    • 4. 发明公开
    • WELDED STEEL PIPE WELDED WITH A HIGH ENERGY DENSITY BEAM, AND A MANUFACTURING METHOD THEREFOR
    • 与用于生产高能量密度焊接钢管和处理JET
    • EP2258493A4
    • 2013-12-25
    • EP09727339
    • 2009-03-30
    • JFE STEEL CORP
    • YANO KOJIOI KENJI
    • B21C37/30B21C37/08B23K13/04B23K26/20B23K26/26B23K31/00B23K37/08
    • F16L9/02B21C37/0811B23K13/046B23K26/262B23K2201/06B23K2203/04B23K2203/05
    • Provided are a welded steel pipe that is joined with a high-energy-density beam so that there are no welding defects in the seam, and a method for efficiently producing the welded steel pipe. Specifically, a steel strip is formed into a cylinder so that opposite ends of the steel strip face each other, while continuously conveying the steel strip, the opposite ends are melted across the entire thickness by irradiating the opposite ends with a high-energy-density beam while applying a pressure with squeeze rolls, a seam is formed by joining the opposite ends, excess weld metal of the seam on the outer side and the inner side of the obtained welded steel pipe is removed by cutting, a repaired seam is then formed by remelting and solidifying a region on the inner side of the welded steel pipe, the region having a depth of 0.5 mm or more from the surface and a width of double or more the width of the seam, and in addition, the center line of the seam is made to coincide with the center line of the repaired seam.
    • 本发明提供一种焊接钢管并接合用高密度能量束,从而thatthere是在接缝没有焊接缺陷,以及用于有效地生产焊接钢管的方法。 具体而言,钢带形成为圆筒所以做了钢带的相对端通过用高能量密度照射两端面对海誓山盟,同时连续输送钢带,相对端在整个厚度熔融 束,同时施加与挤压辊压力,接缝是通过将相对的端部形成的,在外侧,将得到的焊接钢管的内侧的接缝的过量的焊接金属被通过切割除去,一个接缝修补然后形成 通过对焊接钢管的内侧再熔化并固化的区域中,具有0.5mm以上从表面的深度和接缝的双或更多宽度的宽度,此外,中心线的区域 接缝被制成与所述接缝修补部的中心线一致。
    • 7. 发明公开
    • METHOD FOR PRODUCING LASER-WELDED STEEL TUBE
    • 生产激光焊接钢管的方法
    • EP2692476A4
    • 2015-07-15
    • EP11862698
    • 2011-04-28
    • JFE STEEL CORP
    • YANO KOJISUMI HIROYUKIOI KENJI
    • B23K26/20B21C37/08B23K26/00B23K26/04B23K26/067
    • B23K26/282B21C37/08B23K26/0608B23K26/262B23K26/32B23K2203/04B23K2203/50
    • Provided is a method of stably manufacturing a laser welded steel pipe having a high quality weld portion at a high yield ratio by laser welding while a typical problem of the laser welding of frequent occurrence of undercut or underfill is solved. Specifically, a method of manufacturing a laser welded steel pipe by forming a steel strip into a cylindrical open pipe with forming rolls and performing laser welding on edges of the open pipe by emitting a laser beam while pressing the edges with squeeze rolls, the laser welding including: emitting two laser beams along the edges from an upper surface side of the open pipe, the two laser beams being transmitted through different optical fibers and having in-focus spot diameters exceeding 0.3 mm; emitting the laser beams such that a leading laser beam of the two laser beams and a trailing laser beam of the two laser beams are each inclined toward a direction in which welding proceeds at an incident angle with respect to a direction perpendicular to an upper surface of the open pipe, the leading laser beam being ahead of the trailing laser beam on the upper surface of the open pipe in the direction in which welding proceeds, the trailing laser beam being behind the leading laser beam; setting the incident angle of the leading laser beam to be larger than the incident angle of the trailing laser beam; and setting a gap between a center point of the leading laser beam and a center point of the trailing laser beam on a back surface of the open pipe to 1 mm or larger.