热词
    • 5. 发明申请
    • ANTI-DAZZLING OPTICAL LAMINATE
    • 防透光层压板
    • US20080260997A1
    • 2008-10-23
    • US12049439
    • 2008-03-17
    • Yukimitsu IwataGen FuruiYoshihiro NishimuraTakashi Kodama
    • Yukimitsu IwataGen FuruiYoshihiro NishimuraTakashi Kodama
    • B32B5/00G02B1/11
    • G02B5/0278G02B5/0226G02B5/0242Y10T428/24355
    • There is provided an anti-dazzling laminate which has anti-dazzling properties, has a high level of transparency by virtue of freedom from a milky-white impression caused by light diffusion, and can realize excellent black color reproducibility and scintillation preventive properties. The anti-dazzling laminate is an optical laminate comprising a light transparent base material and an anti-dazzling layer provided on the light transparent base material, wherein the outermost surface of the anti-dazzling layer has a concavoconvex shape, and the optical laminate satisfies the following requirements: Ha is more than 0% and less than 8%, Hi is more than 0% and not more than 6%, and Hi/Ha is not less than 0.013 and less than 0.8, wherein Ha represents the whole haze value of the optical laminate; and Hi represents the internal haze value of the optical laminate.
    • 提供了具有防炫目性能的抗眩光层压材料,由于光扩散引起的乳白色印象,具有高水平的透明性,并且可以实现优异的黑色再现性和防闪烁性。 防眩光层压体是包含透光性基材和设置在透光性基材上的抗眩光层的光学层叠体,其中防眩光层的最表面具有凹凸形状,并且光学层叠体满足 以下要求:Ha大于0%且小于8%,Hi大于0%且不大于6%,Hi / Ha不小于0.013且小于0.8,其中Ha代表整个雾度值 光学层压板; Hi表示光学层叠体的内部雾度值。
    • 8. 发明申请
    • OPTICAL LAYERED BODY, POLARIZER AND IMAGE DISPLAY DEVICE
    • US20100195311A1
    • 2010-08-05
    • US12377782
    • 2007-08-16
    • Gen FuruiYukimitsu IwataTakashi KodamaYoshihiro NishimuraKoichi Mikami
    • Gen FuruiYukimitsu IwataTakashi KodamaYoshihiro NishimuraKoichi Mikami
    • G02F1/13357B05D5/06G02B5/22G02B5/30
    • G02B1/11G02B5/0221G02B5/0278G02B5/30
    • It is an object of the present invention to provide an optical layered body which can attain properties such as an antiglare property, scintillation prevention and black color reproducibility such as gloss blackness simultaneously.An optical layered body comprising a light-transmitting substrate and an antiglare layer provided on the light-transmitting substrate, wherein the antiglare layer has a surface roughness on the outermost surface, and wherein in the optical layered body, a mean spacing of tops of local peak of profile S is 0.045 mm or more and 0.10 mm or less determined by the following procedure: a roughness curve of the surface roughness is measured, a mean line of the roughness curve is drown, and a reference length is set in the direction of the mean line, total number (m) of tops of local peak of profile existing above the mean line within the reference length is counted, Si representing a value of a length between a (m)th top of local peak of profile and a (m−1)th top of local peak of profile, and n representing number of Si are introduced into the following formula (I): [ Formula   1 ] S ′ = 1 n  ∑ i = 1 n   S i ( I ) to determine S′, and a value of S′ in the following same reference length is calculated and the calculation is repeated N times, and S′ j representing a value of S′ calculated in the above formula (I) and N representing number of S′ j are introduced into the following formula (II): [ Formula   2 ] S = 1 n  ∑ j = 1 N   S j ′ ( II ) to determine a mean spacing of tops of local peak of profiles S, and wherein when denoting a mean spacing of profile irregularities of the surface of the optical layered body by Sm, a mean inclination angle of profile irregularities by θa, and mean roughness of the surface roughness by Rz, Sm is 50 μm or more and less than 100 μm, θa is 0.1° or more and 1.0° or less, and Rz is more than 0.2 μm and 1.0 μm or less.
    • 9. 发明授权
    • Optical multilayer body, polarization plate using same, and image display
    • 光学多层体,使用相同的偏光板和图像显示
    • US08241737B2
    • 2012-08-14
    • US13230961
    • 2011-09-13
    • Yukimitsu IwataKoichi MikamiYoshihiro NishimuraTakashi Kodama
    • Yukimitsu IwataKoichi MikamiYoshihiro NishimuraTakashi Kodama
    • G09F13/04G02B5/02G02B5/30
    • G02F1/133502G02B1/111G02F1/133528
    • An optical laminate is provided which has anti-dazzling properties and can realize excellent glare preventive properties and black reproducibility (gradation rendering of black at low brightness). The optical laminate includes a light transparent base material and an anti-dazzling layer or a light diffusion layer provided on the light transparent base material, wherein the outermost surface of the anti-dazzling layer or light diffusion layer has a concavoconvex surface. The anti-dazzling layer satisfies the requirements that Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes in the anti-dazzling layer, θa represents the average inclination angle of the concavoconvexes, and Rz represents the average roughness of the concavoconvexes.
    • 提供具有防炫目性能并且可以实现优异的防眩性和黑色再现性(低亮度下的黑色的渐变渲染)的光学层叠体。 光学层叠体包括透光基材和防透光层或设置在透光基材上的光漫射层,其中抗炫目层或光扩散层的最外表面具有凹凸表面。 抗眩光层满足Sm为100μm以上且600μm以下的要求,a为0.1度以上1.2以下,Rz为0.2μm以上, 1μm,其中Sm表示抗眩光层中的凹凸的平均间距,a表示凹凸的平均倾斜角,Rz表示凹凸的平均粗糙度。
    • 10. 发明申请
    • METHOD AND APPARATUS FOR PRODUCING OPTICAL MULTILAYER BODY
    • 用于生产光学多层体的方法和装置
    • US20100252202A1
    • 2010-10-07
    • US12695251
    • 2010-01-28
    • Yukimitsu IWATAKoichi MikamiYoshihiro NishimuraTakashi Kodama
    • Yukimitsu IWATAKoichi MikamiYoshihiro NishimuraTakashi Kodama
    • B29C70/78
    • G02B1/111G02F1/133502Y10T428/26
    • An optical laminate produced by a process for producing an anti-dazzling laminate comprising a light transparent base material and an anti-dazzling layer provided on the light transparent base material. The process includes providing the light transparent base material and forming the anti-dazzling layer having a concavoconvex shape on the light transparent base material, wherein the concavoconvex shape of the anti-dazzling layer satisfies the following requirements: Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes or profile irregularities in the anti-dazzling layer; θa represents the average inclination angle of the concavoconvexes or profile irregularities; and Rz represents the average roughness of the concavoconvexes or profile irregularities.
    • 一种通过用于制造抗光泽层压体的方法制造的光学层压材料,其包含透光基材和设置在透光基材上的防炫目层。 该方法包括提供透光基材并在透光基材上形成具有凹凸形状的防炫光层,其中抗晕眼层的凹凸形状满足以下要求:Sm不小于100μm, 不超过600μm,a不小于0.1度且不大于1.2度,Rz大于0.2μm且不大于1μm,其中Sm表示抗反射层中凹凸或凹凸的平均间距 炫耀层; &thetas; a表示凹凸或轮廓不规则的平均倾角; 并且Rz表示凹凸或轮廓不规则的平均粗糙度。