    • Low melting polyester polymers
    • 低熔聚酯聚合物
    • US20060046004A1
    • 2006-03-02
    • US11018119
    • 2004-12-21
    • Michael EkartFrederick ColhounMary JerniganStephen WeinholdRodney Armentrout
    • Michael EkartFrederick ColhounMary JerniganStephen WeinholdRodney Armentrout
    • B31B45/00
    • C08G63/183B29B2911/1402B29B2911/14026B29B2911/14033B29B2911/1404B29B2911/14106B29B2911/14133B29C49/0005B29C49/06B29C51/002B29K2067/00C08G63/90Y10T428/13Y10T428/1303Y10T428/1352Y10T428/1359Y10T428/139
    • A bulk of polyester polymer particles comprising polyester polymer comprising greater than 75% virgin polyester polymer, the particles having: A) an It.V. of at least 0.72 dl/g, and B) 10 ppm or less of residual acetaldehyde; and C) at least two melting peaks, wherein one of said at least two melting peaks is a low peak melting point within a range of 140° C. to 220° C. and having a melting endotherm area of at least the absolute value of 1 J/g. The particles may also have a degree of crystallinity within a range of 20% and a maximum degree of crystallinity Tcmax defined by the equation: Tcmax=50%−CA−OH where CA is the total mole % of all carboxylic acid residues other than terephthalic acid residues, based on 100 mole % of carboxylic acid residues, and OH is the total mole % of all hydroxyl functional compound residues other than ethylene glycol residues, based on 100 mole % of hydroxyl functional compounds residues. The preforms and bottles made from these particles can be obtained by melt processing these particles at either lower overall power, faster screw speeds, lower residence time, or lower overall cycle time to thereby reduce the level of residual acetaldehyde generated in the melt.
    • 包含大于75%的原始聚酯聚合物的聚酯聚合物的大部分聚酯聚合物颗粒,该颗粒具有:A)It.V. 至少0.72dl / g,B)10ppm或更少的残留乙醛; 和C)至少两个熔融峰,其中所述至少两个熔融峰中的一个是在140℃至220℃的范围内的低峰值熔点,并且其熔融吸热面积至少为 1 J / g。 颗粒也可以具有在以下等式定义的20%范围内和最大结晶度T max cmax的范围内的结晶度:<?in-line-formula description =“In-line Formulas” end =“lead”?> Taxaxax = 50%-CA-OH <?in-line-formula description =“In-line Formulas”end =“tail”?>其中CA是总数 基于100摩尔%的羧酸残基,除对苯二甲酸残基之外的所有羧酸残基的摩尔%,OH是除乙二醇残基之外的所有羟基官能化合物残基的总摩尔%,基于100摩尔%的羟基官能 化合物残基。 由这些颗粒制成的预成型件和瓶可以通过以更低的总功率,更快的螺杆速度,更低的停留时间或更低的总循环时间熔融加工这些颗粒来获得,从而降低熔体中产生的残余乙醛的水平。
    • 3. 发明申请
    • High IV melt phase polyester polymer catalyzed with antimony containing compounds
    • 用含锑化合物催化的高IV熔融相聚酯聚合物
    • US20050203267A1
    • 2005-09-15
    • US10796238
    • 2004-03-09
    • Mary JerniganMichael EkartRichard Bonner
    • Mary JerniganMichael EkartRichard Bonner
    • C08G63/78C08G63/86C08G63/87C08G63/00
    • C08G63/866C08G63/78C08G63/87Y10T428/31504Y10T428/31507
    • A melt phase process for making a polyester polymer melt phase product by adding an antimony containing catalyst to the melt phase, polycondensing the melt containing said catalyst in the melt phase until the It.V. of the melt reaches at least 0.75 dL/g. Polyester polymer melt phase pellets containing antimony residues and having an It.V. of at least 0.75 dL/g are obtained without solid state polymerization. The polyester polymer pellets containing antimony residues and having an It.V. of at least 0.70 dL/g obtained without increasing the molecular weight of the melt phase product by solid state polymerization are fed to an extruder, melted to produce a molten polyester polymer, and extruded through a die to form shaped articles. The melt phase products and articles made thereby have low b* color and/or high L* brightness, and the reaction time to make the melt phase products is short.
    • 一种用于通过向熔融相中加入含锑催化剂来制备聚酯聚合物熔融相产物的熔融相方法,将熔融相中包含所述催化剂的熔体缩聚至It.V. 的熔体达到至少0.75dL / g。 含有锑残留物并具有It.V.的聚酯聚合物熔相颗粒 在没有固态聚合的情况下获得至少0.75dL / g。 含有锑残留物并具有It.V.的聚酯聚合物颗粒 通过固态聚合而不增加熔融相产物的分子量而获得的至少0.70dL / g进料到挤出机中,熔化以产生熔融聚酯聚合物,并通过模头挤出以形成成型制品。 由此制得的熔融相产物和制品具有低的b *色和/或高L *亮度,并且使熔融相产物的反应时间短。
    • 7. 发明申请
    • High IV melt phase polyester polymer catalyzed with antimony containing compounds
    • 用含锑化合物催化的高IV熔融相聚酯聚合物
    • US20060149027A1
    • 2006-07-06
    • US11361655
    • 2006-02-24
    • Mary JerniganMichael EkartRichard Bonner
    • Mary JerniganMichael EkartRichard Bonner
    • C08G63/87
    • C08G63/866C08G63/78C08G63/87Y10T428/31504Y10T428/31507
    • A melt phase process for making a polyester polymer melt phase product by adding an antimony containing catalyst to the melt phase, polycondensing the melt containing said catalyst in the melt phase until the It.V. of the melt reaches at least 0.75 dL/g. Polyester polymer melt phase pellets containing antimony residues and having an It.V. of at least 0.75 dL/g are obtained without solid state polymerization. The polyester polymer pellets containing antimony residues and having an It.V. of at least 0.70 dL/g obtained without increasing the molecular weight of the melt phase product by solid state polymerization are fed to an extruder, melted to produce a molten polyester polymer, and extruded through a die to form shaped articles. The melt phase products and articles made thereby have low b* color and/or high L* brightness, and the reaction time to make the melt phase products is short.
    • 一种用于通过向熔融相中加入含锑催化剂来制备聚酯聚合物熔融相产物的熔融相方法,将熔融相中包含所述催化剂的熔体缩聚至It.V. 的熔体达到至少0.75dL / g。 含有锑残留物并具有It.V.的聚酯聚合物熔相颗粒 在没有固态聚合的情况下获得至少0.75dL / g。 含有锑残留物并具有It.V.的聚酯聚合物颗粒 通过固态聚合而不增加熔融相产物的分子量而获得的至少0.70dL / g进料到挤出机中,熔化以产生熔融聚酯聚合物,并通过模头挤出以形成成型制品。 由此制得的熔融相产物和制品具有低的b *色和/或高L *亮度,并且使熔融相产物的反应时间短。