    • Polyolefin rubbers and process for their preparation
    • 聚烯烃橡胶及其制备方法
    • US5318849A
    • 1994-06-07
    • US720770
    • 1991-07-29
    • Hacene MehallaBrigitte Morese-SeguelaPatrice Breant
    • Hacene MehallaBrigitte Morese-SeguelaPatrice Breant
    • C08F4/62C08F4/60C08F210/16C08L23/16B32B25/04C08F210/08
    • C08F210/16Y10T428/2982Y10T428/2998Y10T428/31663Y10T428/31938
    • Polyolefin rubber which is an ethylene/propylene and/or 1-butene copolymer, which has a melt index of 0.3 to 15 dg/min and a relative density of 0.860 to 0.885, comprising 74-91 mol % of units derived from ethylene and 9-26 mol % of units derived from propylene and/or from 1-butene, characterised by a crystalline melting point J of 100.degree. to 125.degree. C. The process for obtaining this rubber consists in copolymerising, at a temperature of 150.degree.-300.degree. C. and at a pressure of 400-2000 bars, a gas stream containing 15-42% by vol. of ethylene and 58-85% by vol. of propylene and/or 1-butene, in the presence of a Ziegler-type catalyst system comprising at least one compound of a transition metal of groups IVB, VB, VIB and VIII of the Periodic Classification, and at least one organoaluminium compound and, if appropriate, in the presence of at least one chain transfer agent. Manufacture of articles such as seals, shoe components, flexible tubing, damping components, profiles for buildings and motor vehicles, and the like.
    • PCT No.PCT / FR90 / 00801 Sec。 371日期1991年7月29日 102(e)日期1991年7月29日PCT 1990年11月8日PCT PCT。 公开号WO91 / 07447 日期:1991年5月30日。作为乙烯/丙烯和/或1-丁烯共聚物的聚烯烃橡胶,其熔体指数为0.3〜15dg / min,相对密度为0.860〜0.885,包含74-91mol% 衍生自乙烯的单元和9-26mol%衍生自丙烯和/或1-丁烯的单元,其特征在于结晶熔点为100-125℃。获得该橡胶的方法包括在 温度为150-300℃,压力为400-2000巴,含有15-42%(体积)的气流。 的乙烯和58-85%的乙烯。 丙烯和/或1-丁烯的存在下,在包含至少一种元素周期表IVB,VB,VIB和VIII族过渡金属化合物的齐格勒型催化剂体系存在下,和至少一种有机铝化合物, 如果合适的话,在存在至少一种链转移剂的情况下。 诸如密封件,鞋子部件,柔性管,阻尼部件,建筑物和机动车辆的轮廓等物品的制造等。