    • METHOD FOR PRODUCING FIBREBOARDS UTILIZING PALM BIOMASS
    • 用于生产利用PALM生物量的纤维素的方法
    • WO2013051926A2
    • 2013-04-11
    • PCT/MY2012/000258
    • 2012-09-28
    • MALAYSIAN PALM OIL BOARDDONGWHA MALAYSIA HOLDINGS SDN. BHD.IBRAHIM, ZawawiMOKHTAR, AnisABDUL AZIZ, AstimarWAN HASSAN, Wan HassamuddinCHOO, Yuen MaySI, Joon LeeSOO, Bang EuOMAR, RosmaziTABARI, Ahmad, Sirajuddin
    • IBRAHIM, ZawawiMOKHTAR, AnisABDUL AZIZ, AstimarWAN HASSAN, Wan HassamuddinCHOO, Yuen MaySI, Joon LeeSOO, Bang EuOMAR, RosmaziTABARI, Ahmad, Sirajuddin
    • B27N3/04B27N3/08
    • B27N3/04B27N3/08
    • The present invention relates to a method of producing fibreboards using 100% of oil palm trunk (OPT). The present invention also relates to method of producing fibreboards using a mixture comprising OPT, rubber wood (RW) and mixed tropical hardwood (MTH). The method for producing fibreboards using a mixture comprising OPT, rubber wood (RW) and mixed tropical hardwood (MTH) includes the steps of: (i) chipping of oil palm trunk (OPT), rubber wood (RW) and (MTH) within size range of 0.012 to 0.050m; (ii) blending the chipped OPT with RW and MTH chips at a blending ratio of 5 to 50% of chipped OPT, 5 to 50% of RW and 5 to 50% MTH; (iii) treating the mixture obtained from step (ii) under between 2 to 8 bar at temperature between 150 to 180° C for a period between 100 to 400 seconds in digester; (iv) mechanically refining the mixture of OPT, RW and MTH chips in a steam pressurized refiner where the chips are converted to refined fibres; (v) applying resin between 6 to 12% by dry weight of fibres and/or wax between 0.5 to 2.5% by dry weight of fibres to the OPT refined fibres obtained from step (iv); (vi) transforming the resinated fibres obtained from step (v) into mat; (vii) pressing the mat obtained from step (vi) at temperature between 160 to 220° C for a period time of 2 to 5 minutes. As for the method for producing fibreboards using 100% of OPT, the method include steps (i), (iii), (iv), (v), (vi) and (vii) as mentioned above using 100% of OPT only.
    • 本发明涉及使用100%油棕树干(OPT)生产纤维板的方法。 本发明还涉及使用包括OPT,橡胶木(RW)和混合热带硬木(MTH)的混合物生产纤维板的方法。 使用包括OPT,橡胶木(RW)和混合热带硬木(MTH)的混合物生产纤维板的方法包括以下步骤:(i)在油棕榈树干(OPT),橡胶木(RW)和(MTH)内切碎 尺寸范围0.012〜0.050m; (ii)将切片的OPT与切片OPT的5%至50%,RW的5%至50%和5%至50%MTH的混合比与RW和MTH芯片混合; (iii)将从步骤(ii)获得的混合物在2至8巴之间,温度在150至180℃之间,在蒸煮器中处理100至400秒; (iv)在蒸汽加压精炼机中机械地精炼OPT,RW和MTH碎片的混合物,其中芯片转化成精制纤维; (v)将干燥重量为6至12%的纤维和/或0.5至2.5%干纤维之间的树脂施加到由步骤(iv)获得的OPT精制纤维中; (vi)将由步骤(v)获得的树脂纤维转化成垫; (vii)在160-220℃的温度下将从步骤(vi)获得的垫压制2至5分钟的时间。 对于使用100%的OPT生产纤维板的方法,该方法包括仅使用100%OPT的如上所述的步骤(i),(iii),(iv),(v),(vi)和(vii)。