会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明专利
    • Laminate film
    • 层压膜
    • JP2012128232A
    • 2012-07-05
    • JP2010280249
    • 2010-12-16
    • Konica Minolta Advanced Layers Incコニカミノルタアドバンストレイヤー株式会社
    • INAGAKI SHINJIMAEJIMA KATSUMI
    • G02B5/30B32B27/00
    • PROBLEM TO BE SOLVED: To provide a laminate film where cycloolefin layers having different glass transition points (Tg) are laminated and where oblique stripe failure, transverse failure, vertical stripe failure and corner unevenness are improved.SOLUTION: A laminate film produced by film-formation and lamination of a cycloolefin resin layer A and a cycloolefin resin layer B using a melt casting film forming method is characterized in that the glass transition temperature difference ΔTg (Tg(a)-Tg(b)) is 5°C or more when the glass transition temperature of the cycloolefin resin layer A is defined as Tg(a) and the glass transition temperature of the cycloolefin resin layer B is defined as Tg(b), and in that the melt flow rate of both the cycloolefin resin layer A and the cycloolefin resin layer B is 5 g/10 min or more and 50 g/10 min or less.
    • 要解决的问题:为了提供层叠具有不同玻璃化转变点(Tg)的环烯烃层并且倾斜条纹破坏,横向破坏,垂直条纹破坏和拐角不均匀性提高的层压膜。 解决方案:使用熔融流延膜形成方法通过环烯烃树脂层A和环烯烃树脂层B的成膜和层压制备的层压膜的特征在于玻璃化转变温度差ΔTg(Tg(a) - 当环烯烃树脂层A的玻璃化转变温度定义为Tg(a),环烯烃树脂层B的玻璃化转变温度定义为Tg(b)时,Tg(b))为5℃以上, 环烯烃树脂层A和环烯烃树脂层B的熔体流动速率为5g / 10分钟以上且50g / 10分钟以下。 版权所有(C)2012,JPO&INPIT
    • 5. 发明专利
    • Phase difference film and method for manufacturing the same, elongated polarizing plate, and liquid crystal display device
    • 相位差薄膜及其制造方法,延伸的极化板和液晶显示装置
    • JP2012173677A
    • 2012-09-10
    • JP2011037987
    • 2011-02-24
    • Konica Minolta Advanced Layers Incコニカミノルタアドバンストレイヤー株式会社
    • MISHIMA KENJIINAGAKI SHINJIMAEJIMA KATSUMI
    • G02B5/30B29C55/12B29K1/00B29L9/00B29L11/00C08F2/46C08J5/18C08J7/04G02F1/13363
    • PROBLEM TO BE SOLVED: To provide a phase difference film where no streak failure occurs and optical property in a width direction rarely fluctuates in an environmental endurance test, a method for manufacturing the phase difference film as an elongated stretched film, and an elongated polarizing plate and a liquid crystal display device provided with the stretched film.SOLUTION: A phase difference film is provided with a hard coat layer and has the following features: (1) the direction of a slow phase axis of the phase difference film differs from a longitudinal direction and a width direction of the film and is between the two directions; (2) in-plane phase difference value Ro measured under a prescribed condition is within a specific range; and (3) when the phase difference film is preserved in a prescribed high temperature and high humidity environment for many hours and the in-plane phase difference value Ro in the horizontal direction of the phase difference film after preservation is measured under the same condition as said measurement, a difference between the maximum value and the minimum value of variation value with the in-plane phase difference value Ro before preservation as reference is within a specific range.
    • 要解决的问题:为了提供在环境耐久试验中不发生条纹破坏和宽度方向的光学特性很少波动的相位差膜,制造作为细长拉伸膜的相位差膜的方法和 伸长的偏光板和设置有拉伸膜的液晶显示装置。 <解决方案>相位差膜具有硬涂层,具有以下特征:(1)相位差膜的慢相轴方向与膜的长度方向和宽度方向不同, 在两个方向之间; (2)在规定条件下测定的面内相位差值Ro在特定范围内; 和(3)当相位差膜在规定的高温高湿环境下保存数小时,并且在与保存后的相位差膜的水平方向上的面内相位差值Ro在与 所述测量中,作为参考的保存前的面内相位差值Ro的变化值的最大值和最小值之间的差在特定范围内。 版权所有(C)2012,JPO&INPIT