    • 3. 发明申请
    • Powder for sublayer coating type magnetic recording medium
    • 用于亚层涂层型磁记录介质的粉末
    • US20050129945A1
    • 2005-06-16
    • US10508033
    • 2003-04-02
    • Kazuyuki MatsumotoKenichi InoueKen Inoue
    • Kazuyuki MatsumotoKenichi InoueKen Inoue
    • C01G49/06G11B5/738B32B5/16C09C1/22
    • G11B5/738Y10T428/2982
    • A powder for an underlayer of a coating-type magnetic recording medium, which powder comprises flat-acicular iron oxide particles having an average major axis length of 20-200 nm, a short axis cross-section taken perpendicularly to the long axis that has a long width and a short width, and a short axis cross-section ratio defined as the ratio of the long width to the short width that is greater than 1.3 and substantially uniform in the long axis direction, the powder having a specific surface area measured by the BET method of 30-100 m2/g. The underlayer powder preferably contains 0.1-5.0 wt % of P and, optionally, an amount of R(R representing one or more rare earth elements, defined as including Y) such that R/Fe expressed in atomic percentage (at. %) is 0.1-10 at. %.
    • 一种用于涂层型磁记录介质底层的粉末,该粉末包含平均长轴长度为20-200nm的扁平针状氧化铁颗粒,垂直于长轴的短轴截面为 长宽度和短宽度,短轴截面比定义为长宽与短宽的比大于1.3并且在长轴方向上基本均匀,所述粉末的比表面积由 BET法为30-100m 2 / g。 底层粉末优选含有0.1-5.0重量%的P和任选的R(R表示一个或多个稀土元素,定义为包括Y)的量,使得以原子百分比(at。%)表示的R / Fe为 0.1-10 at。 %。
    • 4. 发明授权
    • Powder for underlayer of coating-type magnetic recording medium
    • 涂层型磁记录介质底层粉末
    • US07238438B2
    • 2007-07-03
    • US10508033
    • 2003-04-02
    • Kazuyuki MatsumotoKenichi InoueKen Inoue
    • Kazuyuki MatsumotoKenichi InoueKen Inoue
    • G11B5/733B32B5/16
    • G11B5/738Y10T428/2982
    • A powder for an underlayer of a coating-type magnetic recording medium, which powder comprises flat-acicular iron oxide particles having an average major axis length of 20–200 nm, a short axis cross-section taken perpendicularly to the long axis that has a long width and a short width, and a short axis cross-section ratio defined as the ratio of the long width to the short width that is greater than 1.3 and substantially uniform in the long axis direction, the powder having a specific surface area measured by the BET method of 30–100 m2/g. The underlayer powder preferably contains 0.1–5.0 wt % of P and, optionally, an amount of R(R representing one or more rare earth elements, defined as including Y) such that R/Fe expressed in atomic percentage (at. %) is 0.1–10 at. %.
    • 一种用于涂层型磁记录介质底层的粉末,该粉末包含平均长轴长度为20-200nm的扁平针状氧化铁颗粒,垂直于长轴的短轴截面为 长宽度和短宽度,短轴截面比定义为长宽与短宽的比大于1.3并且在长轴方向上基本均匀,所述粉末的比表面积由 BET法为30-100m 2 / g。 底层粉末优选含有0.1-5.0重量%的P和任选的R(R表示一个或多个稀土元素,定义为包括Y)的量,使得以原子百分比(at。%)表示的R / Fe为 0.1-10 at。 %。
    • 10. 发明授权
    • Member used for casting
    • 会员用于铸造
    • US07159640B2
    • 2007-01-09
    • US11198167
    • 2005-08-08
    • Kenichi InoueKen Inoue
    • Kenichi InoueKen Inoue
    • B22C3/00
    • C23C14/0641B22D17/2209C23C14/06C23C28/044
    • A casting member comprising hot-die steel or high-speed steel as base material and having coating layers at least on its working plane, wherein the outermost layer among the coating layers consists essentially of at least one nitride, oxinitride or carnonitride composed mainly of V, and another coating layer comprising at least one nitride, oxinitride or carnonitride composed mainly of Cr is formed as a layer just above the base material. If necessary, an intermediate layer comprising at least one nitride, oxinitride or carnonitride composed mainly of V and Cr may be formed as a coating layer on the boundary surface between the outermost layer and the layer just above the base material. The thickness of the outermost layer is preferably 0.5 to 5.0 μm, the thickness of the layer just above the base material is preferably 0.5 to 3.0 μm, and the thickness of the intermediate layer is preferably 1.0 μm or less. Said casting member has excellent resistance to seizure, resistance to cracking and resistance to waste by melting.
    • 一种浇铸构件,其包括热模钢或高速钢作为基材并且至少在其工作平面上具有涂层,其中涂层中的最外层基本上由至少一种主要由V形成的氮化物,氮化物或碳氮化物组成 ,并且在基材的正上方形成包含至少一种主要由Cr组成的氮化物,氮氧化物或碳氮化物的另一涂层。 如果需要,可以在最外层和刚好在基材上方的层之间的边界表面上形成包含至少一种主要由V和Cr组成的氮化物,氮氧化物或碳氮化物的中间层作为涂层。 最外层的厚度优选为0.5〜5.0μm,刚好在基材上方的层的厚度优选为0.5〜3.0μm,中间层的厚度优选为1.0μm以下。 所述浇铸构件具有优异的抗咬合性,耐开裂性和耐熔融性。