热词
    • 1. 发明专利
    • Method for partially repairing thermal barrier coating
    • 部分修复热障涂层的方法
    • JP2012180549A
    • 2012-09-20
    • JP2011043293
    • 2011-02-28
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • TANIGAWA HIDETSUGUOKAYA NAOTOSHIMEGA MASAHIKO
    • C23C4/02C23C4/10C23C4/18F01D5/28F01D25/00F02C7/00
    • PROBLEM TO BE SOLVED: To provide a method for partially repairing a thermal barrier coating, capable of forming a repair film having high peeling resistance.SOLUTION: The method for partially repairing a thermal barrier coating includes: a repair film forming step of thermally spraying a thermal spray material mainly composed of zirconia to a damage portion of a ceramic layer 3 mainly composed of zirconia of a member having a metal bond layer 2 and the ceramic layer 3 successively formed on a heat-resisting alloy base material 1 to form a repair film 9; and a vertical crack formation step of irradiating a surface of the repair film 9 with laser beam after coating the surface of the ceramic layer 3 that can be a passage of laser beam around the repair film 9 with a reflecting material having laser reflecting capability to form vertical cracks 11 in the repair film 9.
    • 要解决的问题:提供能够形成耐剥离性高的修补膜的部分修复隔热涂层的方法。 解决方案:用于部分修复热障涂层的方法包括:修复膜形成步骤,其将主要由氧化锆组成的热喷涂材料热喷涂到主要由具有氧化锆的构件的氧化锆组成的陶瓷层3的损伤部分 金属接合层2和陶瓷层3依次形成在耐热合金基材1上以形成修复膜9; 以及垂直裂纹形成步骤,其在用可激光反射能力的反射材料涂覆陶瓷层3的表面之后照射修复膜9的表面,该表面可以是修复膜9周围的激光束通过 修理膜9的垂直裂缝11。版权所有(C)2012,JPO&INPIT
    • 9. 发明专利
    • Repairing method, and heat-resistant member of gas turbine repaired thereby
    • 修复方法和修复的燃气轮机的耐热构件
    • JP2014159641A
    • 2014-09-04
    • JP2014085330
    • 2014-04-17
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • MEGA MASAHIKOTORIGOE TAIJIOHARA MINORUKAMIMURA YOSHIHISAOKAYA NAOTOSHIKANEKO HIDEAKITANIGAWA HIDETSUGU
    • C23C4/02C23C4/06C23C4/10F01D5/28F02C7/00F23R3/42
    • PROBLEM TO BE SOLVED: To provide a method for partly repairing TBC while maintaining heat durability of the TBC.SOLUTION: A method for repairing a damaged part 4 of a top-coat layer 3 of a member where an under-coat layer 2 and the top-coat layer 3 are formed on a base material 1 includes: a top-coat layer removing step for jetting water by pressurization to remove the damaged part 4 of the top-coat layer 3; an under-coat layer removing step for removing the under-coat layer 2 exposed by removing the top coat layer 3 by jetting water by pressurization so that the exposed under-coat layer 2 remains on the outer periphery of a part where the under-coat layer 2 is removed; an under-recoat layer forming step for forming an under-recoat layer 6 on the base material 1 where the under-coat layer 2 exposed in the under-coat layer removing step is removed; and a top-recoat layer forming step for forming a top-recoat layer 7 on the formed under-recoat layer 6.
    • 要解决的问题:提供一种在保持TBC的耐热性的同时部分地修复TBC的方法。解决方案:一种用于修复下涂层2和底涂层2的部件的顶涂层3的损坏部分4的方法 顶涂层3形成在基材1上,包括:顶涂层去除步骤,用于通过加压喷射水以除去顶涂层3的损坏部分4; 通过加压喷射水来除去顶涂层3而露出的底涂层2的下涂层去除步骤,使得曝光的底涂层2残留在下涂层的一部分的外周上 层2被去除; 在基材1上形成底涂层6的下涂层层形成工序,其中在下涂层除去工序中露出的下涂层2被除去; 以及用于在所形成的下涂层6上形成顶部涂层7的顶部涂层层形成步骤。
    • 10. 发明专利
    • Method for manufacturing gas turbine member
    • 制造气体涡轮机构件的方法
    • JP2012184733A
    • 2012-09-27
    • JP2011049564
    • 2011-03-07
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • HORIE JOMEGA MASAHIKOTANIGAWA HIDETSUGU
    • F02C7/00B23K26/00B23K26/38F01D5/18F01D9/02
    • PROBLEM TO BE SOLVED: To provide a means for preventing damage of an inner wall surface in a cooling passage by a laser beam penetrating through a gas turbine member when cooling holes are formed by laser working to the gas turbine member having acute corner part, rib and the like in the cooling passage.SOLUTION: In a method for manufacturing the gas turbine member for forming the cooling holes 14 for introducing a cooling gas to the surface 11a of a turbine stationary blade 10 to the turbine stationary blade 10 having the cooling passage in which the cooling gas is circulated in its inner part by the laser working, the laser working is performed in such a state that an extendable and contractive structure body 17 which can absorb the laser beam L and with which at least a part of the cooling passage is filled is disposed in the cooling passage.
    • 要解决的问题:提供一种用于通过激光加工到具有锐角的燃气轮机部件形成冷却孔时,通过穿透燃气轮机部件的激光束来防止冷却通道内壁表面的损坏的装置 部分,肋等。 解决方案:在用于形成用于形成用于将冷却气体引入到涡轮固定叶片10的表面11a的冷却孔14的燃气轮机部件的制造方法中,所述冷却孔14具有冷却通路的涡轮固定叶片10, 通过激光加工在其内部循环,激光加工在这样的状态下进行,即可以吸收激光束L并且至少部分冷却通道被填充的可延伸和收缩结构体17被布置 在冷却通道中。 版权所有(C)2012,JPO&INPIT