热词
    • 2. 发明专利
    • Method and apparatus for operating air dehumidifier
    • 用于运行空气除湿器的方法和装置
    • JP2007260606A
    • 2007-10-11
    • JP2006091220
    • 2006-03-29
    • Jfe Steel KkJfeスチール株式会社
    • OKAMOTO KENMIDORIKAWA SATORUSUZUKI KEIJI
    • B01D53/26
    • PROBLEM TO BE SOLVED: To provide a method and an apparatus for operating air dehumidifier capable of reducing electric power for operating an air dehumidifier for obtaining air used for removal of moisture and oil on the surface of steel tape or else. SOLUTION: The method for operating air dehumidifier is characterized in that operation and stoppage are performed in accordance with detection values and target values by detecting the dew point of air in inlet side in the air dehumidifier 1, wherein the target values of the operation and stoppage may be set on the low side. The apparatus for operating air dehumidifier is provided with a dew point meter 4 disposed in the middle of an inlet side air piping 2 and a start-up/stoppage switch 5 which performs the operation and stoppage of the air dehumidifier 1 in accordance with the value of the dew point meter 4, with respect to the air dehumidifier 1 provided with the inlet side air piping 2 and an outlet side air piping 3 attached to an inlet and an outlet of the air dehumidifier 1, wherein a timer 7 may be disposed between the start-up/stoppage switch 5 and the air dehumidifier. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种用于操作空气除湿器的方法和装置,其能够降低用于操作空气除湿器的电力,以获得用于除去钢带表面上的水分和油的空气。 解决方案:空气除湿器的操作方法的特征在于,通过检测空气除湿器1的入口侧的空气的露点,根据检测值和目标值进行操作和停止,其中, 操作和停止可能设置在低端。 用于操作空气除湿器的设备设置有设置在入口侧空气管路2的中间的露点计4和启动/停止开关5,其根据该值执行除湿器1的操作和停止 露点计4相对于设置有入口侧空气管路2的空气除湿器1和连接到空气除湿器1的入口和出口的出口侧空气管路3,其中定时器7可以设置在露点计4之间。 启动/停止开关5和空气除湿器。 版权所有(C)2008,JPO&INPIT
    • 3. 发明专利
    • Method for removing surface foreign matter of pickling hot rolled steel sheet
    • 去除热轧钢板表面外观的方法
    • JP2005270997A
    • 2005-10-06
    • JP2004084531
    • 2004-03-23
    • Jfe Steel KkJfeスチール株式会社
    • SUZUKI KEIJIIMAI HISAO
    • B24C1/00B21B45/02B21B45/06
    • PROBLEM TO BE SOLVED: To provide a method for efficiently removing, without impairing productivity, foreign matters that remain sticking to the surface of a pickling hot rolled steel sheet after pickling, that come from hardly dissolving metallic pieces peeled and stuck from a metallic roll at the time of mechanical descaling prior to a pickling process, or that come from rubber pieces peeled and stuck from a dewatering rubber roll arranged in the front and the rear of a pickling tank.
      SOLUTION: The pickling hot rolled steel sheet is processed by shot blasting for the purpose of removing foreign matters stuck to the surface. The pickling hot rolled steel sheet can be the one passed through a mechanical descaling device including a tension leveler before pickling or the one passed through a rubber lining roll or a plastic lining roll.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种在不损害生产率的情况下有效地去除在酸洗后的酸洗热轧钢板表面残留的异物,其是从几乎不溶解的金属片剥离并从 在酸洗过程之前机械除锈时的金属辊,或者是从设置在酸洗槽的前后的脱水橡胶辊剥离并粘贴的橡胶片。 解决方案:酸洗热轧钢板为了除去粘附在表面上的异物,通过喷砂处理。 酸洗热轧钢板可以是通过包括酸洗前的张力矫直机或通过橡胶衬里辊或塑料衬里辊的机械除垢装置的机器除锈装置。 版权所有(C)2006,JPO&NCIPI
    • 5. 发明专利
    • Tension leveler and method for controlling width of metallic sheet using the same
    • 用于控制金属片的宽度的张力调节器和方法
    • JP2006122975A
    • 2006-05-18
    • JP2004316265
    • 2004-10-29
    • Jfe Steel KkJfeスチール株式会社
    • KIJIMA HIDEOSOTANI YASUHIROSUZUKI KEIJI
    • B21D1/05
    • PROBLEM TO BE SOLVED: To provide a tension leveler with which the width of a metallic sheet is efficiently controlled and a controlling method of the width of the metallic sheet by which yield is improved by reducing a trimming allowance by controlling so as to approach a constant width as much as possible by absorbing width variation which is generated by the last stage by changing the width of the metallic sheet by using the tension leveler.
      SOLUTION: A work roll 10 of the tension leveler is made into a cylindrical roll having a hollow part 15 in its interior, a liquid supply port 14 for supplying the liquid such as water and lubricating oil to the hollow part 15 is provided in a neck part 12 and also a lot of liquid jetting holes 13 extended from the hollow part 15 are zigzag arranged on the outer peripheral surface 11a of the roll barrel part 11. In this way, the liquid which is supplied from the liquid supply port 14 in the neck part 12 is fed to the liquid jetting holes 13 through the hollow part 15 and jetted from the outer peripheral surface 11a of the roll barrel 11.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种能够有效控制金属板的宽度的张力矫直机以及金属板的宽度的控制方法,通过控制以减少修整余量来提高成品率,从而 通过吸收通过使用张力矫直机改变金属片的宽度的最后阶段产生的宽度变化,尽可能接近恒定的宽度。 解决方案:将张力矫直机的工作辊10制成在其内部具有中空部分15的圆柱形辊中,提供用于将诸如水和润滑油的液体供应到中空部分15的液体供应口14 在颈部12中,并且从中空部15延伸的大量液体喷射孔13也被设置在辊筒部11的外周面11a上。这样,从液体供给口供给的液体 颈部12的中空部分14通过中空部分15被供给到液体喷射孔13并从辊筒11的外周表面11a喷射。(C)2006年,JPO&NCIPI
    • 6. 发明专利
    • Rolling control method for continuous cold- rolling mill
    • 连续冷轧机的轧制控制方法
    • JP2005066641A
    • 2005-03-17
    • JP2003299630
    • 2003-08-25
    • Jfe Steel KkJfeスチール株式会社
    • SUZUKI KEIJIIMAI HISAOOZAKI MASAYUKI
    • B21B37/38B21B37/00
    • PROBLEM TO BE SOLVED: To provide a rolling control method for a continuous cold-rolling mill. SOLUTION: When continuously rolling materials to be rolled the leading and the rear end of which are joined by welding by using a rolling mill provided with a roll bending device which is a roll bending device for imparting bending force to a work roll and which can be subjected to control by which difference between the bending forces imparted to one shaft end and the other shaft end of the work roll is giveable, before rolling the weld point where the leading and the rear end of the materials to be rolled are joined, rolling is performed by stopping the control by which the difference between the bending forces imparted to the work roll is giveable and controlling so that the difference between the bending forces becomes zero. After that, rolling is performed by restarting the control by which the difference between the bending forces imparted to the work roll is giveable when rolling the weld point. COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供连续冷轧机的轧制控制方法。 解决方案:通过使用具有辊弯曲装置的轧机连续轧制其前端和后端通过焊接而接合的材料,所述辊弯曲装置是用于向工作辊施加弯曲力的辊弯曲装置, 在轧制要被轧制的材料的前端和后端的焊接点被接合之前,可以进行控制,由此赋予一个轴端的弯曲力与工作辊的另一个轴端之间的差异是可以赋予​​的 通过停止赋予工作辊的弯曲力之间的差异的控制来进行轧制,并且控制使得弯曲力之间的差变为零。 之后,通过重新开始轧制焊接点时施加给工作辊的弯曲力之间的差异可以赋予的控制来进行轧制。 版权所有(C)2005,JPO&NCIPI