    • 1. 发明授权
    • Austenitic stainless steel having superior press-formability, hot
workability and high temperature oxidation resistance, and
manufacturing process therefor
    • 具有优异的压制成型性,热加工性和耐高温氧化性的奥氏体不锈钢及其制造方法
    • US5571343A
    • 1996-11-05
    • US416875
    • 1995-04-19
    • Do Y. RyooYong H. LeeJae S. ParkHyun C. KimEung J. Kim
    • Do Y. RyooYong H. LeeJae S. ParkHyun C. KimEung J. Kim
    • C21D8/00C22C38/00C22C38/40C22C38/42C22C38/58
    • C22C38/42
    • An austenitic stainless steel and a manufacturing process therefor are disclosed, in which, instead of the expensive Ni, there are added Cu as an austenite (.tau.) stabilizing element, and tiny amounts of Ti as a ferrite forming element and B for improvement of high temperature hot workability, so that the optimum Md.sub.30 temperature and the optimum delta-ferrite content can be controlled, thereby improving the formability, the season cracking resistance, the hot workability and the high temperature oxidation resistance, and reducing the surface defects during the hot rolling and saving the manufacturing cost by reducing the content of Ni. The austenitic stainless steel according to the present invention includes in weight %: less than 0.07% of C, less than 1.0% of Si, less than 2.0% of Mn, 16-18% of Cr, 6.0-8.0% of Ni, less than 0.005% of Al, less than 0.05% of P, less than 0.005% of S, less than 0.03% of Ti, less than 0.003% of B, less than 3.0% of Cu, less than 0.3% of Mo, less than 0.1% of Nb, less than 0.045% of N, the balance of Fe, and other indispensable impurities. Thus the present invention improves the press formability, the season cracking resistance, the hot workability, and the high temperature oxidation resistance.
    • 公开了一种奥氏体不锈钢及其制造方法,其中代替昂贵的Ni,添加了作为奥氏体(tau)稳定化元素的Cu和少量的作为铁素体形成元素的Ti和用于提高高分子量的B 可以控制最佳Md30温度和最佳δ铁素体含量,从而提高成型性,耐季节性,耐热加工性和高温抗氧化性,并降低热轧过程中的表面缺陷, 通过减少Ni的含量来节省制造成本。 根据本发明的奥氏体不锈钢的重量%:C:小于0.07%,小于1.0%的Si,小于2.0的Mn,16-18%的Cr,6.0-8.0%的Ni,更少的 超过0.005%的Al,小于0.05%的P,小于0.005%的S,小于0.03%的Ti,小于0.003%的B,小于3.0的Cu,小于0.3%的Mo,小于 0.1%的Nb,小于0.045%的N,余量的Fe和其它不可缺少的杂质。 因此,本发明提高了冲压成型性,耐季节性,耐热加工性和耐高温氧化性。
    • 3. 发明授权
    • Electron gun for a color cathode-ray tube
    • 用于彩色阴极射线管的电子枪
    • US5532547A
    • 1996-07-02
    • US312506
    • 1994-09-26
    • Sang W. ParkHyun C. Kim
    • Sang W. ParkHyun C. Kim
    • H01J29/50H01J29/58
    • H01J29/503H01J2229/4841
    • An electron gun for a color cathode-ray tube, adapted for large television sets or high-definition monitors, has first and second quadrupole electrodes connected to a static voltage focus electrode and to a dynamic voltage focus electrode, respectively, to form a quadrupole lens. The first quadrupole electrode is composed of first electrode pieces connected to the static voltage focus electrode and arranged on left and right sides of three beam-passing apertures formed on the static voltage focus electrode, and each of the first electrode pieces has at least one arc having a radius identical to or larger than that of the beam-passing apertures. The second quadrupole electrode is composed of second electrode pieces connected to upper and lower portions of the dynamic voltage focus electrode, and each of the second electrode pieces has arcs having a radius identical or larger than that of the beam-passing apertures. The first electrode pieces are inserted inside of the second electrode pieces.
    • 适用于大型电视机或高清晰度监视器的用于彩色阴极射线管的电子枪具有分别连接到静态电压聚焦电极和动态电压聚焦电极的第一和第二四极电极以形成四极透镜 。 第一四极电极由连接到静电压聚焦电极并布置在形成在静电压聚焦电极上的三个光束通过孔的左侧和右侧的第一电极片组成,并且每个第一电极片具有至少一个弧 其半径等于或大于光束通过孔的半径。 第二四极电极由连接到动态电压聚焦电极的上部和下部的第二电极片组成,并且每个第二电极片具有等于或大于光束通过孔的半径的弧。 第一电极片插入第二电极片的内部。