    • A METHOD FOR MANUFACTURING A WROUGHT METAL PLATE PRODUCT HAVING A GRADIENT IN ENGINEERING PROPERTIES
    • 一种制造具有工程特性等级的金属板制品的方法
    • WO2009043426A1
    • 2009-04-09
    • PCT/EP2008/007378
    • 2008-09-09
    • ALERIS ALUMINUM KOBLENZ GMBHTEN CATE, AndreasKHOSLA, SunilBÜRGER, AchimSPANGEL, Sabine, Maria
    • TEN CATE, AndreasKHOSLA, SunilBÜRGER, AchimSPANGEL, Sabine, Maria
    • C22F1/04C22C21/00
    • C22F1/04C22C21/00
    • The present invention provides a method for manufacturing a heat-treatable wrought metal plate product having a length, width and thickness direction, and having a gradient in engineering properties along at least one dimension of length or width direction of the plate product, comprising the steps of: a) providing a wrought metal plate product selected from a rolled, extruded or forged product, b) subjecting the plate product to a solution heat treatment, and c) rapidly cooling the plate product, d) ageing the cooled product comprising heat treating for time to arrive at different tempers across at least one dimension in a length or width direction of the plate product, said heat treating comprising heating the plate to raise temperature of the plate to temperature T1 at or above ambient temperature, and applying to the heated plate a temperature gradient between temperature T2 and T3, wherein T2>T1 and T2>T3, wherein T3 is at or above ambient temperature, across at least one length or width or thickness direction of the plate by applying a controlled heat- input into the plate from one side of the plate product to temperature T2 and a controlled cooling to temperature T3 from the plate product at the opposite side of the controlled heat- input, and ageing the product plate while applying the temperature gradient between T2 and T3.
    • 本发明提供一种制造具有长度,宽度和厚度方向的可热处理锻造金属板产品的方法,并且沿着板材产品的长度或宽度方向的至少一个尺寸具有工程特性的梯度,该方法包括以下步骤 a)提供选自轧制,挤压或锻造产品的锻造金属板产品,b)使板材经受固溶热处理,和c)快速冷却板产品,d)使包含热处理的冷却产品 为了时间到达板产品的长度或宽度方向上的至少一个尺寸的不同的温度,所述热处理包括加热板以将板的温度升高到等于或高于环境温度的温度T1,并施加到加热的 在温度T2和T3之间铺设温度梯度,其中T2> T1和T2> T3,其中T3处于或高于环境温度,穿过至少一个长度o 通过从板产品的一侧向温度T2施加受控的热输入到板的厚度方向,以及从受控热输入的相反侧的板产品控制冷却到温度T3, 并在施加T2和T3之间的温度梯度的同时老化产品板。
    • 8. 发明申请
    • METHOD FOR CASTING A COMPOSITE INGOT
    • 铸造复合材料的方法
    • WO2010000553A1
    • 2010-01-07
    • PCT/EP2009/056811
    • 2009-06-03
    • ALERIS ALUMINUM KOBLENZ GMBHSTORM, Joost ChristiaanTEN CATE, AndreasKRÖPFL, Ingo GüntherBÜRGER, Achim
    • STORM, Joost ChristiaanTEN CATE, AndreasKRÖPFL, Ingo GüntherBÜRGER, Achim
    • B22D19/00B22D19/08B22D19/16B22D11/00
    • B22D19/16B22D11/008B22D19/0081B22D19/08B22D19/085
    • The invention relates to a method and apparatus for the casting of a composite metal ingot comprising at least two separately formed layers of one or more alloys, the method comprises providing an elongated solid substrate of a first alloy and a molten melt of a second alloy, a casting mould, the substrate and the casting mould being movable relative to one another, and wherein the casting mould comprises a liquid feed end for supplying the casting mould with a molten second alloy and an exit end with at least one outlet for casting the molten second alloy downwardly onto the substrate, and while continuously moving the casting mould and the substrate relative to one another casting the molten second alloy downwardly through the at least one outlet of the casting mould onto an upper surface of the substrate at a temperature wherein the substrate locally at least partly remelts beginning at a reference point of a remelting zone and mixes at least partly with the molten second alloy to form an alloy pool, and after the remelting the molten alloy pool continuously cools and solidifies at a location away from the reference point and joins the substrate to form the composite ingot before discharging from the casting mould.
    • 本发明涉及一种用于铸造复合金属锭的方法和装置,所述复合金属锭包括至少两个单独形成的一种或多种合金的层,所述方法包括提供第一合金的细长固体基体和第二合金的熔融熔体, 铸模,所述基底和所述铸模可相对于彼此移动,并且其中所述铸模包括用于向所述铸模供应熔融的第二合金的液体供给端和具有至少一个出口的出口端,用于铸造所述熔融的 第二合金向下到基板上,并且在连续移动铸模和基板相对于彼此的同时,将熔融的第二合金向下浇铸通过铸模的至少一个出口在基板的上表面上,其中基板 局部至少部分重熔从重熔区的参考点开始,并至少部分地与熔融的第二合金混合至f 在熔融合金池重新熔融之后,在远离参考点的位置连续地冷却和凝固,并且在从铸模排出之前连接基板以形成复合锭。