    • 1. 发明专利
    • Production of metallurgical briquette coke
    • 冶金制品的生产
    • JPS54146803A
    • 1979-11-16
    • JP5443578
    • 1978-05-10
    • Keihan Rentan Kogyo KkNippon Kokan Kk
    • IZAWA TETSUOMORI TAKASHIOKUYAMA YASUOHORIGUCHI MASAHIROYANAGIUCHI MAMORUTSUKADA KOUJIARAKI HIDEAKITAKAI SEIZABUROU
    • C10B53/08C10L5/10
    • PURPOSE: To produce metallurgical briquette coke without pollution, by high- temperature carbonization of molded coal which is obtained by blending finely divided coke as a main raw material with finely divided caking coal and a binder.
      CONSTITUTION: A) 50W75 wt. % of finely divided powder coke having particle diameters of about 0.1W0.5 mm as a main raw material is blended with B) 15W 40 wt. % of a caking coal having a particle size similar to that of the coke and a fluidity not less than 1,000 ddpm (Giesler) and C) 3W10 wt. % of a binder, e.g., asphalt deasphalted by propane and pitch, capable of improving a handling strength after molding and a bond strength in a stage of carbonization, to form briquette, which is carbonized at 1000°C. The powdered coke produced in a coke oven is usable as a metallurgical coke required at a iron mill.
      COPYRIGHT: (C)1979,JPO&Japio
    • 目的:通过将细碎焦炭作为主要原料与细碎的结块煤和粘合剂混合而获得的成型煤的高温碳化,生产无污染的冶金团块焦炭。 构成:A)50-75wt。 以粒径约0.1-0.5mm为主要原料的细碎粉末焦炭的百分比与B)15-40重量% %的具有与焦炭相似的粒度的结块煤,流动性不小于1,000dpm(Giesler)和C)3-10wt。 %的粘合剂,例如由丙烷和沥青脱沥青的沥青,能够提高成型后的处理强度和碳化阶段的粘合强度,以形成在1000℃碳化的团块。 在焦炉中生产的焦炭可用作铁厂所需的冶金焦炭。