    • 4. 发明授权
    • Surface modified nozzle plate
    • 表面改性喷嘴板
    • US6151045A
    • 2000-11-21
    • US235578
    • 1999-01-22
    • Bradley Leonard BeachSean David SmithTonya Harris JacksonJing Xiao Sun
    • Bradley Leonard BeachSean David SmithTonya Harris JacksonJing Xiao Sun
    • B41J2/14B41J2/16B41J2/135
    • B41J2/1606B41J2/1433B41J2002/14491
    • The specification describes a method and composition for treating selected areas of the surface of a polyimide material used to make a nozzle plate for an ink jet printer in order to decrease the surface energy of the polyimide material so ink repellency of the material is increased in the selected areas. The method includes applying a polydialkylsiloxane having reactive end groups to the selected areas of the polyimide material and curing the polydialkylsiloxane on the surface to provide a surface having decreased surface energy. A particularly preferred polydialkylsiloxane is an amine terminated polydialkylsiloxane having a molecular weight ranging from about 500 to about 40,000 number average molecular weight. Because the polydialkylsiloxane is relatively stable at the adhesive curing temperatures used to bond the nozzle plate to a semiconductor chip, the polydialkylsiloxane can be applied prior to curing the adhesive thereby reducing the steps required to provide nozzle plates having decreased ink wettability.
    • 本说明书描述了一种用于处理用于制造用于喷墨打印机的喷嘴板的聚酰亚胺材料的表面的选定区域的方法和组合物,以便降低聚酰亚胺材料的表面能,因此在 选区。 该方法包括将具有反应性端基的聚二烷基硅氧烷应用于聚酰亚胺材料的选定区域并固化表面上的聚二烷基硅氧烷以提供具有降低的表面能的表面。 特别优选的聚二烷基硅氧烷是分子量范围为约500至约40,000数均分子量的胺封端的聚二烷基硅氧烷。 由于聚二烷基硅氧烷在用于将喷嘴板结合到半导体芯片的粘合剂固化温度下相对稳定,因此可以在固化粘合剂之前施加聚二烷基硅氧烷,从而减少提供具有降低的油墨润湿性的喷嘴板所需的步骤。
    • 5. 发明授权
    • Method for forming and inspecting a barrier layer of an ink jet print
cartridge
    • 用于形成和检查喷墨打印墨盒的阻挡层的方法
    • US5953032A
    • 1999-09-14
    • US872509
    • 1997-06-10
    • Leea Danielle HaarzTonya Harris JacksonJeanne Marie Saldanha Singh
    • Leea Danielle HaarzTonya Harris JacksonJeanne Marie Saldanha Singh
    • B41J2/175B41J2/16
    • B41J2/14072B41J2/1603B41J2/1623
    • A process is provided for forming a barrier layer over one or more extending sections of a flexible circuit and one or more bond pads of a print cartridge printhead using an encapsulant material and subsequently inspecting the print cartridge to determine if the encapsulant material has been properly placed on the print cartridge. The process involves providing an inspection mark on an orifice plate of the printhead before the barrier layer is formed. After the barrier layer has been formed, an inspection is made to determine if the barrier layer extends beyond the inspection mark and contacts a second portion of the print cartridge. If it does, then the print cartridge is unacceptable. If not, then the print cartridge is acceptable. Alternatively, the location of the barrier layer may be considered unacceptable if it contacts any portion of the inspection mark even though it may not contact the second portion of the print cartridge.
    • 提供了一种方法,用于在柔性电路的一个或多个延伸部分和打印墨盒打印头的一个或多个接合焊盘之间使用密封材料形成阻挡层,随后检查打印墨盒以确定密封剂材料是否已经被正确放置 在打印碳粉盒上。 该方法包括在形成阻挡层之前在打印头的孔板上提供检查标记。 在形成阻挡层之后,进行检查以确定阻挡层是否延伸超过检查标记并接触打印碳粉盒的第二部分。 如果是,则打印墨盒是不可接受的。 如果没有,那么打印墨盒是可以接受的。 或者,如果阻挡层的位置接触到检查标记的任何部分,即使其不接触打印碳粉盒的第二部分,也可认为是不可接受的。