    • 3. 发明授权
    • 정련로 벽체 열간보수용 스프래이재 조성물
    • 喷雾组合物
    • KR1019970008698B1
    • 1997-05-28
    • KR1019940040107
    • 1994-12-30
    • 주식회사 포스코(주)포스코켐텍
    • 이상완김용훈이원창전진익
    • C04B35/03C04B35/447
    • The composition contains a dolomite clinker having a slaking-resistance as a main material. The spray material composition has excellent durability in UBD, AOD refining furnace for stainless manufacture in which the used temperature is high and the slag alkalinity is low as well as showing more an endurance life than a conventional spray material in an usual furnace. The composition comprises 50-80 wt.% a dolomite clinker having slaking resistance where the rate of weight increase is less than 2.0 wt.% by autoclave examination method(3Kg/cm2, maintaining 2hours) and CaO content is 40-65 wt.%, 1.5 wt.% or less a calcium hydroxide, 2.5-5.5 wt.% a hexameta phosphate of soda, and residue of an aid-binding agent, magnesia clinker and usual dolomite clinker.
    • 该组合物含有具有抗衰老作为主要材料的白云石熟料。 喷涂材料组合物在常规炉中的常规喷涂材料的UBD,不锈钢制造的AOD精炼炉中具有优异的耐久性,其中使用温度高,炉渣碱度低,并且显示出比常规喷涂材料更耐用的寿命。 组合物包含50-80重量%的具有耐光性的白云石熟料,通过高压釜检测方法(3Kg / cm 2,保持2小时),重量增加速率小于2.0重量%,CaO含量为40-65重量% ,1.5重量%以下的氢氧化钙,2.5-5.5重量%的苏打磷酸六铵,助残粘合剂的残渣,氧化镁熟料和通常的白云石熟料。
    • 9. 发明授权
    • 피치 함침 캐스타블 블록의 제조방법
    • 可铸块的制造方法
    • KR100265005B1
    • 2000-09-01
    • KR1019960067972
    • 1996-12-19
    • 주식회사 포스코재단법인 포항산업과학연구원
    • 이상완박노형
    • C04B35/443
    • PURPOSE: A method for preparing pitch-impregnated castable block is provided which improves corrosion-resistance and structural spalling-resistance of the castable block by controlling slag permeation through pores of the castable block. CONSTITUTION: The method comprises steps of: (i) mixing alumina-spinel or alumina-magnesia castable refractory composition with water; (ii) obtaining a dried product by molding the mixture of the step (i) and drying the molded product or obtaining a calcined product by molding the mixture of the step (i), drying the molded product and calcining the dried product at a temperature of not more than 1,750 deg.C; (iii) impregnating pitch into pores of the dried product or calcined product of the step (ii); and (iv) cooling down the product of the step (iii) to room temperature.
    • 目的:提供一种制备沥青浸渍浇注料的方法,其通过控制通过可浇注块的孔隙的渗透而改善浇注料的耐腐蚀性和抗结块剥落性。 方法:该方法包括以下步骤:(i)将氧化铝 - 尖晶石或氧化铝 - 氧化镁可浇注耐火材料组合物与水混合; (ii)通过模制步骤(i)的混合物并干燥模制产品或通过模制步骤(i)的混合物,干燥模制产品并在温度下煅烧干燥产物来获得煅烧产物来获得干燥产物 不超过1750℃; (iii)将沥青浸渍在步骤(ii)的干燥产物或煅烧产物的孔中; 和(iv)将步骤(iii)的产物冷却至室温。
    • 10. 发明授权
    • 제강래들의 구조
    • 年轻的结构
    • KR100229909B1
    • 1999-11-15
    • KR1019950032042
    • 1995-09-27
    • 주식회사 포스코
    • 김종극이상완윤태형
    • B22D41/02
    • 본 발명은 고로, 전기로 등에서 용선을 받아 정련로로 이송하거나, 정련로에서 용강을 받아 주조설비로 이송하는 데에 사용하는 제강래들(ladle)의 구조를 개선하여 내화물 수리 횟수를 줄이고, 내화물의 사용량을 최소화하며, 관리운영에 효율성을 높일 수 있도록 한 제강래들의 구조에 관한 것이다.
      본 발명은 상광하협형 몸체의 외측 양쪽에 크레인 걸고리용 트라니온(2)을 구비한 철피(1)와, 상기 철피(1)의 내측면에 축조설치되는 내화물(3)(4)을 포함하여 구성되는 제강래들(10)에 있어서, 슬래그(7)가 접촉되는 슬래그 내화물(3)이 내부에 설치되는 철피(1)의 상부를 용강(8)이 접촉되는 일반벽체 내화물(4)이 내부에 설치되는 철피(1)의 하부 연장선(9)보다 바깥쪽으로 넓게 확장 형성하여서 슬래그 내화물(3)의 두께를 일반벽체 내화물(4)의 두께보다 두껍게 하여 내화물을 설치한 것을 특징으로 하는 제강래들의 구조를 제공한다.