或更少的第一低密度聚乙烯(第一LDPE),其密度范围为 0.915-0.935g / cm3,熔体指数(I2)在大于0.8至小于或等于5g / 10分钟的范围内,分子量分布(Mw / Mn)在6 到10 (b)5至50重量%的密度在0.915-0.935g / cm3范围内的第二低密度聚乙烯(第二LDPE),熔体指数(I 2)在0.1以下的范围内 或者等于5g / 10分钟,分子量分布(Mw / Mn)在6至10的范围内; 条件是第二LDPE具有与第一LDPE的熔体指数(I 2)不同的熔体指数(I 2); (c)44重量%以上的密度为0.917〜0.950g / cm 3的异相线性低密度聚乙烯(hLLDPE),熔体指数(I 2)为0.1以下 大于或等于5g / 10分钟; (d)任选的水滑石类中和剂(e)任选的一种或多种成核剂; 和(f)任选的一种或多种抗氧化剂。 当所述聚乙烯共混物组合物通过吹塑薄膜法形成薄膜时,相对于基本上由(a)类似的异质线性低密度聚乙烯混合物组合物组成的聚乙烯混合物组合物,输出速率提高至少6%,例如7% 聚乙烯组分; 和(b)类似的第二低密度聚乙烯组分。
    • 6. 发明申请
    • RESIN COMPOSITIONS FOR EXTRUSION COATING
    • 用于挤出涂料的树脂组合物
    • US20120316284A1
    • 2012-12-13
    • US13157428
    • 2011-06-10
    • Jian WangMehmet Demirors
    • Jian WangMehmet Demirors
    • C09D123/06C09D7/12
    • C08L23/0815C08L23/06C08L2205/02C08L2314/06C09D123/0815
    • This invention pertains to polyethylene extrusion compositions. In particular, the invention pertains to ethylene polymer extrusion compositions having high drawdown and substantially reduced neck-in. The compositions comprise from 40 to 90% by weight of the composition of a first polyethylene composition, said first polyethylene composition comprising a linear low density polyethylene having a density in the range of from 0.90 to 0.96 g/cm3, and a melt index (I2) of from 5 to 15 g/10 min; and from 1 to 10% by weight of the composition of a second polyethylene composition, said second polyethylene composition comprising a high pressure low density polyethylene having a density in the range of from 0.915 to 0.930 g/cm3, and a melt index of from 0.1 to 3 g/10 min; and from 10 to 50% by weight of the composition of a third polyethylene composition, said third polyethylene composition comprising a high pressure low density polyethylene having a density in the range of from 0.915 to 0.930 g/cm3, and a melt index of from 5 to 15 g/10 min.
    • 本发明涉及聚乙烯挤出组合物。 特别地,本发明涉及具有高降低和显着降低颈缩的乙烯聚合物挤出组合物。 所述组合物包含组合物的40至90重量%的第一聚乙烯组合物,所述第一聚乙烯组合物包含密度在0.90至0.96g / cm 3范围内的线性低密度聚乙烯和熔体指数(I 2 )为5〜15g / 10min; 和组合物的1至10重量%的第二聚乙烯组合物,所述第二聚乙烯组合物包含密度在0.915-0.930g / cm3范围内的高压低密度聚乙烯,熔体指数为0.1 至3g / 10min; 和组合物的10至50重量%的第三聚乙烯组合物,所述第三聚乙烯组合物包含密度在0.915-0.930g / cm3范围内的高压低密度聚乙烯,熔体指数为5 至15g / 10min。
    • 7. 发明授权
    • Resin compositions for extrusion coating
    • 用于挤出涂层的树脂组合物
    • US09493641B2
    • 2016-11-15
    • US13157428
    • 2011-06-10
    • Jian WangMehmet Demirors
    • Jian WangMehmet Demirors
    • C08L23/00C08L23/08C08L23/06C09D123/08
    • C08L23/0815C08L23/06C08L2205/02C08L2314/06C09D123/0815
    • This invention pertains to polyethylene extrusion compositions. In particular, the invention pertains to ethylene polymer extrusion compositions having high drawdown and substantially reduced neck-in. The compositions comprise from 40 to 90% by weight of the composition of a first polyethylene composition, said first polyethylene composition comprising a linear low density polyethylene having a density in the range of from 0.90 to 0.96 g/cm3, and a melt index (I2) of from 5 to 15 g/10 min; and from 1 to 10% by weight of the composition of a second polyethylene composition, said second polyethylene composition comprising a high pressure low density polyethylene having a density in the range of from 0.915 to 0.930 g/cm3, and a melt index of from 0.1 to 3 g/10 min; and from 10 to 50% by weight of the composition of a third polyethylene composition, said third polyethylene composition comprising a high pressure low density polyethylene having a density in the range of from 0.915 to 0.930 g/cm3, and a melt index of from 5 to 15 g/10 min.
    • 本发明涉及聚乙烯挤出组合物。 特别地,本发明涉及具有高降低和显着降低颈缩的乙烯聚合物挤出组合物。 所述组合物包含组合物的40至90重量%的第一聚乙烯组合物,所述第一聚乙烯组合物包含密度在0.90至0.96g / cm 3范围内的线性低密度聚乙烯和熔体指数(I 2 )为5〜15g / 10min; 和组合物的1至10重量%的第二聚乙烯组合物,所述第二聚乙烯组合物包含密度在0.915-0.930g / cm3范围内的高压低密度聚乙烯,熔体指数为0.1 至3g / 10min; 和组合物的10至50重量%的第三聚乙烯组合物,所述第三聚乙烯组合物包含密度在0.915-0.930g / cm3范围内的高压低密度聚乙烯,熔体指数为5 至15g / 10min。