    • 4. 发明申请
    • A CARBON PRECURSOR COMPOSITION
    • 碳前列素组合物
    • WO2013188052A1
    • 2013-12-19
    • PCT/US2013/041567
    • 2013-05-17
    • DOW GLOBAL TECHNOLOGIES LLC
    • LAKROUT, HamedMARKS, Maurice, J.VALETTE, Ludovic
    • C08J3/00C04B35/524C04B35/83C08L63/00
    • C04B35/524C04B35/83C04B2235/48C08G59/40C08G59/68C08G59/687C08J3/00
    • A liquid carbon precursor composition including (a) at least one aromatic epoxy resin; and (b)(i) at least one aromatic co-reactive curing agent or (b)(ii) at least one catalytic curing agent, or (b)(iii) a mixture thereof; wherein the liquid composition prior to adding optional components and curing, has a neat viscosity of less than 10,000 mPa-s, at 25 °C; and wherein the liquid precursor composition has a neat viscosity of less than 10,000 mPa-s at 25 °C prior to adding optional components, prior to curing, and prior to carbonizing; and wherein the liquid precursor composition being cured has a carbon yield of at least 35 weight percent as measured in the absence of optional components; a cured liquid carbon precursor composition; a carbonized material made from the above liquid carbon precursor composition; and processes for producing the above compositions.
    • 一种液体碳前体组合物,其包含(a)至少一种芳族环氧树脂; 和(b)(i)至少一种芳族共反应性固化剂或(b)(ii)至少一种催化固化剂,或(b)(iii)它们的混合物; 其中在添加任选组分和固化之前,液体组合物在25℃时具有小于10,000mPa·s的纯粘度; 并且其中所述液体前体组合物在25℃下具有小于10,000mPa·s的洁净粘度,然后在固化之前和在碳化之前加入任选组分。 并且其中固化的液体前体组合物具有至少35重量%的碳收率,在不存在任选组分的情况下测量; 固化液体碳前体组合物; 由上述液态碳前体组合物制成的碳化材料; 以及制备上述组合物的方法。
    • 9. 发明申请
    • A CONDUCTIVE CARBONIZED LAYERED ARTICLE
    • 导电碳化层
    • WO2013188048A1
    • 2013-12-19
    • PCT/US2013/041558
    • 2013-05-17
    • DOW GLOBAL TECHNOLOGIES LLC
    • LAKROUT, HamedMARKS, Maurice, J.VALETTE, Ludovic
    • C08J3/00C04B35/524C04B35/83C08L63/00
    • C09D5/24B82Y10/00C03C17/22C03C2217/28C04B35/524C04B35/6269C04B35/63452C04B2235/9653C08J3/00C08L63/00H01B1/04H01B1/24H01L51/0045H01L51/442Y10T428/265
    • A process for preparing a conductive carbonized layered article including the steps of: (I) providing a liquid carbon precursor formulation comprising (a) at least one aromatic epoxy resin; and (b)(i) at least one aromatic co-reactive curing agent, (b)(ii) at least one catalytic curing agent, or (b)(iii) a mixture thereof; wherein the liquid precursor composition has a neat viscosity of less than 10,000 mPa-s at 25 °C prior to adding optional components, prior to curing, and prior to carbonizing; and wherein the liquid precursor composition being cured has a carbon yield of at least 35 weight percent disregarding the weight of the substrate and any optional components present in the composition; (II) applying the liquid formulation of step (I) as a thin coating layer onto at least a portion of the surface of a substrate; (III) curing the liquid formulation of step (II) to form a cured product, wherein the cured product has a carbon yield of at least 35 weight percent disregarding the weight of the substrate and any optional components present in the composition; and (IV) carbonizing the cured product of step (III) to form a conductive carbonized layered article; and a conductive carbonized layered article such as a carbon optical transparent electrode (COTE) prepared by the above process.
    • 一种制备导电碳化层状制品的方法,包括以下步骤:(I)提供液体碳前体制剂,其包含(a)至少一种芳族环氧树脂; 和(b)(i)至少一种芳族共反应性固化剂,(b)(ii)至少一种催化固化剂,或(b)(iii)它们的混合物; 其中所述液体前体组合物在25℃下具有小于10,000mPa·s的纯粘度,然后在固化之前和在碳化之前加入任选组分。 并且其中固化的液体前体组合物具有至少35重量%的碳收率,而不考虑底物的重量和组合物中存在的任何任选组分; (II)将作为薄涂层的步骤(I)的液体制剂施用到基材表面的至少一部分上; (III)固化步骤(II)的液体制剂以形成固化产物,其中固化产物具有至少35重量%的碳产率,而不考虑基质和组合物中存在的任何任选组分的重量; 和(IV)将步骤(III)的固化产物碳化以形成导电性碳化层压制品; 以及通过上述方法制备的碳光透明电极(COTE)等导电性炭化层叠体。
    • 10. 发明申请
    • EPOXY RESIN COMPOSITIONS
    • 环氧树脂组合物
    • WO2011071745A1
    • 2011-06-16
    • PCT/US2010/058695
    • 2010-12-02
    • DOW GLOBAL TECHNOLOGIES LLCMARKS, Maurice, J.
    • MARKS, Maurice, J.
    • C08G65/22C08L63/00
    • C08G65/223C08G59/245C08L63/00C08L2666/22
    • An epoxy resin composition including a divinylarene dioxide, for example a divinylbenzene dioxide, wherein the divinylarene dioxide has an impurity concentration of less than about 15 weight percent styrenic impurities such as ethylstyrene. Such prepared divinylarene dioxides may be used to prepare curable epoxy resin compositions or formulations, including a blend of a divinylarene dioxide and at least another epoxy resin different from the divinylarene dioxide; and a curable epoxy resin composition including (i) the blend of epoxy resins of the divinylarene dioxide and the at least one epoxy resin different from the divinylarene dioxide; (ii) at least one curing agent; and (iii) optionally, at least one catalyst. The significantly lower concentration of styrenic impurities in the divinylarene dioxides of the present invention provides an epoxy resin composition having low viscosity, better storage stability, and better thermal stability.
    • 包含二乙烯基芳烃二氧化物,例如二乙烯基二氧化苯的环氧树脂组合物,其中二乙烯基芳烃二氧化物的杂质浓度小于约15重量%的苯乙烯杂质如乙基苯乙烯。 这种制备的二乙烯基芳烃二氧化物可用于制备可固化环氧树脂组合物或制剂,包括二乙烯基芳烃二氧化物和至少另一种不同于二乙烯基芳烃二氧化物的环氧树脂的共混物; 和可固化环氧树脂组合物,其包含(i)二乙烯基芳烃二氧化物的环氧树脂与至少一种不同于二乙烯基芳烃二氧化物的环氧树脂的共混物; (ii)至少一种固化剂; 和(iii)任选的至少一种催化剂。 本发明的二乙烯基芳烃二氧化物中苯乙烯杂质的浓度显着降低,提供了具有低粘度,更好的储存稳定性和更好的热稳定性的环氧树脂组合物。