    • 5. 发明专利
    • Method for producing artificial lightweight aggregate
    • 生产人造光聚集体的方法
    • JP2003012354A
    • 2003-01-15
    • JP2001192838
    • 2001-06-26
    • Taiheiyo Cement Corp太平洋セメント株式会社
    • NANBU MASAMITSU
    • C04B14/02C04B18/08C04B20/04C04B20/06C04B38/00
    • C04B20/061C04B18/08C04B38/009C04B2111/40Y02W30/92
    • PROBLEM TO BE SOLVED: To solve such problems in the production of an artificial lightweight aggregate using fly ash, etc., containing unburned carbonaceous material as raw materials by conventional rotary kiln that production efficiency and thermal efficiency lower and breakage of pellets occurs.
      SOLUTION: In the method for producing artificial lightweight aggregate, burning of inflammable matter included in the aggregate raw material P is carried out using a tunnel kiln 2, and firing of the aggregate raw material P discharged from the tunnel kiln 2 is carried out using a rotary kiln 3. It is preferable that ≥80 wt.% of the inflammable matter included in the aggregate raw material P is burned using the tunnel kiln, and that burning of the inflammable matter included in the aggregate raw material P is carried out by utilizing flue gas from the rotary kiln 3.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题为了解决生产效率和热效率降低和颗粒破裂的常规回转窑生产含有未燃碳质材料作为原料的飞灰等的人造轻骨料生产中的问题。 解决方案:在生产人造轻质骨料的方法中,使用隧道窑2进行包含在聚集体原料P中的易燃物质的燃烧,并且使用以下方法进行从隧道窑2排出的骨料原料P的烧成 回转窑3.优选使用隧道窑将包含在集料原料P中的≥80重量%的易燃物质燃烧,并且包含在集料原料P中的易燃物质的燃烧由 利用回转窑3的烟道气。
    • 8. 发明专利
    • PRODUCTION OF ARTIFICIAL LIGHTWEIGHT AGGREGATE
    • JP2000272942A
    • 2000-10-03
    • JP8168699
    • 1999-03-25
    • TAIHEIYO CEMENT CORP
    • UEYASU TOMONOBUNANBU MASAMITSUSUGAYA TOMOYUKIHARADA YOSHIKATSUIZAWA YASUOTERAMITSU YASUBUMI
    • B09B3/00C04B14/02C04B18/02C04B18/16C04B38/08
    • PROBLEM TO BE SOLVED: To obtain an aggregate having low water absorption regardless of a low specific gravity, and hardly causing wearing out at the time of kneading of a concrete by milling a waste glass, a binder and a foaming agent so as to have a specific average particle diameter, granulating the milled product, and firing the granulated product. SOLUTION: A flat glass, a bottle glass or the like is cited as the waste glass, and the amount to be formulated is 80-98.9 wt.% based on the whole amount of the raw material. A clayey mineral such as a bentonite, a chlorite and a sericite is cited as the binder, and the bentonite is preferable. The amount to be formulated can be changed according to the average particle diameter of the raw material, but in the range of 1-10 wt.% based on the whole amount of the raw material. Silicon carbide, calcium carbonate, calcium sulfate or the like is used as the foaming agent and the amount to be formulated is 0.01-2 wt.% based on the whole amount of the raw material. These raw materials are pulverized so as to have 15-50 μm average particle diameter, and the pulverized product is kneaded and granulated with a proper amount of added water. The obtained granules is fired to provide the objective aggregate. The firing temperature is preferably 700-900 deg.C, and the particle diameter of the aggregate is preferably 5-20 mm.