    • 2. 发明授权
    • Process for the preparation of flexible polyurethane foams with improved
resistance to hydrolysis and good die cutability
    • 制备柔性聚氨酯泡沫的方法,具有改善的耐水解性和良好的模切性
    • US4362825A
    • 1982-12-07
    • US334157
    • 1981-12-24
    • Herbert GrabhoeferPeter Weyland
    • Herbert GrabhoeferPeter Weyland
    • C08G18/42C08G18/14
    • C08G18/4241C08G18/4219
    • The invention concerns a process for the preparation of flexible polyurethane foams by reacting organic polyisocyanates, liquid polyester polyols having hydroxyl numbers of 40 to 80 and molecular weights of 1500 to 5000, which are produced by the polycondensation of organic dicarboxylic acids with either polyol mixture A, based on the overall polyol weight consisting of:5 to 50 percent by weight of 1,4-butanediol,20 to 60 percent by weight of 1,5-pentanediol,8 to 35 percent by weight of 1,6-hexanediol,2 to 15 percent by weight of at least one triol, and0 to 65 percent by weight of diethylene glycol,or polyol mixture B, based on the overall polyol weight consisting of:10 to 50 percent by weight of 1,4-butanediol,15 to 45 percent by weight of 1,6-hexanediol,15 to 65 percent by weight of diethylene glycol, and2 to 15 percent by weight of at least one triol,in the presence of catalysts and blowing agents as well as optionally chain extenders, auxiliaries and additives.
    • 本发明涉及通过使有机多异氰酸酯,羟基数为40至80的液体聚酯多元醇和分子量为1500至5000的有机多异氰酸酯,通过有机二羧酸与多元醇混合物A的缩聚制备而制备柔性聚氨酯泡沫的方法 ,基于由以下组成的总多元醇重量:5〜50重量%的1,4-丁二醇,20〜60重量%的1,5-戊二醇,8〜35重量%的1,6-己二醇,2 至15重量%的至少一种三醇和0至65重量%的二甘醇或多元醇混合物B,基于总多元醇重量:10至50重量%的1,4-丁二醇,15 至45重量%的1,6-己二醇,15至65重量%的二甘醇和2至15重量%的至少一种三醇,在催化剂和发泡剂以及任选的增链剂的存在下, 助剂和助剂。