    • 7. 发明授权
    • Phosphor and manufacturing method therefore, and light source using the phosphor
    • 因此,荧光体和制造方法,以及使用荧光体的光源
    • US07476335B2
    • 2009-01-13
    • US11063847
    • 2005-02-23
    • Kenji SakaneAkira Nagatomi
    • Kenji SakaneAkira Nagatomi
    • C09K11/59C09K11/64C09K11/55
    • C09K11/7709C04B35/584C04B35/597C04B2235/3224C04B2235/3852C04B2235/3865C04B2235/3873C04B2235/3895C04B2235/5409C04B2235/5436C09K11/0883C09K11/7734
    • To provide a phosphor having a broad emission spectrum with a peak in the range from yellow color to red color (wavelength from 570 nm to 620 nm), having a flat excitation band with large area on the long wavelength side from near ultraviolet/ultraviolet to green color (wavelength from 250 nm to 550 nm), and excellent in emission intensity and luminance, and a method of manufacturing the same, and also a light source such as white LED using the phosphor. As raw materials, Ca3N2(2N), AlN(3N), Si3N4(3N), and Eu2O3(3N) are prepared, and out of each raw material, 0.950/3 mol of Ca3N2, 2 mol of AlN, 4/3 mol of Si3N4, and 0.050/2 mol of Eu2O3 are weighed, and the raw materials thus weighed are mixed by using a mortar. The raw materials thus mixed are put in a BN crucible, and retained/fired for 3 hours at 1700° C. in a nitrogen atmosphere, and thereafter cooled from 1700° C. to 200° C., to thereby obtain the phosphor expressed by a composition formula Ca0.950Al2Si4O0.075N7.917:Eu0.050.
    • 为了提供具有从黄色到红色(波长从570nm到620nm)的范围内的峰的宽发射光谱的荧光体,具有从近紫外/紫外到长波长侧具有大面积的平坦激发带 绿色(波长从250nm至550nm),发光强度和亮度优异,以及其制造方法,以及使用荧光体的白光LED等光源。 作为原料,制备Ca3N2(2N),AlN(3N),Si3N4(3N)和Eu2O3(3N),在每种原料中,加入0.950 / 3mol Ca 3 N 2,2mol AlN,4/3 mol 的Si 3 N 4和0.050 / 2mol的Eu 2 O 3,并将这样称重的原料用研钵混合。 将这样混合的原料放入BN坩埚中,在氮气氛中在1700℃下保持/烧成3小时后,从1700℃冷却至200℃,得到由 组成式<?in-line-formula description =“In-line Formulas”end =“lead”?> Ca0.950Al2Si4O0.075N7.917:Eu0.050。<?in-line-formula description =“In-line 公式“end =”tail“?>
    • 8. 发明授权
    • Light source having phosphor including divalent trivalent and tetravalent elements
    • 具有包含二价三价和四价元素的荧光体的光源
    • US07432647B2
    • 2008-10-07
    • US10932108
    • 2004-09-02
    • Akira NagatomiMasahiro GotohKenji SakaneShuji Yamashita
    • Akira NagatomiMasahiro GotohKenji SakaneShuji Yamashita
    • H01J1/62H01J63/04C09K11/02C09K11/08
    • C09K11/0883C09K11/7734Y02B20/181
    • A phosphor having an excitation band relative to lights in the wide range of wavelengths from ultraviolet to visible light, and having an emission spectrum in the red range and so on, with a wide half value width, and an LED and a light source using the phosphor and emitting white and other color lights with good color rendering properties are provided. Powdered raw materials of Ca3N2 (2N), CaO (2N), AlN (3N), Si3N4 (3N), and Eu2O3 (3N) are prepared, and the respective raw materials are mixed to have a mole ratio of the respective elements of Ca:Al:Si:Eu=0.985:1:1:0.015. The mixed raw materials are fired at 1000° C. or higher in an inert atmosphere for three hours, and thereafter pulverized to obtain a phosphor having a composition of CaAlSiN2.83O0.25:Eu, which is one example of the phosphor satisfying the above described object. Furthermore, by combining the phosphor with an appropriate LED or a light source emitting from ultraviolet light to visible light, the LED and the light source emitting white and other color lights with good color rendering properties can be obtained.
    • 具有相对于从紫外线到可见光的宽波长范围内的光的激发带的荧光体,具有宽半值宽度的红色范围等的发光光谱,以及使用该光源的LED和光源 提供了具有良好显色性能的荧光粉和发出白色等彩色灯。 Ca 3 N 2(2N),CaO(2N),AlN(3N),Si 3 N 4的粉末原料 (3N)和Eu 2 O 3(3N),并将各原料混合以使各原料的摩尔比为 Ca:Al:Si:Eu = 0.985:1:1:0.015。 将混合的原料在惰性气氛中在1000℃以上煅烧3小时,然后粉碎,得到组成为CaAlSiN 2.83 O 0.25的磷光体, :Eu是满足上述目的的荧光体的一个例子。 此外,通过将荧光体与适当的LED或从紫外光发射到可见光的光源组合,可以获得发光白色和其它具有良好显色特性的彩色光的光源。