会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明专利
    • Method for producing weather-resistant coating composition and method for preventing coloration and coated article
    • 生产耐候涂料组合物的方法和防止涂料和涂料的方法
    • JP2013189485A
    • 2013-09-26
    • JP2012054393
    • 2012-03-12
    • Shin-Etsu Chemical Co Ltd信越化学工業株式会社
    • HIGUCHI KOICHI
    • C09D157/00C09D7/12C09D133/14C09D143/04C09D145/00C09D157/06C09D183/04
    • PROBLEM TO BE SOLVED: To provide a method for producing non-colored weather-resistant coating composition and a method for preventing coloration, and to provide a coated article using the composition.SOLUTION: A method for producing a weather-resistant coating composition comprising a vinylic polymer (A) to whose side chains hydrolyzable silyl groups and organic UV ray-absorbing groups are bound, respectively, fine silica particles (B) dispersed in an organic solvent, a carbonyl group-containing organic solvent (C), an orthocarbonic ester (D), and a tertiary amine or its organic acid salt (E), includes: the following step [1] or [2]. [1]: (I) a step of preparing a coating precursor containing one or more components excluding the component (E), and (II) a step of adding the component (E) to the coating precursor. [2]: (III) a step of preparing a coating precursor containing the component (A), or containing (A) and one or more components excluding the components (D), (IV) a step of adding water to the coating precursor to partially hydrolyze the coating precursor, and (V) a step of adding the component (D) to the hydrolysate of the coating precursor.
    • 要解决的问题:提供一种生产无色耐候性涂料组合物的方法和防着色方法,并提供使用该组合物的涂布制品。方法:一种耐候性涂料组合物的制备方法,包括 其侧链可水解甲硅烷基和有机紫外线吸收基的乙烯基聚合物(A)分别结合分散在有机溶剂中的二氧化硅微粒(B),含羰基的有机溶剂(C),正碳酸酯 (D)和叔胺或其有机酸盐(E)包括:以下步骤[1]或[2]。 [1]:(I)制备包含除组分(E)之外的一种或多种组分的涂料前体的步骤,和(II)将组分(E)加入到涂料前体中的步骤。 [2]:(III)制备包含组分(A)或包含(A)和除组分(D),(IV)之外的一种或多种组分的涂料前体的步骤, 部分水解涂料前体,和(V)将组分(D)加入到涂料前体的水解产物中的步骤。
    • 3. 发明专利
    • Method of manufacturing laminate
    • 制造层压板的方法
    • JP2011245684A
    • 2011-12-08
    • JP2010119403
    • 2010-05-25
    • Shin-Etsu Chemical Co Ltd信越化学工業株式会社
    • FUKUSHIMA MOTOOHIGUCHI KOICHIKOMORI HISATOSHI
    • B32B27/30B32B27/00B32B27/36
    • PROBLEM TO BE SOLVED: To provide a laminate that expresses scratch resistance and UV shielding properties maintaining the transparency of visible light, further, which has the stability of a long term.SOLUTION: A method of manufacturing the laminate includes laminating a primer layer and a top layer on a surface of a base material. In addition, the method of manufacturing the laminate includes as follows. A primer composition including: a thermoplastic (meth)acrylic polymer having an alkoxysilyl group and an ultraviolet absorption group; a silicon dioxide fine particle; and a hydrolysis prevention agent preventing hydrolysis condensation of an alkoxysilyl group is applied to a surface of the base material, subsequently, on it a hardtop composition including: a cohydrolysis condensate of an organosilicon compound having an organooxy group and a silicon dioxide fine particle; and a curing catalyst making the alkoxysilyl group of the primer composition react with the organooxy group and making the cohydrolysis condensate cure is applied to be laminated, subsequently, is heated so that the hardtop composition is bridged/cured, and thereby the primer layer having thermoplasticity and the top layer having thermosetting are formed.
    • 要解决的问题:提供表现出耐久性和耐紫外线性的层压体,其保持了长期稳定性的可见光透明度。 解决方案:制造层压体的方法包括在基材的表面上层叠底漆层和顶层。 此外,制造层压体的方法包括如下。 一种底漆组合物,其包含:具有烷氧基甲硅烷基和紫外线吸收基的热塑性(甲基)丙烯酸类聚合物; 二氧化硅微粒; 并且在基材的表面上涂布防止烷氧基甲硅烷基的水解缩合的水解防止剂,接着在其上包含具有有机氧基的有机硅化合物与二氧化硅微粒的共水解缩合物的硬顶组合物; 使使底漆组合物的烷氧基甲硅烷基与有机氧基反应并使共水解缩合物固化的固化催化剂进行层压,随后加热,使得硬顶组合物桥接/固化,由此具有热塑性的底漆层 并且形成具有热固性的顶层。 版权所有(C)2012,JPO&INPIT
    • 4. 发明专利
    • Method for producing primer composition and coated product
    • 生产原料组合物和涂层产品的方法
    • JP2010065076A
    • 2010-03-25
    • JP2008229986
    • 2008-09-08
    • Shin-Etsu Chemical Co Ltd信越化学工業株式会社
    • HIGUCHI KOICHI
    • C09D143/04B32B27/00B32B27/30C08J3/205C08K3/36C08K5/00C08L57/06C09D5/00C09D7/12C09D183/00
    • C08G77/06C09D183/16Y10T428/31663
    • PROBLEM TO BE SOLVED: To provide a method for producing a primer composition forming a protective coating without cracking, peeling and yellowing for a long period of time, and excellent in weatherability, having reproducibility of these properties, having good storage stability without thickening or gelling; and to provide a coated article using the composition. SOLUTION: A method for producing a primer composition to form a polysiloxane hard film comprises the following steps [1] or [2]: [1] (I) a step to prepare a primer precursor containing a vinyl polymer (A) having a hydrolyzable silyl group and an organic UV absorbing group, bonded at side chains thereof and silica fine particles (B) dispersed in an organic solvent, respectively, (II) a step to add water to the primer precursor to hydrolyze, (III) a step to add a dehydrating agent (C) to the composition containing the hydrolyzate to remove moisture contained in the composition, [2] (IV) a step to add water to (A) to hydrolyze, (V) a step to add (B) to the hydrolyzate, and (VI) a step to add (C) to the composition to remove moisture contained in the composition. COPYRIGHT: (C)2010,JPO&INPIT
    • 待解决的问题:提供一种长时间形成保护涂层而不会发生龟裂,剥离和变黄的底漆组合物的制备方法,并具有优异的耐候性,具有这些性能的再现性,具有良好的储存稳定性而没有 增稠或胶凝; 并提供使用该组合物的涂布制品。 解决方案:制备用于形成聚硅氧烷硬膜的底漆组合物的方法包括以下步骤[1]或[2]:[1](I)制备含有乙烯基聚合物(A)的底漆前体的步骤, 具有分别结合在侧链上的可水解甲硅烷基和有机UV吸收基团和分散在有机溶剂中的二氧化硅细颗粒(B),(II)步骤以向引物前体加水以水解,(III) 向含有水解产物的组合物中加入脱水剂(C)以除去组合物中所含的水分的步骤,[2](IV)向(A)中加水以水解的步骤,(V)添加步骤 B)至水解产物,和(VI)向组合物中添加(C)以除去组合物中所含的水分的步骤。 版权所有(C)2010,JPO&INPIT
    • 9. 发明专利
    • Abrasion resistant silicone coating composition, coated article, and making method
    • 耐磨硅胶涂料组合物,涂层制品和制造方法
    • JP2011037948A
    • 2011-02-24
    • JP2009184597
    • 2009-08-07
    • Shin-Etsu Chemical Co Ltd信越化学工業株式会社
    • HIGUCHI KOICHI
    • C09D183/00B05D5/00B05D7/24B32B27/00C08J7/04C09D5/00C09D5/32C09D7/12C09D151/00C09D167/00C09D169/00C09D175/04
    • C09D183/04C08K3/36C08L51/06C08L2666/24
    • PROBLEM TO BE SOLVED: To provide a silicone coating composition directly coatable on an organic resin base material, and providing a cured coated film having excellent transparency, exhibiting scratch resistance and having good long-term adhesiveness, and to provide a coated article obtained by coating the composition. SOLUTION: The abrasion resistant silicone coating composition comprises (A) a hydrolytic condensate obtained by (co)hydrolytic condensation of an alkoxysilane represented by formula (1): R 1 m R 2 n Si(OR 3 ) 4-m-n (1) (wherein, R 1 and R 2 are each H or monovalent hydrocarbon with the proviso that the substituents may be bonded to each other; R 3 is alkyl; and m and n are each 0 or 1 with the proviso that m+n are 0, 1 or 2) or a partial hydrolytic condensation product thereof, (B) colloidal silica, (C) a polycarbonate-based and/or polyester-based urethane-modified vinyl polymer, (D) a curing catalyst, and (E) a solvent, the solid content of component (C) being 1 to 30 mass% of urethane-modified vinyl polymer based on the total solid content of components (A) the hydrolytic condensate and (B) the colloidal silica. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供可直接涂布在有机树脂基材上的硅氧烷涂料组合物,并提供具有优异透明性,显示耐刮擦性和长期粘合性好的固化涂膜,并提供涂布物 通过涂覆组合物获得。 耐磨性有机硅涂料组合物包含(A)通过式(1)表示的烷氧基硅烷(共)水解缩合获得的水解缩合物:R 1 3 > 1 和R 2 各自为H或一价烃,条件是取代基可以彼此键合; R 3是烷基; m和 n分别为0或1,条件是m + n为0,1或2)或其部分水解缩合产物,(B)胶态二氧化硅,(C)聚碳酸酯基和/或聚酯基氨基甲酸酯改性 乙烯基聚合物,(D)固化催化剂和(E)溶剂,基于组分(A)的总固体含量,组分(C)的固含量为氨基甲酸酯改性乙烯基聚合物的1〜30质量% 冷凝物和(B)胶体二氧化硅。 版权所有(C)2011,JPO&INPIT
    • 10. 发明专利
    • Uv-shielding silicone coating composition and coated article
    • 紫外线屏蔽硅胶涂料组合物和涂层制品
    • JP2010202731A
    • 2010-09-16
    • JP2009047965
    • 2009-03-02
    • Shin-Etsu Chemical Co Ltd信越化学工業株式会社
    • HIGUCHI KOICHIKOMORI HISATOSHI
    • C09D183/06C09D5/00C09D7/12C09D183/05C09D201/10
    • C08J7/047C08J7/04C08J2369/00C08J2483/00C09D183/04Y10T428/31663
    • PROBLEM TO BE SOLVED: To provide a silicone coating composition whose coated cured film expresses mar resistance, and UV-shielding property while maintaining visible light transparency, and further simultaneously has weatherability durable against long term out-door exposure and durability, and a coated article using the same. SOLUTION: The UV-shielding silicone coating composition comprises (A) a dispersion in a dispersing medium of composite zinc oxide fine particles which are obtained by coating the surface of the zinc oxide fine particles with at least one kind selected from an oxide or hydroxide of Al, Si, Zr and Sn, the dispersion having a photocatalytic degradability of up to 25%, (B) a silicone resin, (C) a curing catalyst, and (D) a solvent, the solids content of composite zinc oxide nanoparticle dispersion (A) being 1 to 50 mass% based on silicone resin (B). COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种涂覆固化膜表现耐磨性的硅树脂涂料组合物,同时保持可见光透明性的紫外线屏蔽性,并且还具有耐长期暴露和耐久性耐久性的耐候性,以及 使用其的涂布制品。 UV屏蔽硅酮涂料组合物包含(A)复合氧化锌微粒的分散介质中的分散体,其通过用至少一种选自氧化物的氧化锌微粒表面涂覆而获得 或Al,Si,Zr和Sn的氢氧化物,光催化降解性高达25%的分散体,(B)有机硅树脂,(C)固化催化剂和(D)溶剂,复合锌的固体含量 氧化物纳米粒子分散体(A)为1〜50质量%。 版权所有(C)2010,JPO&INPIT