    • 3. 发明专利
    • Corrosion testing method
    • 腐蚀试验方法
    • JP2010286464A
    • 2010-12-24
    • JP2009183051
    • 2009-08-06
    • Autonetworks Technologies LtdSumitomo Electric Ind LtdSumitomo Wiring Syst Ltd住友電気工業株式会社住友電装株式会社株式会社オートネットワーク技術研究所
    • NISHIKAWA TAICHIROKUSAKARI MISATOOTSUKA YASUYUKIYAMANO YOSHIAKISAKURA KAZUNARIFURUKAWA KINGOITO TAKAAKI
    • G01N27/26G01N17/02
    • PROBLEM TO BE SOLVED: To provide a corrosion testing method and a corrosion testing system suitable for evaluating a corrosion resistance of an electric wire with terminal utilized in an environment in which corrosion advances relatively slowly.
      SOLUTION: This corrosion testing method includes the steps of preparing a pair of samples 1 having a terminal member 11 attached to the end of the electric wire 10 provided with an insulation layer 10i on an outer circumference of a conductor 10c; arranging each of the samples 1 with the terminal members 11 thereof separated from each other; preparing an electrolyte carrier 4 having an electrolyte adhered to a granular surface of a nonmetallic insulating material; bringing the electrolyte carrier into contact with both the terminal members 11 and arranging the same so as to be interposed between both the terminal members 11; charging the samples 1 into a constant-temperature, constant-humidity device 2 in this state to hold at a constant temperature and a constant humidity; and applying a constant voltage to both the samples 1 for a predetermined time by a voltage application device 3. A fluid containing electrolyte generated by the electrolyte of the electrolyte carrier 4 and moisture in an atmosphere of the constant-temperature, constant-humidity device 2 is interposed between both the terminal members 11. Utilizing this fluid, a leak current runs and corrodes the terminal members 11.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种腐蚀测试方法和腐蚀测试系统,其适用于在腐蚀进展相对较慢的环境中评估具有端子的电线的耐腐蚀性。 解决方案:该腐蚀测试方法包括制备一对样品1的步骤,该样品1具有附着到在导体10c的外圆周上设置有绝缘层10i的电线10的端部的端子构件11; 将每个样品1与其端子构件11彼此分离; 制备电解质载体4,其具有粘附到非金属绝缘材料的颗粒表面的电解质; 使电解质载体与两个端子构件11接触并将其布置成插入在两个端子构件11之间; 在这种状态下将样品1装入恒温恒湿装置2中以保持恒温和恒湿; 并通过电压施加装置3向样品1施加恒定电压达预定时间。含有由电解质载体4的电解质产生的电解质和在恒温恒湿装置2的气氛中的水分的流体 插入在两个端子构件11之间。利用该流体,泄漏电流运行并腐蚀端子构件11.版权所有(C)2011,JPO和INPIT