    • 2. 发明申请
    • RUBBER COMPOSITIONS WITH FILLER AND KETOXIME OR KETOXIMO SILANE
    • 橡胶组合物与填充剂和KETOXIME或KETOXIMO SILANE
    • WO2012031005A3
    • 2012-05-31
    • PCT/US2011050036
    • 2011-08-31
    • BRIDGESTONE CORPLIN CHENCHY JEFFREYCHEN YAOHONGFUKUSHIMA ATSUSHIHERGENROTHER WILLIAM LHOGAN TERRENCE E
    • LIN CHENCHY JEFFREYCHEN YAOHONGFUKUSHIMA ATSUSHIHERGENROTHER WILLIAM LHOGAN TERRENCE E
    • C08K5/5465C08K3/04C08K3/36C08K9/06C08L9/00
    • C08K5/5465C08K3/04C08K5/548C08L9/06C08L91/00C08L21/00
    • A composition includes an elastomer and a ketoximo silane or a ketoxime additive. The ketoximo silane corresponds to Formula I: where D is selected from a C1 to C60 hydrocarbyl group, or when A is 0 or 1 a hydrogen, or the structure in Formula III; and wherein n and j are independently 1, 2, or 3, m and q are independently 0 or 1, z and t are independently 0 or 1 and (n + m +z) is equal to 3 and (j + q + t) is equal to 3; A is 0 or greater than or equal to 1; R1 and R2 are independently Ci to C60 divalent organic groups and may optionally include O, N S, Si, and/or P heteroatoms with the proviso that when A is 0 either of R1 and R2 may be a chemical bond; R3, R4, R8 and R9 are independently a hydrogen, or a C1 to C60 hydrocarbyl or alkoxy group optionally including O, N, S, Si and/or P; R5 and R6 are independently hydrogen or C1 to C60 hydrocarbyl groups and may optionally include O, N S, Si, and/or P heteroatoms, and may optionally be bonded together to form a cyclic ring; R10 and R11 are independently hydrogen or C1 to C60 hydrocarbyl groups and may optionally include O, N S, Si, and/or P heteroatoms, and may optionally be bonded together to form a cyclic ring.
    • 组合物包括弹性体和酮肟基硅烷或酮肟添加剂。 酮肟基硅烷对应于式I:其中D选自C1至C60烃基,或当A为0或1时为氢或式III中的结构; 并且其中n和j独立地为1,2或3,m和q独立地为0或1,z和t独立地为0或1,并且(n + m + z)等于3且(j + q + t )等于3; A为0或大于或等于1; R 1和R 2独立地为C 1至C 60二价有机基团,并且可任选地包括O,N S,Si和/或P杂原子,条件是当A为0时,R 1和R 2可以是化学键; R 3,R 4,R 8和R 9独立地为氢或任选包括O,N,S,Si和/或P的C 1至C 60烃基或烷氧基; R 5和R 6独立地是氢或C 1至C 60烃基,并且可任选地包括O,N S,Si和/或P杂原子,并且可以任选地结合在一起形成环状环; R 10和R 11独立地为氢或C 1至C 60烃基,并且可以任选地包括O,N S,Si和/或P杂原子,并且可以任选地结合在一起形成环状环。
    • 4. 发明申请
    • METHOD OF PRODUCING A TIRE COMPOSITION HAVING IMPROVED SILICA REINFORCEMENT
    • 生产具有改进的二氧化硅增强的轮胎组合物的方法
    • WO2005105854A3
    • 2005-12-29
    • PCT/US2005014561
    • 2005-04-27
    • BRIDGESTONE CORPLIN CHENCHY JEFFREYARAKI SHUNJIZHOU HAIYING
    • LIN CHENCHY JEFFREYARAKI SHUNJIZHOU HAIYING
    • C08C19/00C08K3/36C08K5/17C08K5/54C08L9/06
    • C08J3/203C08J2321/00C08K3/36C08K5/17C08L21/00
    • A method for preparing a vulcanizable elastomeric composition, the method comprising the steps of: (a) mixing, at a mixer temperature of at least 25 °C, an elastomer having a silica-interactive functional group, a filler comprising silica, and optionally a catalyst, to form an initial composition, where said initial composition comprises less than 5 parts by weight of any of zinc oxide, sulfure, or cure agents per hundred parts by weight rubber; (b) mixing the initial composition obtained in steps (a), at a surface temperature of from 70 °C to 175 °C, optionally with a silica coupling agent, a silica processing aid and additional filler, to form an intermediate composition; and (c) mixing the intermediate composition obtained in step (b), at a surface temperature lower than a vulcanization temperature, with a cure agent, and, optionally, a cure accelerator, to form a vulcanizable elastomer composition.
    • 一种制备可硫化弹性体组合物的方法,所述方法包括以下步骤:(a)在至少25℃的混合器温度下将具有二氧化硅相互作用官能团的弹性体,包含二氧化硅的填料和任选的 催化剂以形成初始组合物,其中所述初始组合物包含每100重量份橡胶小于5重量份的氧化锌,硫化剂或固化剂中的任一种; (b)将步骤(a)中获得的初始组合物,在70℃至175℃的表面温度下,任选地与二氧化硅偶联剂,二氧化硅加工助剂和另外的填料混合以形成中间体组合物; 和(c)在低于硫化温度的表面温度下,将步骤(b)中获得的中间体组合物与固化剂和任选的固化促进剂混合以形成可硫化弹性体组合物。
    • 6. 发明专利
    • Compuesto de caucho reforzado con sílice con baja emisión de compuestos orgánicos volátiles (COV)
    • ES2624856T3
    • 2017-07-17
    • ES10075613
    • 2006-03-23
    • BRIDGESTONE CORP
    • HERGENROTHER WILLIAM LLIN CHENCHY JEFFREYHOGAN TERRENCE EHILTON ASHLEY
    • C08G77/28B60C1/00C08L21/00
    • Una mezcla de silsesquioxanos modificados con alcoxi, comprendiendo los silsesquioxanos modificados con alcoxi uno o más compuestos seleccionados del grupo que consiste en silsesquioxanos modificados con alcoxi que tienen la fórmula**Fórmula** y mezclas de los mismos, en donde w, x e y representan fracciones molares, y no es igual a cero, cualquiera de w o x, pero no ambos, pueden ser cero, y w +x + y >= 1,00, en donde R1, R2 y R3 son iguales o diferentes, y se seleccionan del grupo que consiste en (i) H o un grupo alquilo que tiene de uno a 20 átomos de carbono, (ii) grupos cicloalquilo que tienen de 3 a 20 átomos de carbono, (iii) grupos alquilarilo que tienen de 7 a 20 átomos de carbono, y (iv) R5X, en donde X se selecciona del grupo que consiste en Cl, Br, SH, SaR6, NR62, OR6, CO2H, SCOR6, CO2R6, OH, olefinas, epóxidos, grupos amino, grupos vinilo, acrilatos y metacrilatos, en donde a >= 1 a 8, R5 se selecciona del grupo que consiste en grupos alquileno que tienen de uno a 20 átomos de carbono, grupos cicloalquileno que tienen de 3 a 20 átomos de carbono, y R4 y R6 se seleccionan del grupo que consiste en grupos alquilo que tienen de uno a 5 átomos de carbono, grupos cicloalquilo que tienen de 3 a 20 átomos de carbono, y grupos alquilarilo que tienen de 7 a 20 átomos de carbono, en donde los silsesquioxanos modificados con alcoxi consisten esencialmente en una mezcla de silsesquioxanos modificados con alcoxi que tienen una estructura abierta con un grupo alcoxisililo reactivo, y están esencialmente libres de organosilsesquioxanos poliédricos con estructura de jaula cerrada, y en donde la mezcla de silsesquioxanos modificados con alcoxi libera de 0,05% a 10% en peso de alcohol cuando se trata mediante hidrólisis ácida prácticamente total.