    • 9. 发明申请
    • METHOD AND APPARATUS FOR A PROGRESSIVE PRIZE STRUCTURE IN AN INSTANT GAME
    • 在即时游戏中进步奖励结构的方法和装置
    • US20120122536A1
    • 2012-05-17
    • US12945611
    • 2010-11-12
    • Michael D. FrickMark B. DavisDavid Richard MizeurStan Pade
    • Michael D. FrickMark B. DavisDavid Richard MizeurStan Pade
    • A63F3/06
    • A63F3/0645G07F17/3244G07F17/326G07F17/329
    • A multi-priced instant lottery game with a first price point and a second price point is provided such that (i) the first price point corresponds to a first known potential fixed prize and a first known potential percentage of a progressive prize and (ii) the second price point corresponds to a second known potential fixed prize and a second known potential percentage of the progressive prize. The second price point is greater than the first price point. The second known potential fixed prize being greater than the first known potential fixed prize. The second known potential percentage of the progressive prize is greater than the first known potential percentage of the progressive prize. Further, a set of indicia associated with an instant lottery game ticket is generated. In addition, the instant lottery game ticket with the set of indicia is printed with a lottery ticket printer.
    • 提供具有第一价格点和第二价格点的多价即时彩票游戏,使得(i)第一价格点对应于第一已知潜在固定奖品和先进奖品的第一已知潜在百分比,以及(ii) 第二价格点对应于第二已知潜在固定奖金和第二已知潜在百分比的渐进奖品。 第二个价格点大于第一个价格点。 第二个已知的潜在固定奖大于第一个已知的潜在固定奖。 进步奖的第二个已知潜在百分比大于先进奖的第一个已知潜在百分比。 此外,生成与即时彩票游戏机相关联的一组标记。 此外,具有一组标记的即时彩票游戏机打印有彩票打印机。
    • 10. 发明申请
    • POLYETHYLENE COMPOSITIONS, METHOD OF PRODUCING THE SAME, FIBERS MADE THEREFROM, AND METHOD OF MAKING THE SAME
    • US20110092937A1
    • 2011-04-21
    • US12739511
    • 2009-07-09
    • Randy E. PepperMridula KapurGert J. ClaasenEdward N. KnickerbockerNathan J. WikerWilliam J. Michie, JR.Mark B. Davis
    • Randy E. PepperMridula KapurGert J. ClaasenEdward N. KnickerbockerNathan J. WikerWilliam J. Michie, JR.Mark B. Davis
    • A61F13/51C08F210/02C08F4/72B29C47/00D04H1/56B32B5/02D03D15/00D04H13/00D04B21/00D04H1/46
    • D01F6/30C08F210/02C08L23/04C08L23/0815C08L2205/02C08L2205/16C08L2314/06D01D5/08D01D5/10D01D5/12D01D10/02D01F6/04D04H1/56D04H3/007D04H3/16Y10T428/249921Y10T442/30Y10T442/3976Y10T442/60C08L2666/06
    • The instant invention is a polyethylene composition, method of producing the same, fibers made therefrom, and method of making the same. The polyethylene composition according to instant invention comprises: (a) less than or equal to 100 percent by weight of the units derived from ethylene; and (b) less than 20 percent by weight of units derived from one or more α-olefin comonomers. The polyethylene composition according to instant invention has a density in the range of 0.920 to 0.970 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 0.2 to 1000 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the composition. The process for producing the inventive polyethylene composition comprises the steps of: (1) (co)polymerizing ethylene and optionally one or more α-olefin comonomers in the presence of a hafnium based metallocene catalyst via a gas phase (co)polymerization process in a single stage reactor; and (2) thereby producing the polyethylene composition having a density in the range of 0.920 to 0.970 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 0.2 to 1000 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the composition. The fibers according to the instant invention comprise a polyethylene composition comprising: (a) less than or equal to 100 percent by weight of the units derived from ethylene; and (b) less than 20 percent by weight of units derived from one or more α-olefin comonomers; wherein the polyethylene composition has a density in the range of 0.920 to 0.970 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 0.2 to 1000 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the composition. The process for making a fiber according to instant invention comprises the steps of: (1) selecting a polyethylene composition comprising: (a) less than or equal to 100 percent by weight of the units derived from ethylene; and (b) less than 20 percent by weight of units derived from one or more α-olefin comonomers; wherein the polyethylene composition has a density in the range of 0.920 to 0.970 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 0.2 to 1000 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the composition; (2) spinning the polyethylene composition into a fiber; and (3) thereby forming the fiber.