热词
    • 4. 发明专利
    • MACHINING METHOD FOR MALE-FEMALE FITTING MEMBERS
    • JPH06190642A
    • 1994-07-12
    • JP34779292
    • 1992-12-28
    • HONDA MOTOR CO LTDHONDA ENGINEERING
    • NANBA SOKOKAMATA TERUOTANAKA KEIZO
    • B23P11/02B23P11/00C22C38/58
    • PURPOSE:To facilitate machining with securing clearance precision, etc., by forming at least one fitting part of subzero cooling hardener between both of male-female fitting members and treating the fitting part by means of subzero cooling after carrying out clearance adjustment machining in the fixing part under the ordinary temperature. CONSTITUTION:At least a fitting part 4a of one member 4 to the other member between two members, which male-female fits each other, is formed of a subzero cooling hardener A which is hardened by subzero cooling. While the fitting part 4a is roughly machined, one member 4 is fitted to the other member to carry out clearance adjustment machining. Then, a coolant such as snow dry ice, etc., is heaped up on the fitting part 4a so that the fitting part 4a is treated by subzero cooling. In this way, clearance adjustment machining in the fitting part 4a can be carried out easily as the hardness of the subzero hardener A is low before subzero cooling. On the other hand, the hardness of the fitting part 4a is increased by subzero cooling without any distortion and abrasion resistance and clearance precision are secured.
    • 7. 发明专利
    • METHOD FOR WORKING PRESS DIE
    • JPH10291070A
    • 1998-11-04
    • JP10349497
    • 1997-04-21
    • HONDA MOTOR CO LTDHONDA ENGINEERING
    • TANAKA KEIZO
    • B23K9/04B21D37/20
    • PROBLEM TO BE SOLVED: To stably form a build-up part without blow-hole on a chipped part with an arc welding torch attached on a working head of a machine. SOLUTION: A chipped part Wa with an almost quater circular cross-section is formed on an edge part We of a die raw material W with a ball end mill 6a. After then, the top end of a wire 11 is positioned so that the distance of lateral direction to an upper edge E2 of the chipped face Ws is made longer than the distance of vertical direction from the top end of the wire 11 to the chipped face Ws, a 1st and B1 covering the lower edge E1 of the chipped face Ws is formed, next, the top end of the wire 11 is positioned so as the be on the upper side and on the outside of lateral direction from the upper edge E2 of the chipped face Ws and a 2nd bead B2 is formed, and on the last, the top end of the wire 11 is positioned on the outer side of the lateral direction from the 2nd pass stage and a 3rd bead B3 covering the remaining chipped range is formed.