    • 3. 发明授权
    • Polymer blends useful for forming extrusion blow molded articles
    • 用于成型挤出吹塑制品的聚合物共混物
    • US5283295A
    • 1994-02-01
    • US895069
    • 1992-06-08
    • Ronald R. LightJames W. Mercer, Jr.
    • Ronald R. LightJames W. Mercer, Jr.
    • C08L67/00C08L67/02C08L69/00
    • C08L67/02Y10T428/1352
    • Disclosed is a polymer blend having excellent clarity and impact strength which is suitable for use in extrusion blow molding processes comprisinga) about 50-95 wt % of a polyester having repeat units from at least 95 mol % terephthalic acid, at least 90 mol % ethylene glycol and up to 10 mol % 1,4-cyclohexanedimethanol, the polyester having a weight average molecular weight of 75,000-85,000,b) about 40-4 wt % of recycled scrap polyester having repeat units from at least 90 mol % terephthalic acid and at least 90 mol % ethylene glycol and having a molecular weight of about 40,000-55,000, andc) about 1-10 wt % of a polymeric material containing at least 90 wt % polycarbonate and up to 10 wt % polyethylene terephthalate.
    • 公开了具有优异的透明度和冲击强度的聚合物共混物,其适用于挤出吹塑成型方法,其包括a)约50-95重量%的具有至少95摩尔%对苯二甲酸的重复单元的聚酯,至少90摩尔% 乙二醇和至多10mol%的1,4-环己烷二甲醇,所述聚酯的重均分子量为75,000-85,000,b)约40-4wt%的具有来自至少90mol%对苯二甲酸的重复单元的再循环废旧聚酯 和至少90mol%的乙二醇,分子量为约40,000-55,000,以及c)约1-10wt%的含有至少90wt%聚碳酸酯和至多10wt%聚对苯二甲酸乙二醇酯的聚合物材料。
    • 7. 发明授权
    • Injection moldable glass fiber reinforced polyester with improved
surface finishes
    • 注塑成型玻璃纤维增​​强聚酯,表面光洁度提高
    • US4810744A
    • 1989-03-07
    • US177201
    • 1988-04-04
    • Ronald R. Light
    • Ronald R. Light
    • C08K7/14C08L67/00C08L67/02C08K3/40
    • C08K7/14C08L67/02
    • A glass fiber reinforced poly(ethylene terephthalate) resin, comprising:(i) a poly(ethylene terephthalate) resin;(ii) 10to 60 weight % of reinforced glass fibers; and(iii) 0.1 to 10 weight % of a nucleating agent comprising:(a) a Group I, II, or IV metal cation salt of an ethylene/methacrylic acid copolymer resin having a melt flow index of from about 0.5 g/10 minutes to about 150 g/10 minutes measured at 190.degree. C. under a 10,128-gram load, and(b) a Group I, II, or IV metal cation salt of an ethylene/acrylic acid copolymer resin having a melt flow index of from about 0.5 g/10 minutes to about 150 g/10 minutes measured at 190.degree. C. under a 2,160-gram load.
    • 一种玻璃纤维增​​强聚(对苯二甲酸乙二醇酯)树脂,其包含:(i)聚(对苯二甲酸乙二醇酯)树脂; (ii)10至60重量%的增强玻璃纤维; 和(iii)0.1至10重量%的成核剂,其包含:(a)乙烯/甲基丙烯酸共聚物树脂的I,II或IV族金属阳离子盐,其熔体流动指数为约0.5g / 10分钟 在19012℃下以10,128克负荷测量至约150g / 10分钟,和(b)乙烯/丙烯酸共聚物树脂的I,II或IV族金属阳离子盐,其熔体流动指数为 在190℃下在2,160克负荷下测量约0.5g / 10分钟至约150g / 10分钟。