    • 3. 发明授权
    • Process for producing double helical glass tube, light-emitting tube for fluorescent lamp, and fluorescent lamp
    • 生产双螺旋玻璃管,荧光灯发光管和荧光灯的方法
    • US07901264B2
    • 2011-03-08
    • US11909065
    • 2006-03-28
    • Kenji ItayaKenji Nakano
    • Kenji ItayaKenji Nakano
    • H01J9/00
    • C03B23/06C03B23/045C03B23/07H01J9/247
    • A manufacturing method of a double spiral glass tube having a bump that is difficult to break. The manufacturing method includes the steps of: causing the bump forming section (32) in the central portion (13) to have greater tube thickness than the other sections in the glass tube (23) that has been deformed into a double spiral shape; heating and softening part of the bump forming section; and forming a bump (14) by injecting a nitrogen gas (27) into the inner space of the glass tube from both ends thereof to expand the bump forming section. With this structure, the bump forming section is preliminarily formed to have a greater tube thickness than the other sections. As a result, the bump, which is formed by expanding the bump forming section to have a smaller tube thickness than before the expansion, still maintains a sufficient strength.
    • 具有难以断裂的凸块的双螺旋玻璃管的制造方法。 该制造方法包括以下步骤:使中心部分(13)中的凸块形成部分(32)具有比已经变形为双螺旋形状的玻璃管(23)中的其它部分更大的管厚度; 加热和软化凸块形成部分的一部分; 以及通过从其两端向所述玻璃管的内部空间注入氮气(27)并且使所述凸起形成部分膨胀而形成凸块(14)。 利用这种结构,凸起形成部预先形成为具有比其他部分更大的管厚度。 结果,通过使凸块形成部分膨胀成具有比膨胀之前更小的管厚而形成的凸块仍然保持足够的强度。
    • 4. 发明申请
    • PROCESS FOR PRODUCING DOUBLE HELICAL GLASS TUBE, LIGHT-EMITTING TUBE FOR FLUORESCENT LAMP, AND FLUORESCENT LAMP
    • 生产双螺旋玻璃管,荧光灯和荧光灯的发光管
    • US20090021135A1
    • 2009-01-22
    • US11909065
    • 2006-03-28
    • Kenji ItayaKenji Nakano
    • Kenji ItayaKenji Nakano
    • H01J63/04H01J9/00
    • C03B23/06C03B23/045C03B23/07H01J9/247
    • A manufacturing method of a double spiral glass tube having a bump that is difficult to break. The manufacturing method includes the steps of: causing the bump forming section (32) in the central portion (13) to have greater tube thickness than the other sections in the glass tube (23) that has been deformed into a double spiral shape; heating and softening part of the bump forming section; and forming a bump (14) by injecting a nitrogen gas (27) into the inner space of the glass tube from both ends thereof to expand the bump forming section. With this structure, the bump forming section is preliminarily formed to have a greater tube thickness than the other sections. As a result, the bump, which is formed by expanding the bump forming section to have a smaller tube thickness than before the expansion, still maintains a sufficient strength.
    • 具有难以断裂的凸块的双螺旋玻璃管的制造方法。 该制造方法包括以下步骤:使中心部分(13)中的凸块形成部分(32)具有比已经变形为双螺旋形状的玻璃管(23)中的其它部分更大的管厚度; 加热和软化凸块形成部分的一部分; 以及通过从其两端向所述玻璃管的内部空间注入氮气(27)并且使所述凸起形成部分膨胀而形成凸块(14)。 利用这种结构,凸起形成部预先形成为具有比其他部分更大的管厚度。 结果,通过使凸块形成部分膨胀成具有比膨胀之前更小的管厚而形成的凸块仍然保持足够的强度。
    • 8. 发明申请
    • ARC TUBE AND METHOD OF PHOSPHOR COATING
    • 弧管和磷光涂层的方法
    • US20090134771A1
    • 2009-05-28
    • US12064291
    • 2006-11-01
    • Kenji ItayaToyokazu AmanoJunichi Takahashi
    • Kenji ItayaToyokazu AmanoJunichi Takahashi
    • H01J1/62B05D5/06
    • H01J61/327H01J9/223
    • A method of uniformly applying a phosphor onto the internal surface of a glass tube of spiral configuration having opening at its both ends. After an injection process is performed while glass tube (11) is held with openings (24,25) facing upward, the glass tube is turned upside down and held such that the openings are positioned in the inferior region. While rotating the glass tube around pivot axis (A), the phosphor suspension is caused to flow out. The glass tube is turned upside down once more and held to cause the openings to position in the superior region for a given period of time with the result that the phosphor suspension is caused to flow to uniformize the thickness thereof. Further once more the glass tube is turned upside down to cause the openings to position in the inferior region. In that state, a preliminary drying process is performed.
    • 将荧光体均匀地施加到在其两端具有开口的螺旋构造的玻璃管的内表面上的方法。 在玻璃管(11)保持开口(24,25)朝上的同时进行注射处理之后,将玻璃管上下颠倒并保持使得开口位于下部区域。 在围绕枢转轴线(A)旋转玻璃管时,使荧光体悬浮液流出。 将玻璃管再次翻转并保持使开口在上部位置定位一段时间,结果使荧光体悬浮液流动以使其厚度均匀。 此外,再次将玻璃管倒置以使开口位于下部区域中。 在该状态下,进行预干燥处理。