    • 8. 发明授权
    • Polyoxyalkylene glycol refrigeration lubricants having pendant,
non-terminal perfluoroalkyl groups
    • 具有侧基,非末端全氟烷基的聚氧亚烷基二醇制冷润滑剂
    • US5100569A
    • 1992-03-31
    • US621163
    • 1990-11-30
    • David NalewajekRichard E. EibeckRaymond H. Thomas
    • David NalewajekRichard E. EibeckRaymond H. Thomas
    • C10M107/38C10M171/00
    • C10M171/008C10M107/38
    • The present invention provides a composition for use in refrigeration and air-conditioning comprising: (a) at least one refrigerant selected from the group consisting of hydrofluorocarbon, hydrochlorofluorocarbon, fluorocarbon, and chlorofluorocarbon; and (b) a sufficient amount to provide lubrication of at least one polyoxyalkylene glycol. The polyoxyalkylene glycol has at least one pendant non-terminal perfluorinated alkyl group on its hydrocarbon polymer backbone. The polyoxyalkylene glycol is terminated with a group selected from the group consisting of hydrogen, alkyl, and fluoroalkyl. The polyoxyalkylene glycol has a molecular weight of about 300 to about 4,000 and a viscosity of about 5 to about 300 centistokes at 37.degree. C. The polyoxyalkylene glycol is miscible in combination with the refrigerant in the range between about -40.degree. C. and at least about +20.degree. C.
    • 本发明提供一种用于制冷和空调的组合物,包括:(a)至少一种选自氢氟碳化合物,氢氯氟烃,氟碳化合物和氯氟烃的制冷剂; 和(b)足够的量以提供至少一种聚氧亚烷基二醇的润滑。 聚氧亚烷基二醇在其烃聚合物主链上具有至少一个侧链的非末端全氟化烷基。 聚氧亚烷基二醇用选自氢,烷基和氟代烷基的基团封端。 聚氧亚烷基二醇的分子量为约300至约4,000,在37℃下的粘度为约5至约300厘沲。聚氧亚烷基二醇可与制冷剂混合在约-40℃和 至少约+20℃