热词
    • 3. 发明专利
    • Raw-material composition for resin for optical part, resin for optical part, and optical part
    • 用于光学部件,光学部件和光学部件的树脂的树脂原料组合物
    • JP2010163610A
    • 2010-07-29
    • JP2009284356
    • 2009-12-15
    • Idemitsu Kosan Co Ltd出光興産株式会社
    • OBATA HIROSHIIWASAKI TAKESHITAKEBE TOMOAKI
    • C08F220/10C08K5/04C08L33/04G02B1/04
    • PROBLEM TO BE SOLVED: To provide a raw-material composition for producing a resin for an optical part having excellent transparency, developing no cracks, and being excellent in shape stability, stable to heat to show no yellowing, and excellent also in mold releasability, and an optical part.
      SOLUTION: The raw-material composition for a resin for an optical part comprises an adamantyl group-containing (meth)acrylate compound (A) having a specific structure, a low molecular weight (meth)acrylate compound (B) having a specific structure, and an aliphatic compound (C) represented by general formula (III), wherein R
      4 is a 6C-30C aliphatic hydrocarbon group, and W is H, a metal atom or a 1C-8C hydrocarbon group.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 解决问题的方案为了提供一种用于制造具有优异的透明性,不产生裂纹,形状稳定性优异的光学部件用树脂的原料组合物,耐热稳定性显示不发黄,并且也优异 脱模性和光学部件。 解决方案:用于光学部件的树脂的原料组合物包含具有特定结构的金刚烷基(甲基)丙烯酸酯化合物(A),具有特定结构的低分子量(甲基)丙烯酸酯化合物(B)),具有 特别是由通式(III)表示的脂肪族化合物(C),其中,R“SP”为6C-30C脂肪族烃基,W为H,金属原子或1C-8C 烃基。 版权所有(C)2010,JPO&INPIT
    • 7. 发明专利
    • Method for producing polymer by cationic polymerization
    • 通过阳离子聚合制备聚合物的方法
    • JP2008001771A
    • 2008-01-10
    • JP2006171204
    • 2006-06-21
    • Idemitsu Kosan Co Ltd出光興産株式会社
    • IWASAKI TAKESHIYOSHIDA JUNICHI
    • C08F2/00
    • PROBLEM TO BE SOLVED: To provide a method for producing a polymer by which the polymer having a narrow molecular weight distribution can efficiently be produced even by a cationic polymerization.
      SOLUTION: The method for producing the polymer includes introducing a cationic polymerization initiator and a first cationically polymerizable monomer to the first joining part by each flowing method, mixing the cationic polymerization initiator with the first cationically polymerizable monomer at the joining part, and polymerizing the first cationically polymerizable monomer in the first reaction tube connected to the first joining part. The method is regulated so that the inner diameter X (mm) in the first joining part may be within the range of 0.01-10 mm and the flow rate Y (mL/min) of the liquid in the first reaction tube may satisfy the relation of expression (1): (20×X)≤Y (1).
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种制备聚合物的方法,即使通过阳离子聚合也能够有效地制备具有窄分子量分布的聚合物。 解决方案:聚合物的制造方法包括:通过各种流动方法将阳离子聚合引发剂和第一阳离子聚合性单体引入到第一接合部分,在接合部分将阳离子聚合引发剂与第一阳离子聚合性单体混合, 在与第一接合部连接的第一反应管中聚合第一阳离子聚合性单体。 该方法被调整为使得第一接合部中的内径X(mm)可以在0.01-10mm的范围内,并且第一反应管中的液体的流量Y(mL / min)可以满足关系 (1):(20×X)≤Y(1)。 版权所有(C)2008,JPO&INPIT
    • 8. 发明专利
    • 光学部品用樹脂、光学部品用樹脂に用いる原料組成物及び光学部品
    • 光学组分树脂,用于其的成分组合物和光学组分
    • JP2015045868A
    • 2015-03-12
    • JP2014194414
    • 2014-09-24
    • 出光興産株式会社Idemitsu Kosan Co Ltd
    • OBATA HIROSHIIWASAKI TAKESHITAKEBE TOMOAKI
    • G02B1/04C08F220/18C08F230/08C08K5/00C08L33/06
    • C08F220/68C08F222/1006G02B1/04C08L33/10C08L33/08C08L67/00
    • 【課題】耐熱性を有し、かつ熱に対して安定で黄変が発生せず、透明性や加工性にも優れた光学部品用樹脂、該光学部品用樹脂に用いる原料組成物及び光学部品を提供する。【解決手段】(A1)アダマンタン構造を含む炭化水素基がエステル結合した(メタ)アクリレート化合物単位及び(B1)上記(A1)単位以外の、多官能基を持つ(メタ)アクリレート化合物単位を含む樹脂からなる光学部品であって、(A1)が、アダマンチル基がエステル結合した(メタ)アクリレート化合物単位であり、かつ(A1)(メタ)アクリレート化合物単位の含有量が20〜99質量%であり、(B1)(メタ)アクリレート化合物単位の含有量が1〜80質量%であり、さらに(B1)(メタ)アクリレート化合物単位のうちの少なくとも一種がソフトセグメント部位を含み、(B1)中のソフトセグメント部位を含む(メタ)アクリレート化合物単位の含有量が、25〜100質量%である、光学部品。【選択図】なし
    • 要解决的问题:提供一种耐热,耐热稳定,不发黄,并且透明性和加工性优异的光学部件树脂,并且提供用于其的成分组合物和光学组件。 :光学部件由(A1)与含有金刚烷结构的烃基酯连接的(甲基)丙烯酸酯化合物单元和除具有多官能团的(A1)单元以外的(B1)(甲基)丙烯酸酯化合物单元构成。 (A1)是具有金刚烷基酯的(甲基)丙烯酸酯化合物,(A1)(甲基)丙烯酸酯化合物的含量为20〜99质量%,(B1)(甲基)丙烯酸酯 复合单位为1-80质量%。 (B1)(甲基)丙烯酸酯化合物单元中的至少一种含有软链段区域,在(B1)中含有软链段区域的(甲基)丙烯酸酯化合物单元的含量为25〜100质量%。