    • 4. 发明授权
    • Process for producing functional vitreous layers
    • 生产功能性玻璃体层的方法
    • US5731091A
    • 1998-03-24
    • US635971
    • 1996-08-01
    • Helmut SchmidtMartin MennigThomas BurkhartClaudia Fink-StraubeGerhard JonschkerMike SchmittAnnette Bauer
    • Helmut SchmidtMartin MennigThomas BurkhartClaudia Fink-StraubeGerhard JonschkerMike SchmittAnnette Bauer
    • C03C14/00C03C17/00C03C17/30C04B41/50C04B41/86C23C18/12B05D5/06
    • C03C14/004C03C14/006C03C14/008C03C17/007C03C17/008C03C17/009C04B41/5022C04B41/86C03C2214/32C03C2217/485C03C2217/92
    • To produce functional vitrous, preferably colored or colloid-dyed layers, a composition produced by hydrolysis and polycondensation of (A) at least on hydrolyzable silane of general formula (I) SiX.sub.4 (I) wherein the radicals X are the same or different and represent hydrolyzable groups or hydroxy groups, or an oligomer derived therefrom, and (B) at least one organosilane of general formula (II) R.sup.1.sub.a R.sup.2.sub.b SiX.sub.(4-a-b) (II) wherein R.sup.1 is a non-hydrolyzable radical, R.sup.2 represents a radical carrying a functional group, X has the meaning given above, and a and b have the values 0, 1, 2 or 3, the sum (a+b) having the values 1, 2 or 3, or an oligomer derived therefrom with an (A):(B) substance ratio of 5-50:50-95, and optionally (C) one or more compounds of glass-forming elements, is mixed with at least one function carrier from the group of temperature-stable dyes or pigments, metallic or non-metallic oxides, coloring metallic ions, metallic or metallic compound colloids, and metal ions that react under reduction conditions to form metallic colloids; the composition mixed with the function carrier is applied onto a substrate and the coating is thermally condensed to form a vitreous layer.
    • PCT No.PCT / EP94 / 03423 Sec。 371日期:1996年8月1日 102(e)日期1996年8月1日PCT 1994年10月18日PCT PCT。 公开号WO95 / 13249 日期1995年5月18日为了生产功能性玻璃色,优选着色或胶体染色层,通过(A)至少在通式(I)SiX 4(I)的可水解硅烷上进行水解和缩聚制备的组合物,其中基团X相同 或者不同,表示可水解基团或羟基,或由其衍生的低聚物,和(B)至少一种通式(II)的有机硅烷R 1 a R 2 b SiX(4-ab)(II)其中R 1是不可水解的基团, 带有官能团的基团X具有上述含义,a和b具有值0,1,2或3,具有值1,2或3的和(a + b)或由其衍生的低聚物 (A):(B)的物质比例为5-50:50-95,和任选的(C)一种或多种玻璃形成元素化合物,与至少一种功能性载体从温度稳定的 染料或颜料,金属或非金属氧化物,着色金属离子,金属或金属化合物胶体和金属 在还原条件下反应形成金属胶体的离子; 将与功能性载体混合的组合物施加到基材上,并将涂层热凝聚以形成玻璃质层。