    • Polysiloxane-polycarbonate block copolymers based on certain
dihydroxydiphenylcycloalkanes
    • 基于某些二羟基二苯基环烷烃的聚硅氧烷 - 聚碳酸酯嵌段共聚物
    • US5068302A
    • 1991-11-26
    • US564473
    • 1990-08-08
    • Peter HorlacherVolker SeriniDieter FreitagUlrich GrigoKarsten-Josef IdelUwe Westeppe
    • Peter HorlacherVolker SeriniDieter FreitagUlrich GrigoKarsten-Josef IdelUwe Westeppe
    • C08G64/00C08G64/18C08G77/42C08G77/448
    • C08G64/186C08G77/448
    • Polydiorganosiloxane-polycarbonate block copolymers based on dihydrodiphenylcycloalkanes corresponding to formula (I) ##STR1## in which R.sup.1, R.sup.2 independently of one another represent hydrogen, halogen, preferably chlorine or bromine, C.sub.1-8 alkyl, C.sub.5-6 cycloalkyl, C.sub.6-10 aryl and C.sub.7-12 aralkyl, preferably phenyl-C.sub.1-4 -alkyl, more especially benzyl,n=2 or 3 andthe substituents R.sup.5 independently of one another are hydrogen or C.sub.1-12 alkyl, with the proviso that at least one of the substituents R.sup.5 is not hydrogen,having an average molecular weight M.sub.w (weight average) in the range from 10,000 to 300,000 (as measured by ultracentrifugation or scattered light measurement) and a content of carbonate containing dihydroxydiphenylcycloalkanes of formula I and, optionally, other diphenols in co-condensed form of from 75% by weight of 99.0% by weight and a content of polydiorganosiloxane having a degree of polymerization Pn of 5 to 300 of from 25% by weight of 1% by weight.
    • 对应于式(I)的二氢二苯基环烷烃的聚二有机硅氧烷 - 聚碳酸酯嵌段共聚物其中R 1,R 2彼此独立地表示氢,卤素,优选氯或溴,C 1-8烷基,C 5-6环烷基,C 6 -10芳基和C7-12芳烷基,优选苯基-C1-4 - 烷基,更特别是苄基,n = 2或3,取代基R5彼此独立地为氢或C 1-12烷基,条件是至少一个 的取代基R5不是氢,平均分子量Mw(重均分子量)为10,000〜300,000(通过超速离心或散射光测定测定)和含有式I的二羟基二苯基环烷烃的碳酸酯的含量,以及任选的其它 共缩合形式的双酚75重量%为99.0重量%,聚二有机硅氧烷的聚合度Pn为5〜300的25重量%的1重量%的含量。
    • 6. 发明授权
    • Thermoplastic molding compositions of a polysiloxane block
copolycarbonate and a polycarbonate based on certain
dihydroxydiphenylcycloalkanes
    • 基于某些二羟基二苯基甲烷的聚硅氧烷嵌段共聚碳酸酯和聚碳酸酯的热塑性成型组合物
    • US5100960A
    • 1992-03-31
    • US493036
    • 1990-03-12
    • Ulrich GrigoPeter HorlacherDieter FreitagKarsten-Josef IdelUwe WesteppeWolfgang BeerWerner Nouvertne
    • Ulrich GrigoPeter HorlacherDieter FreitagKarsten-Josef IdelUwe WesteppeWolfgang BeerWerner Nouvertne
    • C08L69/00C08L83/10
    • C08L69/00C08L83/10
    • The invention relates to a thermoplastic molding composition comprising(A) from 10 to 98 parts by weight of a polydiorganosiloxane-polycarbonate block copolymer having a weight average molecular weight of from 10,000 to 200,000 and containing from 75 to 97.5 wt. % of aromatic carbonate structural units and from 25 to 2.5 wt. % of polydiorganosiloxane structural units;(B) from 2 to 90 parts by weight of a thermoplastic, aromatic polycarbonate having a weight average molecular weight of at least 10,000, andcontaining bifunctional carbonate structural units corresponding to ##STR1## wherein R.sup.1 and R.sup.2 independently represent hydrogen, halogen, C.sub.1 -C.sub.8 alkyl, C.sub.5 -C.sub.6 cycloalkyl, C.sub.6 -C.sub.10 aryl or C.sub.7 -C.sub.12 aralkyl;m represents an integer of from 4 to 7,R.sup.3 and R.sup.4, which may be selected individually for each X, independently represent hydrogen or C.sub.1 -C.sub.6 alkyl; andx represents carbon,with the proviso that, on at least one atom X, R.sup.3 and R.sup.4 both represent alkyl; and(C) from 0.5 to 30 parts by weight of a rubber having a glass transition temperature of less than -20.degree. C.The composition of the invention is useful for the preparation of injection molded articles having an excellent surface and a particularly good toughness at low temperatures.
    • 本发明涉及一种热塑性模塑组合物,其包含(A)10至98重量份的重均分子量为10,000至200,000的聚二有机硅氧烷 - 聚碳酸酯嵌段共聚物,并且含有75至97.5重量% %的芳族碳酸酯结构单元和25〜2.5wt。 %的聚二有机硅氧烷结构单元; (B)2至90重量份的重均分子量为至少10,000的热塑性芳族聚碳酸酯,并且含有对应于(Ia)的双官能碳酸酯结构单元,其中R 1和R 2独立地表示氢,卤素 C 1 -C 8烷基,C 5 -C 6环烷基,C 6 -C 10芳基或C 7 -C 12芳烷基; m表示4至7的整数,可以为每个X单独选择的R 3和R 4独立地表示氢或C 1 -C 6烷基; 并且x表示碳,条件是在至少一个原子X,R 3和R 4都表示烷基; 和(C)0.5〜30重量份玻璃化转变温度低于-20℃的橡胶。本发明的组合物可用于制备具有优异表面和特别良好韧性的注塑制品 在低温下。
    • 8. 发明申请
    • PROCESS FOR THE DISTILLATION OF FATTY ACID ESTERS
    • 消毒脂肪酸酯的方法
    • US20130331588A1
    • 2013-12-12
    • US14000443
    • 2012-03-03
    • Dieter HietschPeter Horlacher
    • Dieter HietschPeter Horlacher
    • C07C67/54C07C69/587
    • C07C67/54C07C67/60C07C69/587C11C1/10C11C3/003
    • The present invention relates to a method for working up a mixture which contains esters of EPA and/or DHA with monohydric alcohols having 1 to 6 carbon atoms, esters of other fatty acids with monohydric alcohols having 1 to 6 carbon atoms, and free cholesterol, wherein the method comprises adding a transesterification catalyst to the mixture, converting at least some of the free cholesterol into esterified cholesterol and thereafter distilling the mixture, wherein the distillation is carried out in such a manner that a product is obtained which contains EPA and/or DHA, both in the form of esters thereof with monohydric alcohols having 1 to 6 carbon atoms, in a higher relative amount, based on all fatty acids in free or bound form present in the product, than said mixture. In addition, the present invention relates to a product which is obtainable by the method according to the invention, wherein the product contains 10 to 99.99% by weight of esters of EPA and/or of DHA with monohydric alcohols having 1 to 6 carbon atoms and 0.0001 to a maximum of 0.3% by weight of cholesterol in free or bound form.
    • 本发明涉及一种用于处理含有EPA和/或DHA的酯与具有1至6个碳原子的一元醇的混合物的混合物的方法,其它脂肪酸与具有1至6个碳原子的一元醇的酯和游离胆固醇, 其中所述方法包括向所述混合物中加入酯交换催化剂,将至少一些游离胆固醇转化为酯化胆固醇,然后蒸馏混合物,其中蒸馏是以获得含有EPA和/或 DHA,以其与具有1至6个碳原子的一元醇的酯的形式,以相对于所述混合物中存在的游离或结合形式的所有脂肪酸的相对量较高。 另外本发明涉及通过本发明的方法获得的产品,其中该产品含有10至99.99重量%的EPA和/或DHA的酯与具有1至6个碳原子的一元醇的酯和 0.0001至最大0.3重量%的游离或结合形式的胆固醇。