会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 5. 发明申请
    • PREFORMED DENTAL COMPOSITE CROWN, PROCESS OF PRODUCTION AND USE THEREOF
    • 预成形的牙合成冠,生产过程及其用途
    • WO2017155692A1
    • 2017-09-14
    • PCT/US2017/018856
    • 2017-02-22
    • 3M INNOVATIVE PROPERTIES COMPANY
    • HERRMANN, AndreasSCHECHNER, GallusHECHT, ReinholdMAYR, HelmarKORTEN, MalteHOFMANN, BernhardRAIA, GioacchinoMEURER, Till
    • A61K6/09A61C5/00A61C13/00
    • The invention relates to a preformed dental composite crown being characterized by its shape and chemical composition, the shape being characterized as follows: having an occlusal top surface and depending buccal, mesial, distal and lingual side surfaces, the side surfaces being connected to each other and forming a crown cervix, the wall thickness of the crown at the crown cervix being lower than 0.6 mm; at least two of opposing depending side surfaces having a concave shape; the chemical composition of the material the preformed dental composite crown is made of being a hardened composition comprising the following components: nano-filler(s) in an amount from 20 to 70 wt.%, resin matrix in an amount from 20 to 75 wt.%, wt.% with respect to the weight of the chemical composition, the resin matrix comprising urethane(meth)acrylate(s) and (meth)acrylate(s) not comprising a urethane moiety. The invention also relates to a kit of parts comprising such a preformed dental composite crown, processes for producing such crowns and the use of such a crown for treating a dental tooth.
    • 本发明涉及一种预成型牙科复合冠,其特征在于其形状和化学组成,其形状特征如下:具有咬合顶部表面和依靠的颊侧,近侧,远侧和舌侧表面, 所述侧表面彼此连接并形成冠状宫颈,所述冠状宫颈处的冠状部的壁厚小于0.6mm; 至少两个相对的从属侧表面具有凹入形状; 预成型的牙科复合材料牙冠的材料的化学组成由硬化的组合物制成,所述硬化的组合物包含以下组分:20-70重量%的纳米填料,20-75重量%的树脂基质 (甲基)丙烯酸酯和不包含氨基甲酸酯部分的(甲基)丙烯酸酯的树脂基体相对于化学组合物的重量的重量%。 本发明还涉及包含这种预成形的牙科复合冠的部件套件,用于制造这种冠部的方法以及使用这种冠部来治疗牙齿。