    • 1. 发明专利
    • BR102012024229A2
    • 2013-08-06
    • BR102012024229
    • 2012-09-24
    • BAYER IP GMBHSTARCK H C GMBH
    • BULAN ANDREASWEBER RAINERALBRECHT SVENMEESE-MARKTSCHEFFEL JULIANEOBRICH ARMIN
    • C25B11/04C25B11/08
    • A silver oxide is precipitated at 20-80[deg] C by simultaneously adding an aqueous sodium-hydroxide solution and silver nitrate solution to receiver vessel, using a mechanical stirrer to introduce stirring energy of 0.01-10 W/l, and pH is maintained constant to 10-12. The precipitated silver oxide is removed from the suspension. The silver oxide is dried at 80-200[deg] C. The silver oxide is processed with an electroconductive carrier material to obtain a flat oxygen-consuming electrode. A silver oxide is precipitated at 20-80[deg] C by simultaneously adding an aqueous sodium-hydroxide solution and silver nitrate solution to receiver vessel, using a mechanical stirrer to introduce stirring energy of 0.01-10 W/l, and pH is maintained constant to 10-12. The precipitated silver oxide is removed from the suspension. The silver oxide is dried at 80-200[deg] C, optionally under reduced pressure and under inert gas atmosphere. The silver oxide is processed with an electroconductive carrier material, catalyst comprising silver particles, and finely-divided fluorinated polymer to obtain a flat oxygen-consuming electrode. An independent claim is included for electrolysis cell for electrolysis of alkali metal chloride, which comprises oxygen-consuming electrode as cathode.