    • METHOD FOR PRODUCING A DEEP-DRAWN FILM PART FROM A THERMOPLASTIC MATERIAL
    • 用于生产深拉薄膜部分热塑性
    • WO2009043539A2
    • 2009-04-09
    • PCT/EP2008008182
    • 2008-09-26
    • BAYER MATERIALSCIENCE AGNIEBLING CURTMEYER KLAUS
    • NIEBLING CURTMEYER KLAUS
    • B29C51/42
    • B29C51/421B29C47/0021B29C47/043B29C47/065B29C51/002B29C51/02B29C51/10B29C51/14B29C51/16B29C51/422B29C51/46B29C2035/0822B29C2791/007B29C2795/002B29K2033/12B29K2069/00B29K2075/00B29K2705/00B29L2031/3008
    • The invention relates to a method for producing a deep-drawn film part that is at least partially imprinted, metallized and/or otherwise coated. The method comprises the following steps: making available a plain piece of film from a thermoplastic material that is at least partially imprinted, metallized and/or otherwise coated on one or both surfaces and that comprises at least one film section that corresponds to the deep-drawn part to be produced in terms of its size and imprint, metallization and/or coating; applying said piece of film in a defined orientation to a frame, only the edge sections of the piece of film lying on the frame; introducing the piece of film lying on the frame into a heating zone and heating at least the film section to a predetermined temperature; and quickly introducing the piece of film so heated into a deformation zone and subjecting it indirectly or directly to a pressure medium pressure of more than 20 bar by means of a fluid pressure medium and deforming it isotactically to the desired deep-drawn part in a period of less than 5 seconds. The method is characterized in that the heating step is carried out in such a manner that at least one side of the entire film section or of most of the part of the film section has a film surface temperature in the range of 10 to 65°C above the Vicat softening point B/50.
    • 一种用于一制备方法中,至少部分地印刷,金属化和/或以其他方式涂覆深拉膜的一部分,其至少包括以下方法步骤:提供一平面的,在一个或两个表面(S)至少部分地印刷,金属化和/或以其他方式 提供了一种从至少一种热塑性材料薄膜包衣片,它包括的薄膜至少对应于深拉部分的截面到关于大小及印刷,金属化和/或涂覆来制造; 这块薄膜装配在限定的排列到一个帧时,只在所述框架上的片膜静息的的边际部分; 使得搁置在框架件的膜被引入到加热区中,加热存在和至少膜的部分,以规定的温度; 并且将这样加热的薄膜片然后被引入迅速进入一个变形区域和有具有大于20巴的加压介质的压力下的流体压力介质立即并直接进行和等静压变形,其特征在于,进行这样的加热的小于5秒的时间段内的期望深冲件 是使得膜的整个部分或具有在10的范围内的膜表面温度的薄膜部分的至65℃的主要部分的维卡软化温度B /第50次以上的至少一个侧