    • 4. 发明申请
    • RESIN BLEND FOR MELTING PROCESS
    • 用于熔融工艺的树脂混合物
    • US20130295397A1
    • 2013-11-07
    • US13862159
    • 2013-04-12
    • LG CHEM, LTD.
    • Houng Sik YOOJin Young RYUHak Shin KIMEun Joo CHOIYoung Jun HONGHyun Seok YANG
    • C08L33/14
    • C08L33/20C08L33/06C08L33/14C08L35/06C08L101/02Y10T428/2998Y10T428/31536Y10T428/31931C08L101/12C08L101/00
    • Provided are a resin blend for forming a layer-separated structure, a pellet, a method of preparing a resin article using the same and a resin article. The resin blend may include a first resin, and a second resin that comprises a resin to which at least one organic functional group selected from the group consisting of an alkyl group having 2 to 20 carbon atoms, an alicyclic group having 5 to 40 carbon atoms and an aromatic group having 6 to 40 carbon atoms is introduced, that has a difference in melt viscosity from the first resin of 0.1 to 3000 pa*s at a shear rate of 100 to 1000 s−1 and a processing temperature of the resin blend, and that has a difference in glass transition temperature from the first resin of 10° C. to 150° C. The resin blend can improve mechanical and surface characteristics of a resin article. Further, since coating or plating is not required for manufacturing a resin article, a manufacturing time and/or cost can be reduced, and productivity can be increased.
    • 提供了用于形成层分离结构的树脂共混物,颗粒,使用其的树脂制品的制备方法和树脂制品。 树脂共混物可以包括第一树脂和第二树脂,其包含选自碳原子数2〜20的烷基中的至少一种有机官能团的碳原子数为5〜40的脂肪族基团的树脂, 引入碳原子数为6〜40的芳香族基团,在100〜1000秒-1的剪切速度下,与第一树脂的熔融粘度不同,熔融粘度为0.1〜3000Pa·s,树脂共混物的加工温度 ,并且与10℃至150℃的第一树脂的玻璃化转变温度不同。树脂共混物可以改善树脂制品的机械和表面特性。 此外,由于制造树脂制品不需要涂覆或电镀,因此可以降低制造时间和/或成本,并且可以提高生产率。