    • 3. 发明申请
    • METHOD FOR LOCALIZED ANNEALING OF CHEMICALLY STRENGTHENED GLASS
    • 化学强化玻璃的局部退火方法
    • WO2015031151A1
    • 2015-03-05
    • PCT/US2014/052037
    • 2014-08-21
    • CORNING INCORPORATED
    • CLEARY, Thomas, MichaelFRISKE, Mark, StephenWAGNER, Robert, Stephen
    • C03B25/08B32B17/10C03C21/00
    • C03B25/08B32B17/10091B32B17/10137B32B17/10743B32B17/10761B32B17/1077B32B17/10788B32B2605/00C03C21/00C03C23/0025C03C23/0065
    • A method of providing locally annealed regions for a glass article comprising: (a) providing a strengthened glass article having a first surface compressive stress and a first depth of layer of compressive stress; (b) targeting first portions of the glass article on a first side thereof; (c) annealing the targeted first portions to a second surface compressive stress and a second depth of layer of compressive stress; and (d) repeating steps (b) and (c) to create a pattern of annealed portions of the glass article on the first side thereof. Targeted annealing can be done e.g. by focusing a laser or using microwave energy or an induction source. A method for making a laminate structure comprising a first glass layer (12), a second glass layer (16), and at least one polymer interlayer (14) intermediate the first and second glass layers. The first glass layer (12) can be comprised of a strengthened glass having a first portion with a first surface compressive stress and a first depth of layer of compressive stress and a second portion with a second surface compressive stress and a second depth of layer of compressive stress. In other embodiments, the second glass layer (16) can be comprised of a strengthened glass having a third portion with a third surface compressive stress and a third depth of layer of compressive stress and a fourth portion with a fourth surface compressive stress and a fourth depth of layer of compressive stress.
    • 提供一种用于玻璃制品的局部退火区域的方法,包括:(a)提供具有第一表面压缩应力和压缩应力层的第一深度的强化玻璃制品; (b)在玻璃制品的第一侧上对准第一部分玻璃制品; (c)将目标第一部分退火到第二表面压缩应力和压缩应力层的第二深度; 和(d)重复步骤(b)和(c)以在其第一侧上产生玻璃制品的退火部分的图案。 目标退火可以例如进行。 通过聚焦激光或使用微波能量或感应源。 一种制造层压结构的方法,包括第一玻璃层(12),第二玻璃层(16)和至少一个位于第一和第二玻璃层之间的聚合物中间层(14)。 第一玻璃层(12)可以由具有第一部分的强化玻璃构成,第一部分具有第一表面压缩应力和第一压缩应力层,第二部分具有第二表面压缩应力和第二深度层 压应力。 在其他实施例中,第二玻璃层(16)可以由具有第三部分的第三表面压缩应力和第三压缩应力层深度的加强玻璃和具有第四表面压应力的第四部分组成, 压应力层深度。
    • 6. 发明公开
    • METHOD FOR LOCALIZED ANNEALING OF CHEMICALLY STRENGTHENED GLASS
    • VERFAHREN ZUMÖRTLICHENGLÜHENVON CHEMISCHVERSTÄRKTEMGLAS
    • EP3038979A1
    • 2016-07-06
    • EP14758474.2
    • 2014-08-21
    • Corning Incorporated
    • CLEARY, Thomas, MichaelFRISKE, Mark, StephenWAGNER, Robert, Stephen
    • C03B25/08B32B17/10C03C21/00
    • C03B25/08B32B17/10091B32B17/10137B32B17/10743B32B17/10761B32B17/1077B32B17/10788B32B2605/00C03C21/00C03C23/0025C03C23/0065
    • A method of providing locally annealed regions for a glass article comprising: (a) providing a strengthened glass article having a first surface compressive stress and a first depth of layer of compressive stress; (b) targeting first portions of the glass article on a first side thereof; (c) annealing the targeted first portions to a second surface compressive stress and a second depth of layer of compressive stress; and (d) repeating steps (b) and (c) to create a pattern of annealed portions of the glass article on the first side thereof. Targeted annealing can be done e.g. by focusing a laser or using microwave energy or an induction source. A method for making a laminate structure comprising a first glass layer (12), a second glass layer (16), and at least one polymer interlayer (14) intermediate the first and second glass layers. The first glass layer (12) can be comprised of a strengthened glass having a first portion with a first surface compressive stress and a first depth of layer of compressive stress and a second portion with a second surface compressive stress and a second depth of layer of compressive stress. In other embodiments, the second glass layer (16) can be comprised of a strengthened glass having a third portion with a third surface compressive stress and a third depth of layer of compressive stress and a fourth portion with a fourth surface compressive stress and a fourth depth of layer of compressive stress.
    • 一种为玻璃制品提供局部退火区域的方法,包括:(a)提供具有第一表面压缩应力和压缩应力层的第一深度的强化玻璃制品; (b)将玻璃制品的第一面的第一面朝向第一侧; (c)将目标第一部分退火到第二表面压缩应力和压缩应力层的第二深度; 和(d)重复步骤(b)和(c)以在其第一侧上产生玻璃制品的退火部分的图案。 靶向退火可以例如进行。 通过聚焦激光或使用微波能量或感应源。 一种制造层压结构的方法,包括第一玻璃层(12),第二玻璃层(16)和至少一个在第一和第二玻璃层之间的聚合物中间层(14)。 第一玻璃层(12)可以由具有第一部分的加强玻璃构成,第一部分具有第一表面压缩应力和第一压缩应力层,第二部分具有第二表面压缩应力和第二深度层 压应力。 在其它实施例中,第二玻璃层(16)可以由具有第三部分的第三表面压缩应力和第三压缩应力层深度的加强玻璃和具有第四表面压应力的第四部分组成, 压应力层深度。