    • Process for production of highly polymerized aromatic polycarbonate resin
    • 生产高聚合芳族聚碳酸酯树脂的方法
    • US08674053B2
    • 2014-03-18
    • US13510780
    • 2010-11-18
    • Yoshinori IsahayaShu YoshidaNoriyuki KatoHiroki Furuhashi
    • Yoshinori IsahayaShu YoshidaNoriyuki KatoHiroki Furuhashi
    • C08G64/00C08G63/02
    • C08G64/42C08G64/305
    • A method for highly polymerizing an aromatic polycarbonate resin, which enables the increase in molecular weight of the aromatic polycarbonate resin satisfactorily while keeping good quality of the resin. An aromatic polycarbonate is linked to an aliphatic diol compound having a boiling point of 240° C. or higher (preferably in an amount of 0.01 to 1.0 mole per mole of the total amount of the terminal of the aromatic polycarbonate) through a transesterification reaction in the presence of a transesterification catalyst under reduced pressure conditions (preferably at a reduced pressure ranging from 13 kPaA (100 torr) to 0.01 kPaA (0.01 torr)), thereby increasing the molecular weight of the resulting molecule. The weight average molecular weight (Mw) of the aromatic polycarbonate after the transesterification reaction can be increased preferably by 5,000 or more compared to that of the aromatic polycarbonate before the transesterification reaction.
    • 芳香族聚碳酸酯树脂的高度聚合的方法,能够令树脂的良好品质保持良好,能够令芳香族聚碳酸酯树脂的分子量提高。 通过酯交换反应将芳族聚碳酸酯与沸点为240℃以上的脂肪族二醇化合物(优选为每摩尔芳族聚碳酸酯的末端的总量为0.01〜1.0摩尔)连接, 在减压条件下(优选在13kPaA(100乇)至0.01kPa(0.01乇))的减压条件下存在酯交换催化剂,从而提高所得分子的分子量。 与酯交换反应前的芳香族聚碳酸酯相比,酯交换反应后的芳香族聚碳酸酯的重均分子量(Mw)优选提高5000以上。
    • 4. 发明申请
    • PROCESS FOR PRODUCTION OF HIGHLY POLYMERIZED AROMATIC POLYCARBONATE RESIN
    • 生产高分子量芳族聚碳酸酯树脂的方法
    • US20130197166A1
    • 2013-08-01
    • US13510780
    • 2010-11-18
    • Yoshinori IsahayaShu YoshidaNoriyuki KatoHiroki Furuhashi
    • Yoshinori IsahayaShu YoshidaNoriyuki KatoHiroki Furuhashi
    • C08G64/42
    • C08G64/42C08G64/305
    • A method for highly polymerizing an aromatic polycarbonate resin, which enables the increase in molecular weight of the aromatic polycarbonate resin satisfactorily while keeping good quality of the resin. An aromatic polycarbonate is linked to an aliphatic diol compound having a boiling point of 240° C. or higher (preferably in an amount of 0.01 to 1.0 mole per mole of the total amount of the terminal of the aromatic polycarbonate) through a transesterification reaction in the presence of a transesterification catalyst under reduced pressure conditions (preferably at a reduced pressure ranging from 13 kPaA (100 torr) to 0.01 kPaA (0.01 torr)), thereby increasing the molecular weight of the resulting molecule. The weight average molecular weight (Mw) of the aromatic polycarbonate after the transesterification reaction can be increased preferably by 5,000 or more compared to that of the aromatic polycarbonate before the transesterification reaction.
    • 芳香族聚碳酸酯树脂的高度聚合的方法,能够令树脂的良好品质保持良好,能够令芳香族聚碳酸酯树脂的分子量提高。 通过酯交换反应将芳族聚碳酸酯与沸点为240℃以上的脂肪族二醇化合物(优选为每摩尔芳族聚碳酸酯的末端的总量为0.01〜1.0摩尔)连接, 在减压条件下(优选在13kPaA(100乇)至0.01kPa(0.01乇))的减压条件下存在酯交换催化剂,从而提高所得分子的分子量。 与酯交换反应前的芳香族聚碳酸酯相比,酯交换反应后的芳香族聚碳酸酯的重均分子量(Mw)优选提高5000以上。