    • 3. 发明授权
    • Linear priction welding of steeples and device thereof
    • 尖塔的直线摩擦焊接及其装置
    • US6022194A
    • 2000-02-08
    • US877844
    • 1997-06-18
    • Dennis Ray AmosSallie Ann Bachman
    • Dennis Ray AmosSallie Ann Bachman
    • F01D5/02F01D5/30F04D29/34
    • F01D5/3061F01D5/02F01D5/3007Y10T29/49321
    • The invention provides a blade-rotating device for rotating a plurality of radially-oriented blades having a blade base with two grooved base sides. The device has a portion, such as a disc or a rotor disc of a turbine, for rotating the blades with the portion having an outer cylindrical surface. The device also has a plurality of steel steeples each having a steeple base and two opposite grooved steeple sides extending therefrom. Each of the opposite steeple sides complements at least one of the grooved sides of at least one of the blade bases. The steeple bases are linear friction welded to the outer cylindrical surface in an approximately longitudinal direction such that the blade bases are engagable with the steel steeples.
    • 本发明提供了一种用于旋转多个径向取向叶片的叶片旋转装置,叶片具有带有两个凹槽基部侧面的叶片基座。 该装置具有一部分,例如涡轮机的盘或转子盘,用于使具有外圆柱形表面的部分转动叶片。 该装置还具有多个钢尖塔,每个具有尖顶基部和从其延伸的两个相对的带槽的尖顶侧。 每个相对的尖锐侧面补充至少一个叶片基部的至少一个带槽侧面。 尖顶基座在大致纵向方向上与外圆柱形表面线性摩擦焊接,使得刀片基座可与钢尖塔接合。
    • 5. 发明授权
    • Turbine rotor modernization and repair method
    • 涡轮转子现代化修复方法
    • US06118098A
    • 2000-09-12
    • US136848
    • 1998-08-19
    • Dennis Ray AmosKent Wixon Beedon
    • Dennis Ray AmosKent Wixon Beedon
    • B23K9/00B23K9/04B23K9/167B23K9/173B23K9/18B23K10/02B23P6/00B65B1/06F01D5/00
    • B23P6/007B23K9/04B65B1/06F01D5/005B23K2201/001
    • This invention relates to an improved method for repairing damaged or worn surfaces of turbine components or upgrading older designs to new, improved designs. This improved method applies to both high pressure and low pressure turbine components applications. This method includes depositing a plurality of individual spaced apart weld volumes onto a prepared surface of a turbine rotor. These individual spaced apart weld volumes form individual fingers without the need to machine the individual fingers from a single rectangular weld volume. Multiple weld volumes are formed concurrently with a space maintain between each weld volume using multiple torches without the problems normally associated with closely spaced welding arcs. Each individual spaced apart weld volume is formed by a plurality of layers of weld metal, with each layer being formed from a single oscillating weld bead to form a predetermined width. The filler wire may be heated by applying a current through the filler wire before it is fed into the weld pool. Welding parameters are also changed to increase the amount of weld deposition without adversely affecting the mechanical weld properties. The invention provides for reduced cycle time for repair work by using multiple torches simultaneously without causing arc instability. The invention also reduces cycle time, by eliminating the need of machining individual fingers on control stages from a single weld volume, by changing the weld buildup of multiple projections, slightly larger than the fingers which hold the blades.
    • 本发明涉及一种用于修复涡轮机部件的损坏或磨损表面或将旧设计升级为新的改进设计的改进方法。 这种改进的方法适用于高压和低压涡轮机部件应用。 该方法包括在涡轮转子的制备表面上沉积多个单独的间隔开的焊接体积。 这些单独的间隔开的焊接体积形成单独的手指,而不需要将单个手指从单个矩形焊接体积加工。 多个焊缝体积与使用多个焊炬的每个焊接体积之间的空间同时形成,而没有通常与紧密间隔的焊接弧相关联的问题。 每个单独的间隔开的焊接体积由多个焊接金属层形成,每个层由单个振荡焊道形成以形成预定宽度。 填充线可以在被送入焊池之前通过将填充线施加电流来加热。 也改变焊接参数以增加焊接沉积的量,而不会不利地影响机械焊接性能。 本发明通过同时使用多个割炬而减少了修理工作的周期时间,而不会导致电弧不稳定。 本发明还通过改变比保持叶片的手指稍大的多个突起的焊缝积聚来消除从单个焊接体积加工单独手指在控制台上的需要,从而缩短了循环时间。
    • 6. 发明授权
    • Optimized welding technique for NiMoV rotors for high temperature
applications
    • 用于高温应用的NiMoV转子的优化焊接技术
    • US5831241A
    • 1998-11-03
    • US778607
    • 1997-01-06
    • Dennis Ray Amos
    • Dennis Ray Amos
    • B23K9/04
    • B23K9/046Y10T29/49321
    • A welding process of repairing a ferrous NiMoV low alloy steel turbine component. A first and a second layer of weld material are welded to the turbine component at electrical current levels chosen so as to prevent a substantial decrease and a substantial increase in the hardness of the component. This method involves selecting these electrical current levels. Additionally, this invention relates to selecting appropriate electrical current levels that minimizes the difference between a maximum and a minimum level of hardness while welding a first and a second layer of weld material. This invention also includes a method for preventing a substantial decrease in the hardness of the component as a result of the welding process.
    • 一种修复含镍NiMoV低合金钢轮组件的焊接工艺。 焊接材料的第一层和第二层以选定的电流水平焊接到涡轮机部件,以防止组件的硬度显着降低和显着提高。 该方法涉及选择这些电流水平。 另外,本发明涉及选择在焊接第一和第二焊接材料层时使最大和最小硬度水平之间的差最小化的合适的电流水平。 本发明还包括一种用于防止由于焊接过程而导致的部件的硬度显着降低的方法。