    • PROCESS FOR PREPARING Sic-BONDED POLYETHER SILOXANE
    • 制备矽胶结合聚硅氧烷的方法
    • JP2008223025A
    • 2008-09-25
    • JP2008059698
    • 2008-03-10
    • Evonik Goldschmidt Gmbhエヴォニク ゴールドシュミット ゲーエムベーハー
    • NEUMANN THOMASKLAUS DIETER KLEIN
    • C08G77/46
    • C08G77/46C08G77/34
    • PROBLEM TO BE SOLVED: To provide a process for preparing Sic-bonded polyether siloxane.
      SOLUTION: Disclosed is a process for preparing a polyoxyalkylene-polysiloxane-block mixed polymer or an alkylpolysiloxane-polyoxyalkylene polysiloxane-block mixed polymer, in which a polysiloxane block is bonded to a polyether block or an alkyl residue by an Sic bond, the process being characterized by treating the polyoxyalkylene-polysiloxane-block mixed polymer, the alkylpolysiloxane-polyoxyalkylene polysiloxane-block mixed polymer or a solution thereof with a fluid hydrogen gas and, optionally, another inactive gas in the presence of a combination of a hydrogenation catalyst known per se, an acid-activated support material and water at a temperature of 20-200°C, under normal pressure for 0.5-10 hours.