会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 3. 发明专利
    • Method for producing dehydrated fluororubber particles
    • 生产脱氢氟橡胶颗粒的方法
    • JP2009161677A
    • 2009-07-23
    • JP2008001760
    • 2008-01-09
    • Daikin Ind Ltdダイキン工業株式会社
    • SENDAN HIROYUKITANAKA YOSHIYUKIKITAHATA HISAHARUHARAGUCHI OKAHIRO
    • C08J3/12B01D33/00B01D35/20
    • PROBLEM TO BE SOLVED: To provide a method for producing dehydrated fluororubber particles with high efficiency without aggregating the highly adhesive hydrous fluororubber particles. SOLUTION: In the method for producing the dehydrated fluororubber particle, the dehydrated fluororubber is produced by vibrating a screen so as to transport the hydrous fluororubber on the screen 1 while jumping up and down to dehydrate the hydrous fluororubber. Concretely, the vibration is applied on the screen along a direction Di intersecting the screen surface Ps. The vibration is preferably applied to the hydrous fluororubber from the transporting direction upstream side Su to the downstream side Sd. The wedge wire screen is obliquely mounted so that the screen surface makes an angle of 70-85° to the vertical direction Dg and the hydrous fluororubber particles are preferably supplied from the high position side Sh onto the wedge wire screen. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种高效率生产脱水氟橡胶颗粒的方法,而不会聚集高粘性含水氟橡胶颗粒。 解决方案:在脱水氟橡胶颗粒的制造方法中,通过使筛网振动,将水合氟橡胶输送到筛网1上,同时上下跳跃以使含水氟橡胶脱水而制造脱水氟橡胶。 具体地说,沿与屏幕表面Ps相交的方向Di在屏幕上施加振动。 振动优选从输送方向上游侧Su向下游侧Sd施加到含水氟橡胶。 楔形丝网被倾斜地安装,使得屏幕表面与垂直方向Dg形成70-85°的角度,并且含水氟橡胶颗粒优选地从高位置侧Sh提供到楔形丝网上。 版权所有(C)2009,JPO&INPIT
    • 4. 发明专利
    • Continuous coagulation method of resin dispersion
    • 树脂分散的连续凝聚方法
    • JP2009173776A
    • 2009-08-06
    • JP2008014066
    • 2008-01-24
    • Daikin Ind Ltdダイキン工業株式会社
    • SENDAN HIROYUKITANAKA YOSHIYUKIKITAHATA HISAHARUHARAGUCHI OKAHIRO
    • C08F6/22
    • PROBLEM TO BE SOLVED: To provide a continuous coagulation method of a resin dispersion that can perfectly coagulate a resin in a resin dispersion in a short time and can easily control the particle size of obtained coagulated particles.
      SOLUTION: The continuous coagulation method of a resin dispersion comprises a first shearing step and a second shearing step. In the first shearing step, first shearing force is applied to the resin dispersion or a coagulated resin dispersion. In the second shearing step, shearing force different from the first shearing force is applied to a coagulated resin dispersion formed from the resin dispersion in the first shearing step or a coagulated resin dispersion obtained through the first shearing step.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种可以在短时间内使树脂分散体中的树脂完全凝固的树脂分散体的连续凝固方法,并且可以容易地控制获得的凝固颗粒的粒径。 解决方案:树脂分散体的连续凝固方法包括第一剪切步骤和第二剪切步骤。 在第一剪切步骤中,对树脂分散体或凝固树脂分散体施加第一剪切力。 在第二剪切步骤中,与第一剪切步骤中的树脂分散体形成的凝固树脂分散体或通过第一剪切步骤获得的凝固树脂分散体施加与第一剪切力不同的剪切力。 版权所有(C)2009,JPO&INPIT
    • 5. 发明专利
    • Process for continuous coagulation of resin dispersion
    • 连续分散树脂分散的方法
    • JP2009173775A
    • 2009-08-06
    • JP2008014065
    • 2008-01-24
    • Daikin Ind Ltdダイキン工業株式会社
    • SENDAN HIROYUKITANAKA YOSHIYUKIHIRAGA YOSHIYUKI
    • C08C1/02
    • PROBLEM TO BE SOLVED: To provide a continuous process for coagulation of resin dispersion, which can continuously coagulate even resin dispersion such as rubber latex without problems, resulting in resin coagulated particles having sizes within a given range. SOLUTION: According to the present process for continuous coagulation of a resin dispersion, in a step for production of fat-coagulated particles, a resin dispersion and a coagulation solution are stirred and mixed by a comminuting blade 32 in a comminution space SPc, while the coagulated resin produced by stirring and mixing of the resin dispersion and the coagulation solution is comminuted with the comminuting blade, to sequentially produce resin coagulated particles having sizes within a defined range, which are continuously fed into a shear space sPs. Further, in a shear step, the resin coagulated particles are continuously delivered into an emission space SPe, while applying shear force onto the resin coagulated particles by fluid delivery blades 34a, 34b, 34c and a fixed blade 111 in the shear space. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了提供可以连续凝固树脂分散体如橡胶胶乳的树脂分散体的连续方法,没有问题,导致尺寸在给定范围内的树脂凝固颗粒。 解决方案:根据本发明的树脂分散体的连续凝固方法,在生产脂肪凝固颗粒的步骤中,将树脂分散体和凝固溶液通过粉碎刀片32在粉碎空间SPc中搅拌和混合 同时通过搅拌和混合树脂分散体和凝固溶液产生的凝固树脂用粉碎刀片粉碎,以顺序地制备尺寸在规定范围内的树脂凝固颗粒,其连续地供入剪切空间sPs。 此外,在剪切步骤中,树脂凝固颗粒被连续地传送到发射空间SPe中,同时在剪切空间中由流体输送叶片34a,34b,34c和固定叶片111在树脂凝固颗粒上施加剪切力。 版权所有(C)2009,JPO&INPIT