    • 6. 发明申请
    • Lead Storage Battery and Manufacturing Method of the Same
    • 铅蓄电池及其制造方法
    • US20080107960A1
    • 2008-05-08
    • US11720602
    • 2005-09-27
    • Jun FurukawaToshimichi TakadaDaisuke MonmaHidetoshi Abe
    • Jun FurukawaToshimichi TakadaDaisuke MonmaHidetoshi Abe
    • H01M2/02H01M10/08H01M10/12
    • H01M10/08H01M4/685H01M10/12H01M2300/0005Y02E60/126Y02P70/54
    • There is disclosed a lead storage battery comprising a group of plates housed in a battery jar, and an electrolyte injected therein to impregnate the group of plates with the electrolyte, thus performing formation treatment, the lead storage battery being adapted to be used in a partial state of charge where the state of charge is confined within the range of more than 70% to less than 100%, wherein the group of plates are formed of a stack constituted by a large number of negative substrates comprising grid substrates filled with a negative active material, by a large number of positive substrates comprising grid substrates filled with a positive active material, and by a porous separator interposed between the negative electrodes and positive electrodes, and the electrolyte contains at least one kind of ion selected from the group consisting of aluminum ions, selenium ions and titanium ions.
    • 公开了一种铅蓄电池,其包括容纳在电池罐中的一组板和注入其中的电解质以使电解质浸渍该组板,从而进行形成处理,该铅蓄电池适于部分地使用 其中电荷状态被限制在大于70%至小于100%的范围内的电荷状态,其中所述板组由由大量负极基板构成的堆叠构成,所述负极基板包括填充有负极活性物质的栅格基板 材料,通过大量正极基板,其包括填充有正极活性材料的栅格基板,以及插入在负极和正极之间的多孔隔板,并且所述电解质包含选自铝中的至少一种离子 离子,硒离子和钛离子。
    • 7. 发明授权
    • Lead storage battery and manufacturing method of the same
    • 铅蓄电池及其制造方法相同
    • US08771871B2
    • 2014-07-08
    • US11720602
    • 2005-09-27
    • Jun FurukawaToshimichi TakadaDaisuke MonmaHidetoshi Abe
    • Jun FurukawaToshimichi TakadaDaisuke MonmaHidetoshi Abe
    • H01M4/56H01M6/04
    • H01M10/08H01M4/685H01M10/12H01M2300/0005Y02E60/126Y02P70/54
    • There is disclosed a lead storage battery comprising a group of plates housed in a battery jar, and an electrolyte injected therein to impregnate the group of plates with the electrolyte, thus performing formation treatment, the lead storage battery being adapted to be used in a partial state of charge where the state of charge is confined within the range of more than 70% to less than 100%, wherein the group of plates are formed of a stack constituted by a large number of negative substrates comprising grid substrates filled with a negative active material, by a large number of positive substrates comprising grid substrates filled with a positive active material, and by a porous separator interposed between the negative electrodes and positive electrodes, and the electrolyte contains at least one kind of ion selected from the group consisting of aluminum ions, selenium ions and titanium ions.
    • 公开了一种铅蓄电池,其包括容纳在电池罐中的一组板和注入其中的电解质以使电解质浸渍该组板,从而进行形成处理,该铅蓄电池适于部分地使用 其中电荷状态被限制在大于70%至小于100%的范围内的电荷状态,其中所述板组由由大量负极基板构成的堆叠构成,所述负极基板包括填充有负极活性物质的栅格基板 材料,通过大量正极基板,其包括填充有正极活性材料的栅格基板,以及插入在负极和正极之间的多孔隔板,并且所述电解质包含选自铝中的至少一种离子 离子,硒离子和钛离子。
    • 9. 发明申请
    • ENERGY STORAGE DEVICE
    • 能源储存装置
    • US20100203362A1
    • 2010-08-12
    • US12518521
    • 2007-12-12
    • Lan Trieu LamJun Furukawa
    • Lan Trieu LamJun Furukawa
    • H01M12/02
    • H01M10/4235H01G11/04H01G11/12H01G11/22H01G11/32H01G11/46H01M4/56H01M4/62H01M4/73H01M10/06H01M10/08H01M12/005H01M2004/021H01M2004/028Y02E60/126Y02E60/13Y02T10/7016Y02T10/7022
    • An energy storage device comprising at least one negative electrode, wherein each negative electrode is individually selected from (i) an electrode comprising negative battery electrode material; (ii) an electrode comprising capacitor electrode material; (iii) a mixed electrode comprising either—a mixture of battery and capacitor electrode material or—a region of battery electrode material and a region of capacitor electrode material, or—a combination thereof, and wherein the energy storage device either comprises at least one electrode of type (iii), or comprises at least one electrode of each of types (i) and (ii),—at least one positive electrode, wherein the positive electrode comprises positive battery electrode material and a charging ability-increasing additive, such as one or a mixture of: (a) carbon nanomaterial, vapour grown carbon fibre, fullerene, or a mixture thereof, and (b) tin dioxide conductive materials.
    • 一种能量存储装置,包括至少一个负电极,其中每个负电极分别选自(i)包含负电池电极材料的电极; (ii)包括电容器电极材料的电极; (iii)混合电极,其包括电池和电容器电极材料的混合物或电池电极材料的区域和电容器电极材料的区域或其组合,并且其中所述能量存储装置包括至少一个 (iii)类型的电极,或者包括至少一种类型(i)和(ii)中的每一种的电极, - 至少一个正电极,其中所述正电极包括正电池电极材料和充电增加添加剂, 作为一种或其混合物:(a)碳纳米材料,气相生长碳纤维,富勒烯或其混合物,和(b)二氧化锡导电材料。
    • 10. 发明申请
    • PROCESS FOR PRODUCING NEGATIVE PLATE FOR LEAD STORAGE BATTERY, AND LEAD STORAGE BATTERY
    • 铅蓄电池负极板生产工艺及铅蓄电池
    • US20120094174A1
    • 2012-04-19
    • US13265944
    • 2010-03-19
    • Jun FurukawaDaisuke MommaToshimichi TakadaTrieu Lan LamRosalie LoueyPeter Nigel Haigh
    • Jun FurukawaDaisuke MommaToshimichi TakadaTrieu Lan LamRosalie LoueyPeter Nigel Haigh
    • H01M10/06H01M10/12H01M10/08B05D5/12B05D3/14
    • H01M4/20H01M4/0416H01M4/0445H01M4/0452H01M4/22H01M4/366H01M4/622H01M4/623H01M4/625H01M10/06H01M2004/027Y02E60/126Y02P70/54
    • To provide a method for producing a lead-acid battery negative plate for use in a storage battery which provides improved deteriorated rapid discharge characteristics by preventing an interfacial separation between a negative active material-filled plate and a carbon mixture-coated layer, which is a problem in a negative plate having such a configuration that the carbon mixture coated layer is formed on the surface of the negative active material-filled plate.A coating layer of a carbon mixture is formed at least in a part of a surface of a negative active material-filled plate. The carbon mixture is prepared by mixing two kinds of carbon materials consisting of a first carbon material having conductive properties and a second carbon material having capacitive capacitance and/or pseudo capacitive capacitance and a binding agent. Subsequently, a sufficient amount of lead ions are generated enough to be moved from the negative active Material-filled plate into the carbon mixture-coated layer. Thereafter, a formation treatment or an initial charge treatment is performed to precipitate lead so that the carbon mixture-coated layer and the negative plate are connected and integrated, at least in a part of a respective interfacial surface thereof, by the precipitated lead.
    • 本发明提供一种蓄电池用铅酸蓄电池用负极板的制造方法,其特征在于,通过防止负极活性物质填充板和碳混合物涂层之间的界面分离而提供改善的快速放电特性, 具有这样一种构造的负极板的问题,即在负极活性材料填充板的表面上形成碳混合物涂层。 在负极活性物质填充板的表面的至少一部分中形成碳混合物的涂层。 碳混合物通过混合由具有导电性质的第一碳材料和具有电容电容和/或伪电容电容的第二碳材料和粘合剂组成的两种碳材料来制备。 随后,产生足够量的铅离子以从负极活性材料填充板移动到碳混合物涂覆层中。 此后,进行形成处理或初始充电处理以使铅沉淀,使得碳混合物涂覆层和负极板通过沉淀的铅连接并整合至其一部分相应的界面。