会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 6. 发明申请
    • POLYPROPYLENE COMPOSITION WITH HIGH STIFFNESS AND IMPACT STRENGTH
    • 具有高强度和抗冲击强度的聚丙烯组合物
    • WO2010089121A1
    • 2010-08-12
    • PCT/EP2010/000701
    • 2010-02-04
    • BOREALIS AGGAHLEITNER, MarkusMALM, BoBERNREITNER, KlausBRAUN, Juliane
    • GAHLEITNER, MarkusMALM, BoBERNREITNER, KlausBRAUN, Juliane
    • C08F10/06C08K3/00
    • C08F10/00C08F10/06C08F110/06C08F4/6543C08F4/6492C08F4/651C08F210/16C08F2500/04C08F2500/19C08F2500/12C08F2500/11C08F2500/20C08F2500/24
    • The present invention is directed to a polypropylene composition comprising a propylene homo- or copolymer (A) with a polydispersity index (Pl), determined according ISO 6721-1, of at least 5.8 Pa -1 ; and an inorganic filler (B) in an amount from 2.0 to 20 parts per weight based on 100 parts per weight of (A) + (B); The present invention is furthermore directed to a polypropylene composition comprising - a propylene homo- or copolymer (A); and an inorganic filler (B); whereby the following relation is fulfilled (80 F + 1700) MPa ≤ T wherein F are the parts per weight of component (B) based on 100 parts per weight of the total amount of (A) + (B). T is the tensile modulus in MPa, determined according to ISO 527-2, of the polypropylene composition measured on a test specimen prepared by injection molding according to ISO 1873-2. The present invention is also directed to a process for the production of the polypropylene compositions according to the invention and to an article made of the polypropylene compositions according to the invention. The present invention is furthermore directed to the use of the polypropylene compositions according to the invention for the production of pipes, car components, appliance housings, transport containers.
    • 本发明涉及一种聚丙烯组合物,其包含根据ISO 6721-1测定的至少5.8Pa-1的具有多分散指数(Pl)的丙烯均聚物或共聚物(A) 和每100重量份(A)+(B))为2.0〜20重量份的无机填料(B)。 本发明还涉及包含丙烯均聚物或共聚物(A)的聚丙烯组合物; 和无机填料(B); 由此满足以下关系(80 F + 1700)MPa = T其中F是基于(A)+(B)的总量的100重量份,组分(B)的每重量份数。 T是根据ISO 527-2测定的根据ISO 1873-2通过注射成型制备的试样上测量的聚丙烯组合物的拉伸弹性模量(MPa)。 本发明还涉及一种生产根据本发明的聚丙烯组合物和由本发明的聚丙烯组合物制成的制品的方法。 本发明还涉及根据本发明的聚丙烯组合物用于生产管道,汽车部件,电器外壳,运输容器的用途。