    • 1. 发明专利
    • Low temperature thermal decomposition treatment furnace
    • 低温热分解炉
    • JP2014094326A
    • 2014-05-22
    • JP2012245615
    • 2012-11-07
    • Gojo:Kk株式会社五常Kikuo Naito亀久夫 内藤
    • NAITO KIKUOONODERA YOSHIAKI
    • B09B3/00
    • PROBLEM TO BE SOLVED: To perform decomposition treatment to waste substances at a low temperature such that dioxin is not generated and make the waste substances into ash.SOLUTION: A low temperature thermal decomposition treatment furnace includes: a lower thermal decomposition treatment chamber 3 formed in an outer tank 1; an air chamber 2 which is divided from the thermal decomposition treatment chamber at a lower part of the outer tank 1; a feeding pipe 5 which supplies magnetization air to the air chamber 2; an air supply hole 4a which allows the air chamber 2 to communicate with the lower thermal decomposition treatment chamber 3; an eaves part 4b which covers an upper part of the air supply hole 4a; and a guide member 4c which protrudes below the air supply hole 4a.
    • 要解决的问题:在低温下对废物进行分解处理,使得不产生二恶英并使废物成灰。解决方案:低温热分解处理炉包括:形成在下部的热分解处理室3 外箱1; 在外罐1的下部与热分解处理室分隔的空气室2; 供给管5,其向空气室2供给磁化空气; 使空气室2与下部热分解处理室3连通的供气孔4a; 覆盖空气供给孔4a的上部的檐部4b; 以及在空气供给孔4a的下方突出的引导部件4c。
    • 2. 发明专利
    • Device and method for bending metal bar material
    • 用于弯曲金属棒材料的装置和方法
    • JP2011104647A
    • 2011-06-02
    • JP2009265067
    • 2009-11-20
    • Gojo:Kk株式会社五常
    • ONODERA YOSHIAKI
    • B21D7/16B21D7/10
    • PROBLEM TO BE SOLVED: To improve work efficiency by maintaining eccentric amount of a metal bar material in constant during bending and simplifying a structure of a device. SOLUTION: The bending device 10 for steel pipe 1 includes a heating section 11 to heat the steel pipe 1, a cooling section 20 to cool the heated portion, a moving means to move the heating section 11 and a cooling section 20 relatively to the steel pipe 1, a steel pipe carrying section 6 which draws a front end pinching part 2 attached to an end of the steel pipe 1 and a wire 4b locked to the front end pinching part and applies compression force on the eccentric axis line eccentrically shifted by a designated distance from the central axis of the steel pipe 1, an end part rotating arm to rotate the front end pinching part 2 with the rotation axis conforming to the bending curvature or the bending profile as the center, an eccentric distance maintaining member 8 with the shape conforming to the bending curvature or the bending profile, around which the wire 4b is wound, and a pressure roller 34 supported by a rotation shaft 31 of the end part rotating arm 33 and rotatably pressed on the steel pipe 1. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:通过在弯曲期间保持金属棒材料的偏心量恒定并且简化装置的结构来提高工作效率。 解决方案:钢管1的弯曲装置10包括用于加热钢管1的加热部分11,用于冷却加热部分的冷却部分20,使加热部分11和冷却部分20相对移动的移动装置 向钢管1供给钢管承载部6,该钢管承载部6拉出安装在钢管1的端部的前端夹持部2和锁定在前端夹持部上的线4b,偏心地对偏心轴线施加压缩力 偏转距离钢管1的中心轴线指定的距离;端部旋转臂,其以与弯曲曲率或弯曲轮廓为中心的旋转轴线旋转前端夹持部2;偏心距离保持部件 8,其形状符合卷绕线4b的弯曲曲率或弯曲轮廓,以及由端部旋转臂33的旋转轴31支撑并可旋转地按压的加压辊34 钢管1.版权所有(C)2011,JPO&INPIT