    • 3. 发明授权
    • Process for the production of emulsifier-free, self-crosslinkable rubber
latices
    • 生产无乳化剂,自交联橡胶胶乳的方法
    • US4246156A
    • 1981-01-20
    • US55184
    • 1979-07-06
    • Ferdinand HeinsMartin Matner
    • Ferdinand HeinsMartin Matner
    • C08F2/00C08F2/22C08F4/28C08F4/30C08F212/02C08F236/00C08F236/04
    • C08F2/22C08F212/02C08F236/04
    • A process for the production of an emulsifier-free self-crosslinkable rubber latex (meth)acrylic acid, N-alkoxymethyl (meth)acrylamide and acyclic conjugated dienes arylvinyl monomers and/or (meth)acrylonitrile, wherein an aqueous emulsion is prepared by adding at least part of the (meth)acrylic acid, part of the diene and further monomers to water, the polymerization reaction is initiated by the addition of an aqueous solution of a peroxodisulphate and is carried out in a first stage at a pH-value of from 3.5 to 7 until at least 50% of the monomers have been polymerized, the rest of the monomers and initiator are added in one or more further stages and the polymerization reaction is continued at a pH-value of from 3.5 to 7 until at least 50% of the monomers and, in the last stage, until from 85 to 100% of the monomers have been polymerized.
    • 一种生产无乳化剂的自交联橡胶胶乳(甲基)丙烯酸,N-烷氧基甲基(甲基)丙烯酰胺和非环状共轭二烯芳基乙烯基单体和/或(甲基)丙烯腈的方法,其中水乳液通过加入 至少部分(甲基)丙烯酸,二烯的一部分和其它单体与水的混合,通过加入过氧二硫酸盐水溶液引发聚合反应,并在第一阶段进行pH值为 从3.5至7直到至少50%的单体已经聚合,剩余的单体和引发剂在一个或多个其它阶段中加入,并且聚合反应在3.5至7的pH值下持续至少 50%的单体,在最后阶段,直到85至100%的单体已经聚合。
    • 7. 发明授权
    • Process for dressing leather by a treatment using rubber latices
    • 使用橡胶胶乳处理皮革的方法
    • US4330597A
    • 1982-05-18
    • US206069
    • 1980-11-12
    • Ferdinand HeinsLeo TorkWolfgang Hohne
    • Ferdinand HeinsLeo TorkWolfgang Hohne
    • C14C11/00B05D3/02B05D3/12B32B9/02C14C9/00
    • C14C11/003Y10T428/4935
    • Advantages in the dressing of leather, especially of split leather, with a synthetic rubber latex are obtained if in the leather dressing, the rubber latex is reacted with from 0.5 to 50% by weight, based on solid rubber, of one or more oxides and/or hydroxides of one or more bivalent metals and the leather is treated with a non-polymerized rubber latex which is produced in a one-stage process up to a monomer conversion of from 70 to 95% by weight, by emulsion polymerization of:(A) from 1 to 10 parts by weight of one or more .alpha.,.beta.-monoethylenically unsaturated carboxylic acids; and(B) from 90 to 99 parts by weight of a mixture of(a) from 10 to 90 parts by weight of butadiene and(b) from 10 to 90 parts by weight of styrene and/or acrylonitrile, wherein the quantity of acrylonitrile in the mixture amounts to a maximum of 50 parts by weight.
    • 如果在皮革敷料中,橡胶胶乳以0.5至50重量%的比例以固体橡胶为基础与一种或多种氧化物反应,则可获得皮革,特别是分裂皮革的皮革的修整与合成橡胶胶乳的优点, /或一种或多种二价金属的氢氧化物,并且皮革用未分解的橡胶胶乳处理,所述非聚合橡胶胶乳通过乳液聚合在一步法中制备直至单体转化率为70至95重量% A)1至10重量份的一种或多种α,β-单烯属不饱和羧酸; 和(B)90至99重量份的(a)10至90重量份的丁二烯和(b)10至90重量份的苯乙烯和/或丙烯腈的混合物,其中丙烯腈的量 在混合物中最多达50重量份。