    • AROMATIC POLYAMIDE FILAMENT AND METHOD OF MANUFACTURING THE SAME
    • 芳香族聚酰胺纤维及其制造方法
    • US20100237532A1
    • 2010-09-23
    • US12792304
    • 2010-06-02
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • B29C47/08
    • D01F6/605B01F7/00766B01F2215/0454C08G69/32Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized in that, in the process of preparing the wholly aromatic polyamide polymer, the aromatic diamine, aromatic diacid chloride and polymerization solvent put into the reactor 20 are agitated by an agitation device which is installed in the reactor 20 and consists of: (i) a rotor 3 driven by a motor 2 and having a plurality of pins 3a; and (ii) a stator 4 having a plurality of pins 4a, wherein spin speed of the rotor 3 is controlled to 10 to 100 times of both of feeding rates for the aromatic diacid chloride and the aromatic diamine in the polymerization solvent into the reactor and, at the same time, contact frequency between the pins 3a and the pins 4a is regulated within a range of 100 to 1,000 Hz. The present invention is effective to progress uniform and homogeneous polymerization over all of area of a polymerization reactor 20, thereby reducing deviation in degree of polymerization, since polymeric monomers are miscible and react together very well in the reactor 20. Accordingly, the wholly aromatic polyamide filament produced exhibits narrow PDI and lowered paracrystalline parameter gII leading to reduction of defects of a crystal itself, so as to considerably improve strength and modulus thereof.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,在制备全芳香族聚酰胺聚合物的方法中,通过搅拌装置搅拌加入到反应器20中的芳族二胺,芳族二酰氯和聚合溶剂 其安装在反应器20中并且包括:(i)由电动机2驱动并具有多个销3a的转子3; 和(ii)具有多个销4a的定子4,其中转子3的旋转速度被控制在聚合溶剂中的芳族二酰氯和芳族二胺的进料速率的两倍到反应器中的10至100倍, 同时,引脚3a和引脚4a之间的接触频率调节在100至1000Hz的范围内。 本发明有效地在聚合反应器20的所有区域上进行均匀均匀的聚合,由此降低聚合度的偏差,因为聚合物单体是可混溶的并且在反应器20中非常好地反应。因此,全芳族聚酰胺 所生产的长丝表现出窄的PDI和降低的结晶参数gII,导致晶体本身缺陷的减少,从而显着提高其强度和模量。
    • 2. 发明授权
    • Process of making aromatic polyamide filament
    • 制备芳香族聚酰胺丝的工艺
    • US08419990B2
    • 2013-04-16
    • US12792304
    • 2010-06-02
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • B01F7/16C08F2/06C08G69/26D01D5/06D01F6/60
    • D01F6/605B01F7/00766B01F2215/0454C08G69/32Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized in that, in the process of preparing the wholly aromatic polyamide polymer, the aromatic diamine, aromatic diacid chloride and polymerization solvent put into the reactor 20 are agitated by an agitation device which is installed in the reactor 20 and consists of: (i) a rotor 3 driven by a motor 2 and having a plurality of pins 3a; and (ii) a stator 4 having a plurality of pins 4a, wherein spin speed of the rotor 3 is controlled to 10 to 100 times of both of feeding rates for the aromatic diacid chloride and the aromatic diamine in the polymerization solvent into the reactor and, at the same time, contact frequency between the pins 3a and the pins 4a is regulated within a range of 100 to 1,000 Hz. The present invention is effective to progress uniform and homogeneous polymerization over all of area of a polymerization reactor 20, thereby reducing deviation in degree of polymerization, since polymeric monomers are miscible and react together very well in the reactor 20. Accordingly, the wholly aromatic polyamide filament produced exhibits narrow PDI and lowered paracrystalline parameter gII leading to reduction of defects of a crystal itself, so as to considerably improve strength and modulus thereof.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,在制备全芳香族聚酰胺聚合物的方法中,通过搅拌装置搅拌加入到反应器20中的芳族二胺,芳族二酰氯和聚合溶剂 其安装在反应器20中并且包括:(i)由电动机2驱动并具有多个销3a的转子3; 和(ii)具有多个销4a的定子4,其中转子3的旋转速度被控制在聚合溶剂中的芳族二酰氯和芳族二胺的进料速率的两倍到反应器中的10至100倍, 同时,引脚3a和引脚4a之间的接触频率调节在100至1000Hz的范围内。 本发明有效地在聚合反应器20的所有区域上进行均匀均匀的聚合,由此降低聚合度的偏差,因为聚合物单体是可混溶的并且在反应器20中非常好地反应。因此,全芳族聚酰胺 所生产的长丝表现出窄的PDI和降低的结晶参数gII,导致晶体本身缺陷的减少,从而显着提高其强度和模量。
    • 3. 发明申请
    • Aromatic Polyamide Filament and Method of Manufacturing the Same
    • 芳香族聚酰胺丝及其制造方法
    • US20080227947A1
    • 2008-09-18
    • US11994642
    • 2006-07-05
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • D01F6/60C08G69/28
    • D01F6/605B01F7/00766B01F2215/0454C08G69/32Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized in that, in the process of preparing the wholly aromatic polyamide polymer, the aromatic diamine, aromatic diacid chlrodie and polymerization solvent put into the reactor 20 are agitated by an agitation device which is installed in the reactor 20 and consists of: (i) a rotor 3 driven by a motor 2 and having a plurality of pins 3a; and (ii) a stator 4 having a plurality of pins 4a, wherein spin speed of the rotor 3 is controlled to 10 to 100 times of both of feeding rates for the aromatic diacid chloride and the aromatic diamine in the polymerization solvent into the reactor and, at the same time, contact frequency between the pins 3a and the pins 4a is regulated within a range of 100 to 1,000 Hz. The present invention is effective to progress uniform and homogeneous polymerization over all of area of a polymerization reactor 20, thereby reducing deviation in degree of polymerization, since polymeric monomers are miscible and react together very well in the reactor 20. Accordingly, the wholly aromatic polyamide filament produced exhibits narrow PDI and lowered paracrystalline parameter gII leading to reduction of defects of a crystal itself, so as to considerably improve strength and modulus thereof.
    • 公开了全芳族聚酰胺长丝及其制造方法,其特征在于,在制备全芳香族聚酰胺聚合物的方法中,通过搅拌装置搅拌放入反应器20中的芳族二胺,芳族二酸氯乙烯和聚合溶剂 其安装在反应器20中并且包括:(i)由电动机2驱动并具有多个销3a的转子3; 和(ii)具有多个销4a的定子4,其中转子3的旋转速度被控制在聚合溶剂中的芳族二酰氯和芳族二胺的进料速率的两倍至反应器的10到100倍 并且同时,引脚3a和引脚4a之间的接触频率被调节在100至1000Hz的范围内。 本发明有效地在聚合反应器20的所有区域上进行均匀均匀的聚合,由此降低聚合度的偏差,因为聚合物单体是可混溶的并且在反应器20中非常好地反应。因此,全芳族聚酰胺 产生的长丝表现出窄的PDI和降低的结晶参数g II II导致晶体本身缺陷的减少,从而显着提高其强度和模量。
    • 4. 发明授权
    • Aromatic polyamide filament and method of manufacturing the same
    • 芳香族聚酰胺丝及其制造方法
    • US07776439B2
    • 2010-08-17
    • US11994642
    • 2006-07-05
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • In-Sik HanJae-Young LeeJae-Young KimTae-Hak ParkSo-Yeon Kwon
    • D02G3/00
    • D01F6/605B01F7/00766B01F2215/0454C08G69/32Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized in that, in the process of preparing the wholly aromatic polyamide polymer, the aromatic diamine, aromatic diacid chloride and polymerization solvent put into the reactor 20 are agitated by an agitation device which is installed in the reactor 20 and consists of: (i) a rotor 3 driven by a motor 2 and having a plurality of pins 3a; and (ii) a stator 4 having a plurality of pins 4a, wherein spin speed of the rotor 3 is controlled to 10 to 100 times of both of feeding rates for the aromatic diacid chloride and the aromatic diamine in the polymerization solvent into the reactor and, at the same time, contact frequency between the pins 3a and the pins 4a is regulated within a range of 100 to 1,000 Hz. The present invention is effective to progress uniform and homogeneous polymerization over all of area of a polymerization reactor 20, thereby reducing deviation in degree of polymerization, since polymeric monomers are miscible and react together very well in the reactor 20. Accordingly, the wholly aromatic polyamide filament produced exhibits narrow PDI and lowered paracrystalline parameter gII leading to reduction of defects of a crystal itself, so as to considerably improve strength and modulus thereof.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,在制备全芳香族聚酰胺聚合物的方法中,通过搅拌装置搅拌加入到反应器20中的芳族二胺,芳族二酰氯和聚合溶剂 其安装在反应器20中并且包括:(i)由电动机2驱动并具有多个销3a的转子3; 和(ii)具有多个销4a的定子4,其中转子3的旋转速度被控制在聚合溶剂中的芳族二酰氯和芳族二胺的进料速率的两倍到反应器中的10至100倍, 同时,引脚3a和引脚4a之间的接触频率调节在100至1000Hz的范围内。 本发明有效地在聚合反应器20的所有区域上均匀均匀聚合,从而降低聚合度的偏差,因为聚合物单体是可混溶的,并且在反应器20中非常好地反应。因此,全芳族聚酰胺 所生产的长丝表现出窄的PDI和降低的结晶参数gII,导致晶体本身缺陷的减少,从而显着提高其强度和模量。
    • 5. 发明授权
    • Process of making wholly aromatic polyamide filament
    • 制造全芳香族聚酰胺丝的工艺
    • US08834755B2
    • 2014-09-16
    • US12792225
    • 2010-06-02
    • In-Sik HanJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • In-Sik HanJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • D01F13/04D01D5/06D01F6/60
    • D01F6/605D01D5/06Y02P20/582Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized by comprising multi-stage injection of a coagulant with sulfuric acid concentration lowered sequentially stage by stage, to a spun material fed into a coagulant injection tank. The present invention enables increase of a spinning and take-up velocity without occurrence of thread cutting by uniformly and evenly coagulating surface and inside of the spun material. In addition, the present invention recovers the coagulant or water already used and reuses the recovered coagulant or water in the earlier stages, so that it has advantages of saving production costs and reducing environmental contamination. Accordingly, the wholly aromatic polyamide filament produced according to the present invention has high crystallinity X, large apparent crystal size ACS and reduced defects in the crystal itself, thereby exhibiting more improved physical properties such as strength and modulus.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,包括多阶段将硫酸浓度逐级降低的凝结剂注入供给到凝结剂注入槽中的纺丝材料。 本发明通过使纺丝材料的表面和内部均匀均匀地凝固,能够提高纺丝和卷取速度,而不会产生螺纹切割。 此外,本发明回收已经使用的凝结剂或水,并且在早期阶段重新使用回收的凝结剂或水,从而具有节省生产成本和减少环境污染的优点。 因此,根据本发明生产的全芳族聚酰胺长丝具有高结晶度X,大的表观晶体尺寸ACS,并减少了晶体本身的缺陷,从而表现出更好的物理性能如强度和模量。
    • 6. 发明授权
    • Aromatic polyamide filament and method of manufacturing the same
    • 芳香族聚酰胺丝及其制造方法
    • US07851061B2
    • 2010-12-14
    • US11994641
    • 2006-07-05
    • In-Sik HanJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • In-Sik HanJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • D02G3/00
    • D01F6/605D01D5/06Y02P20/582Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized by comprising multi-stage injection of a coagulant with sulfuric acid concentration lowered sequentially stage by stage, to a spun material fed into a coagulant injection tank. The present invention enables increase of a spinning and take-up velocity without occurrence of thread cutting by uniformly and evenly coagulating surface and inside of the spun material. In addition, the present invention recovers the coagulant or water already used and reuses the recovered coagulant or water in the earlier stages, so that it has advantages of saving production costs and reducing environmental contamination. Accordingly, the wholly aromatic polyamide filament produced according to the present invention has high crystallinity X, large apparent crystal size ACS and reduced defects in the crystal itself, thereby exhibiting more improved physical properties such as strength and modulus.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,包括多阶段将硫酸浓度逐级降低的凝结剂注入供给到凝结剂注入槽中的纺丝材料。 本发明通过使纺丝材料的表面和内部均匀均匀地凝固,能够提高纺丝和卷取速度,而不会产生螺纹切割。 此外,本发明回收已经使用的凝结剂或水,并且在早期阶段重新使用回收的凝结剂或水,从而具有节省生产成本和减少环境污染的优点。 因此,根据本发明生产的全芳族聚酰胺长丝具有高结晶度X,大的表观晶体尺寸ACS,并减少了晶体本身的缺陷,从而表现出更好的物理性能如强度和模量。
    • 7. 发明申请
    • Aromatic Polyamide Filament And Method Of Manufacturing The Same
    • 芳香族聚酰胺丝及其制造方法
    • US20080200640A1
    • 2008-08-21
    • US11994641
    • 2006-07-05
    • In-Sik HanJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • In-Sik HanJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • D01F6/60C08G69/26
    • D01F6/605D01D5/06Y02P20/582Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized by comprising multi-stage injection of a coagulant with sulfuric acid concentration lowered sequentially stage by stage, to a spun material fed into a coagulant injection tank. The present invention enables increase of a spinning and take-up velocity without occurrence of thread cutting by uniformly and evenly coagulating surface and inside of the spun material. In addition, the present invention recovers the coagulant or water already used and reuses the recovered coagulant or water in the earlier stages, so that it has advantages of saving production costs and reducing environmental contamination. Accordingly, the wholly aromatic polyamide filament produced according to the present invention has high crystallinity X, large apparent crystal size ACS and reduced defects in the crystal itself, thereby exhibiting more improved physical properties such as strength and modulus.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,包括多阶段将硫酸浓度逐级降低的凝结剂注入供给到凝结剂注入槽中的纺丝材料。 本发明通过使纺丝材料的表面和内部均匀均匀地凝固,能够提高纺丝和卷取速度,而不会产生螺纹切割。 此外,本发明回收已经使用的凝结剂或水,并且在早期阶段重新使用回收的凝结剂或水,从而具有节省生产成本和减少环境污染的优点。 因此,根据本发明生产的全芳族聚酰胺长丝具有高结晶度X,大的表观晶体尺寸ACS,并减少了晶体本身的缺陷,从而表现出更好的物理性能如强度和模量。
    • 8. 发明申请
    • AROMATIC POLYAMIDE FILAMENT AND METHOD OF MANUFACTURING THE SAME
    • 芳香族聚酰胺纤维及其制造方法
    • US20100301516A1
    • 2010-12-02
    • US12792225
    • 2010-06-02
    • In-Sik HANJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • In-Sik HANJae-Young LeeSeung-Hwan LeeJae-Young KimSo-Yeon Kwon
    • D01F1/10
    • D01F6/605D01D5/06Y02P20/582Y10T428/2913Y10T428/2969
    • Disclosed are wholly aromatic polyamide filament and a method of manufacturing the same, characterized by comprising multi-stage injection of a coagulant with sulfuric acid concentration lowered sequentially stage by stage, to a spun material fed into a coagulant injection tank. The present invention enables increase of a spinning and take-up velocity without occurrence of thread cutting by uniformly and evenly coagulating surface and inside of the spun material. In addition, the present invention recovers the coagulant or water already used and reuses the recovered coagulant or water in the earlier stages, so that it has advantages of saving production costs and reducing environmental contamination. Accordingly, the wholly aromatic polyamide filament produced according to the present invention has high crystallinity X, large apparent crystal size ACS and reduced defects in the crystal itself, thereby exhibiting more improved physical properties such as strength and modulus.
    • 公开了全芳香族聚酰胺长丝及其制造方法,其特征在于,包括多阶段将硫酸浓度逐级降低的凝结剂注入供给到凝结剂注入槽中的纺丝材料。 本发明通过使纺丝材料的表面和内部均匀均匀地凝固,能够提高纺丝和卷取速度,而不会产生螺纹切割。 此外,本发明回收已经使用的凝结剂或水,并且在早期阶段重新使用回收的凝结剂或水,从而具有节省生产成本和减少环境污染的优点。 因此,根据本发明生产的全芳族聚酰胺长丝具有高结晶度X,大的表观晶体尺寸ACS,并减少了晶体本身的缺陷,从而表现出更好的物理性能如强度和模量。