热词
    • 5. 发明授权
    • Process for the production of a biaxially highly oriented polypropylene
film
    • 制备双轴取向聚丙烯薄膜的方法
    • US5766532A
    • 1998-06-16
    • US439598
    • 1995-05-12
    • Herbert PeifferUrsula MurschallDetlef BuschHarald Lohmann
    • Herbert PeifferUrsula MurschallDetlef BuschHarald Lohmann
    • B29C55/00C08F8/00B29C55/12
    • B29C55/005C08F8/00B29K2023/12
    • A process for the production of a biaxially oriented propylene polymer film contains, in its single ply (or, if it is a multi-ply film, in its base ply) a low molecular weight resin, and the film has improved stretchability and other desirable physical properties, even though the propylene polymer of the sole or base ply is preferably a homopolymer. The n-heptane-insoluble fraction of the film has a chain isotacticity index, measured by means of .sup.13 C-NMR spectroscopy, of at least 85 to 94%. The sole or base ply contains less than 10% by weight of resin. The film is stretched in such a way that the product of tensile strength in the longitudinal and transverse direction is greater than 50,000 (N/mm.sup.2).sup.2. The film is made by, among other steps, carrying out the orientation in the longitudinal and transverse directions such that the product of the longitudinal stretching ratio and the transverse stretching ratio is.gtoreq.60.
    • 制造双轴取向丙烯聚合物膜的方法在其单层(或者如果是其多层膜中在基底层中)含有低分子量树脂,并且该膜具有改善的拉伸性和其它所需的 物理性质,即使鞋底或底层的丙烯聚合物优选为均聚物。 所述膜的正庚烷不溶级分具有至少85至94%的通过13 C-NMR光谱法测量的链全同立构指数。 底层或底层含有少于10重量%的树脂。 该膜以拉伸强度在纵向和横向上的乘积大于50,000(N / mm 2)2的方式拉伸。 除了其他步骤之外,通过纵向和横向方向进行取向,使得纵向拉伸比和横向拉伸倍数的乘积为> 60°而制成薄膜。