    • 3. 发明授权
    • Method of continuous metallurgical processing of copper-lead matte
    • 铜铅锍连续冶金加工方法
    • US4614541A
    • 1986-09-30
    • US766756
    • 1985-08-16
    • Gerhard BerndtWerner Marnette
    • Gerhard BerndtWerner Marnette
    • C22B13/02C22B15/00C22B15/06C22B15/14
    • C22B15/006C22B15/0041
    • A method for the continuous pyrometallurgical processing of copper-lead matte having a high lead content relative to copper. In order to ensure an economical and ecologically satisfactory processing, the following steps are performed in a continuous sequence: (a) In one processing stage a suitable atmosphere is provided and temperatures above 1250.degree. C. and a high turbulence are maintained in a molten bath, volatile lead components are incorporated in a fine dust and liquid matte having a decreased lead content and metallic lead included in a copper-containing lead alloy are produced; (b) in another processing stage, gases which contain free oxygen are blown into or onto the liquid matte which has been produced in stage (a) and is at a temperature above 1250.degree. C. whereby a high-oxygen converter slag and a converter copper containing less than 1% by weight lead are produced and volatilizable impurities contained in the matte are incorporated in a fine dust; and (c) in a third processing stage the converter copper, which contains less than 1% by weight Pb and other impurities, such as Ni, As, Sb, is refined in that a gas which contains free oxygen is blown into or onto the molten bath. The impurities are slagged by a selective oxidation, and a prerefined copper is formed.
    • 一种相对于铜具有高铅含量的铜 - 铅锍的连续火法冶金加工方法。 为了确保经济和生态上令人满意的加工,以下连续顺序进行:(a)在一个加工阶段,提供合适的气氛,温度高于1250℃,高湍流保持在熔池中 产生挥发性铅成分,并含有含铅含量降低的细灰尘和液态锍,含铜铅合金中含有金属铅; (b)在另一个处理阶段,将含有游离氧气的气体吹到已经在阶段(a)中生产并处于1250℃以上的温度下的液态锍中或其上,由此将高氧转化炉渣和转化器 产生含有少于1重量%的铅的铜,并且将含有的无光泽的杂质掺入细粉尘中; 和(c)在第三处理阶段,含有小于1重量%的Pb和其它杂质如Ni,As,Sb的转化器铜被精制,因为含有游离氧的气体被吹入 熔浴 杂质通过选择性氧化而排渣,形成预精制铜。
    • 5. 发明授权
    • Current-feeding cathode-mounting device
    • 电流馈电阴极安装装置
    • US4647358A
    • 1987-03-03
    • US762603
    • 1985-08-05
    • Adalbert BartschGerhard Berndt
    • Adalbert BartschGerhard Berndt
    • C25C7/02C25B11/00
    • C25C7/02
    • A current-feeding cathode-mounting device comprises a metal-sheathed carrying rail of copper and a permanent cathode plate consisting of the same material as the sheath and joined by welding at least along part of a longitudinal edge and wherein at least an end portion of the rail is unsheathed at least along part of its extent. In order to increase the creep strength and durability and to ensure a low-resistance contact, the carrying rail consists of a hollow copper section, the sheath consists of special steel, the sheath is joined to the carrying rail by a diffusion-preventing non-porous weld, and the permanent cathode of special steel is joined to the sheath by an interrupted seal weld. The carrying rail consists suitably of a copper tube. In accordance with a further feature the copper tube provided with a special steel sheath has been deformed to constitute a composite having an elliptical or oval cross-section or a cross-section having two parallel sides, and the major axis of said cross-section lies in the plane of the cathode plate.
    • 电流馈送阴极安装装置包括铜的金属护套承载轨道和由与护套相同材料组成的永久阴极板,并且通过至少沿纵向边缘的一部分进行焊接而连接,并且其中至少一个端部 轨道至少沿着它的一部分程度是无缝的。 为了提高蠕变强度和耐久性,并确保低电阻接触,承载导轨由中空铜部分组成,护套由特殊钢构成,护套通过防扩散非金属材料接合到承载轨道上, 多孔焊接,特殊钢的永久阴极通过间断的密封焊接接合到护套。 承载轨道由铜管组成。 根据进一步的特征,设置有特殊钢护套的铜管已经变形以构成具有椭圆形或椭圆形横截面的复合材料或具有两个平行边的横截面,并且所述横截面的长轴位于 在阴极板的平面上。