    • 1. 发明申请
    • METHOD FOR FORMING OPAQUE QUARTZ GLASS COMPONENTS
    • 用于形成OPAQUE QUARTZ玻璃组件的方法
    • WO2015099659A1
    • 2015-07-02
    • PCT/US2013/077505
    • 2013-12-23
    • HERAEUS QUARTZ AMERICA LLC
    • DONELON, Matthew, J.PITZEN, Arno
    • C03B19/06C03B23/00C03B23/047C03B23/07C03B20/00
    • C03B23/053C03B19/066C03B23/00C03B23/047C03B23/07
    • A method of forming an opaque quartz glass component is provided. The method includes (a) providing a starting preform made of quartz glass; (b) heating at least a portion of the starting preform to a predetermined temperature at which the quartz glass of the starting preform has a viscosity in a range of 10E2 to 10E12 poise; and (c) deforming at least a portion of the heated preform at the predetermined temperature to change a shape and/or dimension(s) of the heated perform in order to form the opaque quartz glass component. The starting preform and the heated preform have respective densities of at least 2.15 g/cm 3 and at least 2.10 g/cm 3 . The starting perform and the opaque quartz glass component have respective direct spectral transmissions of approximately 0.1-1% and 0.2-3% in the wavelength range of λ=190 nm to λ=4990 nm at a wall thickness of 3 mm and a diffuse reflectance of at least 60% in a wavelength range of λ=190 nm to λ=2500 nm.
    • 提供了形成不透明石英玻璃部件的方法。 该方法包括(a)提供由石英玻璃制成的起始预制件; (b)将起始预型件的至少一部分加热到预定温度,在预定温度下,起始预型件的石英玻璃的粘度在10E2至10E12泊的范围内; 和(c)使加热的预制件的至少一部分在预定温度下变形,以改变加热的表面的形状和/或尺寸,以便形成不透明的石英玻璃组分。 起始预成型件和加热的预制件具有至少2.15g / cm 3和至少2.10g / cm 3的相应密度。 起始性能和不透明石英玻璃组分在λ= 190nm至λ= 4990nm的波长范围内在壁厚为3mm的情况下分别具有约0.1-1%和0.2-3%的直接光谱透射率,漫反射率 在λ= 190nm至λ= 2500nm的波长范围内至少为60%。