    • 7. 发明授权
    • Composition and method for producing boron carbide/titanium diboride
composite ceramic powders using a boron carbide substrate
    • 使用碳化硼基板制造碳化硼/二硼化钛复合陶瓷粉末的组合物和方法
    • US5342811A
    • 1994-08-30
    • US698435
    • 1991-05-10
    • Bijan KhazaiWilliam G. Moore
    • Bijan KhazaiWilliam G. Moore
    • C04B35/563C04B35/58C04B35/56
    • C04B35/58071C04B35/563C04B35/645C04B35/65
    • A composition and method for producing boron carbide/titanium diboride composite ceramic powders is disclosed. The process comprises the ordered steps of (a) intimately mixing as reactants boron carbide and a titanium source, such that the average reactant particle size is less than about 20 microns and substantially all discrete reactant areas are less than about 50 microns, and (b) reacting the product of step (a) under conditions sufficient to produce a boron carbide/titanium diboride composite ceramic powder wherein at least a portion of the boron carbide particles form substrates to which at least a portion of the titanium diboride particles are attached. The method can be used to produce a composite ceramic powder having boron carbide and titanium diboride particles less than about 20 microns in diameter. This powder can then be densified using known densification techniques to form a densified part wherein the titanium diboride grains have an average size of less than about 20 microns in diameter and the boron carbide grains having an average size of less than about 50 microns.
    • 公开了一种用于生产碳化硼/二硼化钛复合陶瓷粉末的组合物和方法。 该方法包括(a)作为反应物碳化硼和钛源充分混合的有序步骤,使得平均反应物粒度小于约20微米,并且基本上所有离散的反应物区域小于约50微米,和(b )在足以产生碳化硼/二硼化钛复合陶瓷粉末的条件下使步骤(a)的产物反应,其中至少一部分碳化硼颗粒形成至少部分二硼化钛颗粒所附着的基底。 该方法可用于生产具有直径小于约20微米的碳化硼和二硼化钛颗粒的复合陶瓷粉末。 然后可以使用已知的致密化技术将该粉末致密化以形成致密化部分,其中二硼化钛颗粒的直径平均尺寸小于约20微米,碳化硼颗粒的平均尺寸小于约50微米。